journal article·2012-07

Revealing crack profiles in polycrystalline tetragonal zirconia by ageing

F.G. Marro, E. Camposilvan, M. Anglada

Publisher page

Abstract

Exposure to hot water vapour is shown to be useful for staining indentation crack profiles in doped zirconia polycrystals. This is illustrated here in 3Y-TZP with two different grain sizes, for which Vickers indentation cracks are of Palmqvist type, as well as in 3Y-TZP with 2.5 wt.% cerium oxide, for which indentation cracks are half-penny. The crack profile is clearly revealed on the fracture surface after biaxial flexural testing in all the specimens previously exposed to hot water vapour. The contrast in 3Y-TZP is induced by t–m transformation caused by hydrothermal degradation, which induces an intergranular fracture zone in front of the initial position of the indentation crack tip. The biaxial strength and apparent fracture toughness of 3Y-TZP increase substantially with the time of exposure at a rate that depends on the grain size. On the contrary, in 3Y-TZP doped with ceria no signal of t–m transformation is found and the flexure biaxial stress remains practically constant, but the initial position of the indentation crack is also clearly revealed by an intergranular fracture zone in front of the initial position of the crack tip. In this case, this is associated to environmentally assisted slow crack growth under the indentation residual stress during exposure to hot water vapour in autoclave.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Fracture toughness of ceramics by the surface crack in flexure (SCF) method
2. Effect of crack “halos” on fracture toughness determined by the surface crack in flexure method10.1111/j.1151-2916.1998.tb02620.x ↗
3. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
4. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
5. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
6. Surface modification of 3Y-TZP with cerium oxide10.1016/j.jeurceramsoc.2010.10.008 ↗
7. Contact damage in a Ce-TZP/Al2O3 nanocomposite10.1016/j.jeurceramsoc.2011.05.022 ↗
8. Low temperature degradation ageing of zirconia: a critical review of the relevant aspects in dentistry
9. Corrosion screening tests of high-performance ceramics in supercritical water containing oxygen and hydrochloric acid10.1016/S0955-2219(96)00072-6 ↗
10. Disintegration process of yttria-stabilized zirconia ceramics using hydrothermal conditions10.1007/s10853-006-1167-4 ↗
11. Strengthening of Vickers indented 3Y-TZP by hydrothermal ageing10.1016/j.jeurceramsoc.2011.08.019 ↗
12. Evaluation of KIC of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
13. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
14. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
15. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
16. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
17. The ball on three balls test for strength testing of brittle discs. Part II. Analysis of possible errors in the strength determination10.1016/j.jeurceramsoc.2003.10.035 ↗
18. Simple expressions for the evaluation of stresses in sphere-loaded discs under biaxial flexure10.1520/JTE101402 ↗
19. Biaxial flexure test for ceramics
20. Subsurface evaluation of hydrothermal degradation of zirconia10.1016/j.actamat.2010.09.047 ↗
21. Ageing behaviour of Y-TZP
22. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
23. Quantification of hydrothermal degradation in zirconia by nanoindentation10.1016/j.actamat.2008.04.050 ↗
24. Study of near surface changes in YTZP after LTD10.3139/146.101791 ↗
25. Toughening of layered ceramic composites with residual surface compression10.1111/j.1151-2916.1996.tb07883.x ↗
26. Strengthening of oxide ceramics by transformation-induced stress10.1111/j.1151-2916.1987.tb04952.x ↗
27. Weibull characterization of the flexural strength of hydrothermally degraded 3Y-TZP zirconia
28. Fracture of brittle solids10.1017/CBO9780511623127 ↗
29. Schell · Eng Fract Mech · 2009 · 76 · 248610.1016/j.engfracmech.2009.08.008 ↗