Abstract

Abstract In this work boria based welding flux was used to remove the native oxide layer on ZrB 2 and promote bonding/wetting with copper. Without boria welding flux the Cu/ZrB 2 system showed no wetting. When flux was used at the interface no dissolution or reaction was observed between Cu, ZrB 2 and the flux. The effectiveness of boria in dissolving zirconia oxide surface layer was further confirmed on wetting tests carried out on pre-oxidised ZrB 2 samples having an oxide scale of 15 μm thickness. A mock joint was made using copper with flux, and it had no trapped porosity induced by the presence of the boria flux. This work suggests a novel, low cost and scalable route to promote joining/wetting of dissimilar materials having melting points differing by 2000 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Electronic structure, bonding, and ground-state properties of AlB 2-type transition-metal diborides10.1103/PhysRevB.63.045115 ↗
2. Overview on wetting and joining in transition metals diborides, advances in science and technology
3. Joining of ZrB2‐Based ultra‐high‐temperature ceramic composites to Cu–clad–molybdenum for advanced aerospace applications10.1111/j.1744-7402.2008.02291.x ↗
4. Thermal characterisation of ceramic/metal joining techniques for fusion applications using x-ray tomography10.1016/j.fusengdes.2014.05.002 ↗
5. Contact reaction between refractory compounds and liquid metals10.1007/BF00791269 ↗
6. The wetting of refractory carbides, borides, and nitrides by molten metals10.1007/BF00780116 ↗
7. Liquid metal/ceramic interactions in the (Cu, Ag, Au)/ZrB 2 systems10.1016/j.jeurceramsoc.2006.12.008 ↗
8. Wetting and infiltration of zirconium diboride by copper and copper/boron alloys
9. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
10. The stoichiometry of hydrogen reduced zirconia and its influence on catalytic activity part 1: volumetric and conductivity studies10.1039/b109887j ↗
11. Zirconia transport by liquid convection during oxidation of zirconium diboride–silicon carbide10.1111/j.1551-2916.2007.02142.x ↗
12. Wetting and interfacial phenomena of Ni-Ta alloys on CVD-SiC
13. Flash spark plasma sintering (FSPS) of pure ZrB210.1111/jace.13109 ↗
14. Jacobson · 2005
15. Wettability of some metals against zirconia ceramics10.1007/BF01729384 ↗
16. A comparison of the wettability of copper-copper oxide and silver-copper oxide on polycrystalline alumina10.1007/BF01154485 ↗
17. Wettability of zirconium diboride ceramics by Ag, Cu and their alloys with Zr10.1016/S1359-6462(02)00361-5 ↗