Inhibiting the sp2 carbon deposition by adjunction of sulphurous species in refractory ceramics subjected to CO and H2 reducing atmosphere
Source abstract
Abstract
Abstract The formation of sp2 carbon by the Boudouard reaction significantly damages the refractory ceramics. Sulphur is an efficient way to prevent the carbon deposition catalysed by Fe3C, in the presence of H2. Thermogravimetric analysis was carried out on Fe2O3 samples exposed to a CO/H2 gas mixture at 600 °C. Solid sulphur was mixed with Fe2O3 powder or continually added in the form of gas into the CO/H2 reducing gas. The samples were characterised by X-ray diffraction, Raman spectroscopy, SEM and TEM. The addition of 100 ppm of sulphur species in the gas prevents the formation of carbon. The mechanism that governs the inhibition of the reaction is proposed, in which the formation of a thin protective FeS layer (0.5–1 nm) is involved. This study paves the way to an effective solution to inhibit the sp2 carbon deposition in the refractories by poisoning the Fe3C catalyst with sulphur.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Les phénomènes de combustion dans les foyers industriels
2. Catalytic effect of iron on decomposition of carbon monoxide: I. Carbon deposition in H2-CO mixtures10.1007/BF02642919 ↗
3. Carbon formation from carbon monoxide-hydrogen mixtures over iron catalysts. I. properties of carbon formed. II. rates of carbon formation10.1021/j150572a002 ↗
4. Carbon formation on iron and nickel foils by hydrocarbon pyrolysis—reactions at 700°C10.1016/0008-6223(74)90060-8 ↗
5. Dokl. Akad
6. Hughes · Thomas J. Fuel · 1962 · 41 · 297
7. Interaction of evaporated carbon with heated metal substrates10.1016/0008-6223(67)90056-5 ↗
8. Carbon formation from methane pyrolysis over some transition metal Surfaces -I. Nature and properties of the carbons formed10.1016/0008-6223(70)90076-X ↗
9. Pyrolytic carbon formation from carbon suboxide10.1038/192450a0 ↗
10. Growth of single-crystal graphite by pyrolysis of acetylene over metals10.1016/0008-6223(69)90002-5 ↗
11. The solid reaction products of the catalytic decomposition of carbon monoxide on iron at 550°C10.1016/0008-6223(69)90005-0 ↗
12. Catalytic disproportionation of CO in the absence of hydrogen: encapsulating shell carbon formation10.1016/0008-6223(94)90169-4 ↗
13. Single-wall nanotubes produced by metal-catalyzed disproportionation of carbon monoxide10.1016/0009-2614(96)00862-7 ↗
14. The predictability of CO resistance of refractory materials by state-of-the-art test methods-a technical and scientific approach
15. The catalytic effect of iron oxides on the formation of Nano-carbon by the Boudouard reaction in Refractories10.1016/j.jeurceramsoc.2016.02.052 ↗
16. Probing the structural organisation of sp2 carbons obtained by the Boudouard reaction using in situ Raman scattering in reducing conditions10.1016/j.vibspec.2016.10.003 ↗
17. Mechanical and thermal properties of carbon nanotubes10.1016/0008-6223(95)00021-5 ↗
18. Challenges and benefits of utilizing carbon nanofilaments in cementitious materials10.1155/2012/371927 ↗
19. Drzal · 2006
20. Thermodynamics, mechanisms and kinetics of metal dusting10.1002/(SICI)1521-4176(199805)49:5<303::AID-MACO303>3.0.CO;2-P ↗
21. Relationship between the growth of carbon nanofilaments and metal dusting corrosion10.1021/cm050712u ↗
22. Mechanisms of metal dusting10.1149/1.1483099 ↗
23. On the mechanism of catastrophic carburization: metal dusting10.1016/0010-938X(93)90334-D ↗
24. Effect of H2S on formation and decomposition of Fe3C and Fe5C2 under metal dusting conditions10.1002/srin.200005710 ↗
25. Decomposition of methane over Iron catalysts at the range of moderate temperatures: the influence of structure of the catalytic systems and the reaction conditions on the yield of carbon and morphology of carbon filaments10.1006/jcat.2001.3243 ↗
26. Influence of impurities and role of iron carbides in deposition of carbon from CO10.1111/j.1151-2916.1956.tb15838.x ↗
27. Schneider · 2007 · vol. 31 · 141
28. Effect of H2S on metal dusting of iron10.1002/maco.200303735 ↗
29. Inhibition of carbon deposition on iron and steel surfaces10.1016/0008-6223(71)90083-2 ↗
30. Thermal expansion and crystal structure of cementite, Fe3C, between 4 and 600 K determined by time-of-flight neutron powder diffraction10.1107/S0021889803024695 ↗
31. Crystal structure determination of Hägg carbide, x-Fe5C2 by first-principles calculations and Rietveld refinement10.1524/zkri.2012.1490 ↗
32. Characterizing various types of defects in nuclear graphite using Raman scattering: heat treatment, ion irradiation and polishing10.1016/j.carbon.2015.07.095 ↗
33. How to obtain a reliable structural characterization of polished graphitized carbons by Raman micro spectroscopy10.1002/jrs.3014 ↗
34. Determination of crystallite size in polished graphitized carbon by Raman spectroscopy10.1103/PhysRevB.86.134205 ↗
35. Studying disorder in graphite-based systems by Raman spectroscopy10.1039/B613962K ↗
36. Raman spectra of ground natural graphite10.1016/0008-6223(78)90043-X ↗
37. Resonance Raman contribution to the D band of carbon materials: modeling defects with quantum chemistry10.1063/1.1710853 ↗
38. Raman spectroscopy of polyconjugated molecules and materials: confinement effect in one and two dimensions10.1098/rsta.2004.1448 ↗
39. Annular reactor testing and Raman surface characterization in the CPO of methane and propylene10.1016/j.apcata.2013.06.005 ↗
40. Influence of H2S on metal dusting10.1002/(SICI)1521-4176(199805)49:5<336::AID-MACO336>3.0.CO;2-1 ↗
41. Reduction of SO2 to elemental sulfur with H2 and mixed H2/CO gas in an activated carbon bed10.1016/j.cherd.2017.03.014 ↗
42. Role of sulphur in carburization, carbide formation and metal dusting of iron10.1002/sia.1319 ↗