Novel measurement technique of crack length for indentation fracture (IF) method using high contrast image of crack tips through thin film coating
Source abstract
Abstract
Abstract In order to improve the reproducibility of the indentation fracture (IF) method, a novel visualizing technique of the crack tips was developed. Coating a visualizing solution on the indented surface of silicon carbide could enhance the contrast of the crack tips. In order to verify our new approach, a round-robin test on the indentation fracture resistance, K IFR , of silicon carbide was conducted with nine laboratories. The clear identification of the crack tips could reduce the errors in reading crack lengths markedly even when measured with the ordinal metallurgical microscope at a low total magnification of 100×. Thus, good matching of K IFR was obtained between laboratories. Two main mechanisms of the enhanced contrast of the crack tips were proposed as follows; (a) the reduction of diffuse scattering from the smooth surface of the coating, (b) the interference color due to the slight change in thickness of the coating around the cracks.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
2. Evaluation of fracture toughness for ceramic materials by a single-edge-precracked-beam method10.1111/j.1151-2916.1988.tb05049.x ↗
3. Testing methods for fracture toughness of fine ceramics, Japanese Industrial Standard, JIS R 1607, 1995.
4. Fine ceramics (Advanced ceramics, Advanced technical ceramics)—determination of fracture toughness of monolithic ceramics at room temperature by the surface crack in flexure (SCF) method, International Organization for Standards, ISO 18756, Geneva, 2003.
5. Fine Ceramics (Advanced ceramics, Advanced technical ceramics)—silicon nitride materials for rolling bearing balls, International Organization for Standards, ISO 26602, 2009.
6. Standard specification for silicon nitride bearing balls, ASTM standard F 2094/M2094M, 2008.
7. Fine ceramics (advanced ceramics, advanced technical ceramics)—test method for fracture resistance of silicon nitride materials for rolling bearing balls at room temperature by Indentation Fracture (IF) Method, International Organization for Standards, ISO 14627, 2012.
8. The VAMAS hardness round-robin on ceramic materials
9. Result of the fracture toughness test round robin on ceramics—VAMAS Project10.2109/jcersj.99.417 ↗
10. The VAMAS fracture toughness test round-robin on ceramics
11. Report of preliminary investigation for standardization of fine ceramics, Japanese Fine Ceramics Association, Japan, 1988.
12. Fracture toughness of ceramics by the Vickers indentation crack length method: a critical review10.1002/9780470291313.ch5 ↗
13. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
14. Round robin on indentation fracture resistance of silicon carbide ceramics by using a powerful optical microscope10.1016/j.ceramint.2012.06.072 ↗
15. Improved accuracy of the measurements of indentation fracture resistance for silicon nitride ceramics by the powerful optical microscopy10.1016/j.ceramint.2013.05.068 ↗
16. Refined measurements of indentation fracture resistance of alumina using powerful optical microscopy10.1016/j.ceramint.2013.10.039 ↗
17. Evaluation of KIc of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
18. Accuracy (Trueness and Precision) of measurement methods and results—Part 2: Basic method for the determination of repeatability and reproducibility of a standard measurement method, Japanese Industrial Standard, JIS Z 8402-2, 1999.