Tribological behavior of TZ4YS-MoSi2 composites obtained by Spark Plasma Sintering
Source abstract
Abstract
[EN] The aim of this work was to evaluate the role of MoSi2 content (5, 10, 15 wt%) in the mechanical and tribological behavior of TZ4YS-MoSi2 composites obtained by colloidal processing and spark plasma sintering (SPS) at 1500 degrees C. Firstly, the densification of TZ4YS-MoSi2 composite and the shrinkage-rate curves by SPS applying 80 MPa from 1300 degrees C to 1500 degrees C is studied. The hardness and fracture toughness values confirmed that up to 99.9% densification is gradually reached with increasing MoSi2 percentage. Secondly, pin-on-disk tribological tests at different distances (1, 5, 15 and 2000 m) with Al2O3 as counterpart were performed to record the behavior of the materials in the initial and final stages of wear. The MoSi2 content was associated to the beginning of the transition from mild to severe wear, higher the amount of MoSi2 faster is the transition. This behavior was correlated with MoSi2 content, which aids the formation of a tribolayer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Basu · 2011
2. Development of a new TBC system for more efficient gas turbine engine application10.1016/j.matpr.2016.06.019 ↗
3. Borrell · 2018
4. Eliaz · 2012
5. Thermal cycling and reactivity of a MoSi2/ZrO2 composite designed for self-healing thermal barrier coatings10.1016/j.matdes.2016.01.054 ↗
6. ZrB2-MoSi2 ceramics: A comprehensive overview of microstructure and properties relationships. Part I: Processing and microstructure10.1016/j.jeurceramsoc.2019.01.022 ↗
7. Effect of Nano-ZrO2 on the Microstructure and High Temperature Tribological Properties of MoSi2 Coating10.1007/s11666-013-9924-9 ↗
8. Tribological Behavior of MoSi2 and Its Composites in Sliding Against Ni-Based Alloys10.1023/B:TRIL.0000009712.77946.55 ↗
9. Effect of MoSi2 content on the lubricated sliding-wear resistance of ZrC–MoSi2 composites10.1016/j.jeurceramsoc.2010.11.017 ↗
10. Tribological behaviour and wear resistance of a SiC–MoSi2 composite dry sliding against Al2O310.1016/j.wear.2010.04.021 ↗
11. Key issues of MoSi2-UHTC ceramics for ultra high temperature heating element applications: Mechanical, electrical, oxidation and thermal shock behaviors10.1016/j.jallcom.2018.11.384 ↗
12. Effect of microstructure on oxidation resistance of MoSi2 fabricated by spark plasma sintering10.1016/j.vacuum.2003.12.081 ↗
13. Better ceramics through colloid chemistry10.1016/j.jeurceramsoc.2019.10.014 ↗
14. Microstructure dependent physical and mechanical properties of spark plasma sintered ZrB2-MoSi2–SiCw composites10.1016/j.ijrmhm.2018.11.017 ↗
15. Microstructure and mechanical properties of 4YTZP-SiC composites obtained through colloidal processing and Spark Plasma Sintering10.1016/j.bsecv.2020.01.014 ↗
16. ASTM C373-88 · 1988
17. ASTM E384–17 · 2017
18. Evaluation ofK Ic of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
19. ASTM G99–17 · 2020
20. Handbook of contact mechanics: exact solutions of axisymmetric contact problems
21. Ductile-to-brittle transition in MoSi2
22. Mechanical and electrical properties of MoSi2-based ceramics with various ZrB2-20 vol% SiC as additives for ultra high temperature heating element10.1016/j.ceramint.2017.10.043 ↗
23. Microstructural design of sliding-wear-resistant liquid-phase-sintered SiC: an overview10.1016/j.jeurceramsoc.2007.02.190 ↗
24. Influence of flash temperatures on the tribological behaviour in low-speed sliding: a review10.1016/j.msea.2004.03.031 ↗
25. Effect of particle hardness on mild–severe wear transition of hard second phase materials10.1016/j.wear.2012.12.016 ↗
26. Grain size effect on abrasive wear mechanisms in alumina ceramics10.1016/0043-1648(93)90508-J ↗
27. Fracture, fatigue, and sliding-wear behavior of nanocomposites of alumina and reduced graphene-oxide10.1016/j.actamat.2019.12.035 ↗
28. Role of zirconia toughening in the abrasive wear of intermetallic and ceramic composites10.1016/S0043-1648(97)00114-2 ↗
29. Wear and wear transition mechanisms of ceramics10.1016/0043-1648(95)06800-7 ↗
30. Tribological behavior of various plasma-sprayed ceramic coatings10.1016/S0257-8972(96)02918-0 ↗
31. Microstructural, mechanical and tribological properties of finely grained Al2O3 coatings obtained by SPS and S-HVOF methods10.1016/j.surfcoat.2020.126463 ↗