Optimized etching of porcelain and polycrystalline alumina with a glass phase
Source abstract
Abstract
Abstract Chemical and thermal etching techniques are commonly used in ceramography to enhance microstructural features. While thermal etching works well for high purity ceramic systems, this technique may not be appropriate where glass is present. Porcelain and industrial alumina both contain a glass phase, typically 40−60 vol% and 4−30 vol%, respectively, and these glass chemistries are proposed to be similar. Chemical etching of porcelain is common, but the images published in the literature are frequently over-etched. When glass is present in the grain boundaries of alumina, thermal etching can cause the glass to disappear or to recrystallize, obscuring the microstructure. Because of this, it is proposed that both chemical and thermal etching are necessary to prepare an industrial alumina microstructure for grain size measurements. In addition, it was observed that chemical etching is sensitive to the residual stress in the glass phase, becoming more aggressive when there is residual tension in the glass.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Recycling and utilization of industrial and municipal waste in materials production · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Taffner · 2004 · 1057
2. Surface coating technique for revealing grain structures in Alumina10.1111/j.1151-2916.1988.tb05865.x ↗
3. Thermal etching of SiC10.1016/j.apsusc.2011.12.132 ↗
4. Lam · 2007
5. Observations on the glass phase composition in porcelains
6. DeCarlo · 2008
7. Dissolution of alumina in silicate glasses and the glass formation boundary
8. Unity molecular formula approach to glaze development
9. Lam · 2010
10. Whipkey · 2020 · 124
11. Lerdprom · 2014 · 84
12. Porcelain—raw materials, processing, phase evolution, and mechanical behavior10.1111/j.1151-2916.1998.tb02290.x ↗
13. Tseng · 2015
14. Petzow · 1999 · 154
15. Comparison of strength of triaxial porcelains containing alumina and silica10.1111/j.1151-2916.1967.tb15128.x ↗
16. Properties related phase evolution in porcelain ceramics10.1016/j.jeurceramsoc.2007.02.096 ↗
17. Properties of triaxial porcelain bodies: interpretation of statistical modeling10.1111/j.1551-2916.2006.01245.x ↗
18. Effect of firing conditions, filler grain size and quartz content on bending strength and physical properties of sanitaryware porcelain10.1016/j.jeurceramsoc.2003.07.003 ↗
19. New body mixes for porcelain stoneware tiles with improved mechanical characteristics10.1016/j.jeurceramsoc.2006.05.007 ↗
20. The use of nepheline-syenite in a body mix for porcelain stoneware tiles10.1016/j.ceramint.2004.05.006 ↗
21. Enhancing the mechanical properties of porcelain stoneware tiles: a microstructural approach10.1016/S0955-2219(00)00266-1 ↗
22. Lundin · 1964 · 93
23. Porcelain—raw materials, processing, phase evolution, and mechanical behavior10.1111/j.1151-2916.1998.tb02290.x ↗
24. Fired porcelain microtructures revisited10.1111/j.1151-2916.1999.tb02282.x ↗
25. Microstructural evolution in triaxial porcelain10.1111/j.1151-2916.2000.tb01692.x ↗
26. Recycle of waste glass into "Glass-Ceramic stoneware"10.1111/j.1551-2916.2008.02460.x ↗
27. Creation of microcracks in porcelain during firing10.1016/j.jeurceramsoc.2011.05.045 ↗
28. Effect of firing temperature on sintering of porcelain stoneware tiles10.1016/j.ceramint.2007.06.006 ↗
29. Effect of quartz particle size on the strength of triaxial porcelain10.1016/j.jeurceramsoc.2006.01.012 ↗
30. The effect of quartz and mullite phases on strength of triaxial porcelain
31. Influence of Lithium oxide as auxiliary flux on the properties of triaxial porcelain bodies10.1016/j.jeurceramsoc.2005.01.036 ↗
32. Influence of mixing on mullite formation in porcelain10.1016/S0955-2219(01)00274-6 ↗
33. Interactions between an ABS type leadless glaze and a biscuit fired bone China body during glost firing. Part II: investigations of interactions10.1016/S0955-2219(01)00420-4 ↗
34. Reduction of the porcelain firing temperature by preparation of the raw materials10.1016/j.jeurceramsoc.2009.03.029 ↗
35. Pinto · 2006 · 207
36. Pinto · 2001
37. X-ray strain measurement techniques for ceramics bodies10.1111/j.1151-2916.1961.tb11659.x ↗
38. Internal stresses in model ceramic systems10.1111/j.1151-2916.1959.tb12967.x ↗
39. Special benefits of bauxite for a stable porcelain microstructure in high-voltage insulation
40. Chinn · 2002 · 45
41. Elssner · 1999 · 39
42. Metallographic specimen preparation
43. The influence of surface energy on thermal etching10.1016/0001-6160(58)90150-0 ↗
44. The thermal etching of silver10.1098/rspa.1948.0057 ↗
45. Carty · 1992
46. Otminski · 2013
47. Compositional dependence of fragility and glass forming ability of calcium aluminosilicate melts10.1016/j.jnoncrysol.2009.04.004 ↗
48. Skovira · 2006 · 87
49. Lundin · 1964 · 93
50. X-ray measurement of strain in quartz particles of whiteware bodies10.1111/j.1151-2916.1968.tb11920.x ↗