Corrosion behavior of a Mo(Si, Al)2 composite at 1700°C in 95% N2 + 5% H2
Source abstract
Abstract
Abstract A Mo(Si, Al)2 based composite was pre-oxidized to establish an alumina scale on the material surface. Thereafter, the corrosion behavior of the composite was examined at 1700 °C for up to 24 h in 95% N2 + 5% H2. The weight change was followed by recording the material weight before and after exposure. The crystalline corrosion products were analyzed with X-ray diffraction (XRD) and the microstructure of the cross sectioned material was characterized using scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDS). It was shown that AlN and Al5O6N layers developed on top of the pre-oxidized alumina layer and alumina threads develop out from the specimen surface. The accompanied aluminum consumption converts the substrate Mo(Si,Al)2 into Mo5Si3 immediately below the alumina scale to the extent that the Mo5Si3 becomes porous underneath the alumina scale. Corrosion mechanisms are discussed with the support of thermodynamic calculations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. The beneficial effect of water vapour on the oxidation at 600 and 700 °C of a MoSi2-based composite10.1016/j.jeurceramsoc.2004.01.005 ↗
2. High-temperature oxidation of MoSi210.1007/s10853-009-4012-8 ↗
3. Microstructures of SiO2 scales formed on MoSi210.4028/www.scientific.net/MSF.522-523.595 ↗
4. An investigation of the microstructure in the pest oxide of a MoSi2- based composite10.1002/9780470294635.ch57 ↗
5. On the mechanism of MoSi2 pesting in the temperature range 400–500C10.1002/9780470294635.ch56 ↗
6. Low temperature oxidation of fully dense and porous MoSi210.1016/S0921-5093(98)01078-8 ↗
7. Effect of third elements on the pesting suppression of Mo-Si-X intermetallics (X = Al, Ta, Ti, Zr and Y)10.1016/0966-9795(96)00019-2 ↗
8. Oxidation kinetics and composite scale formation in the system Mo(Al,Si) 210.1111/j.1151-2916.2002.tb00109.x ↗
9. Influences of Al content and secondary phase of Mo5(Si,Al)3 on the oxidation resistance of Al-rich Mo(Si,Al)2-base composites10.1016/S0966-9795(03)00072-4 ↗
10. Microstructure and properties stability of Al-alloyed MoSi2 matrix composites10.1016/j.intermet.2003.10.001 ↗
11. The intermediate and high-temperature oxidation behaviour of Mo(Si,Al,), intermetallic alloys10.1016/S0966-9795(96)00068-4 ↗
12. High temperature oxidation of intermetallic compounds of Mo(Si1-xAlx)210.1016/0010-938X(93)90312-5 ↗
13. The behaviour of commercial FeCrAIRE alloys in nitrogen-oxygen - water vapour bioxidant environments
14. Properties of alumina/chromia scales in N2-containing low oxygen activity environment investigated by experiment and theory10.1007/s11085-016-9703-3 ↗
15. High temperature corrosion of commercial FeCrAl alloys (Kanthal AF) in nitrogen gas10.2298/JMMB181121012V ↗
16. Oxidation - nitridation of Ni-Cr-Al alloys10.1590/S1516-14392004000100003 ↗
17. Reprint of: FactSage thermochemical software and databases, 2010–2016
18. Volatility of the oxides of tungsten and molybdenum in the presence of water vapour10.1038/163601b0 ↗
19. Oxidation behavior of a Mo(Si,Al)2 composite at 900–1600 C in dry air10.1007/s10853-012-6906-0 ↗
20. Oxidation behaviour of a Mo(Si,Al)2 based composite at 1500°C10.1016/j.intermet.2011.05.002 ↗
21. Huang · 2018
22. High-temperature oxidation