A bi-phasic numerical approach for non-linear response and stiffness recovery related to residual thermal stress in UHTCMCs
Source abstract
Abstract
The tensile properties of sintered Cf-ZrB2/SiC UHTCMCs were investigated for different lamination sequences, revealing ultimate strengths of 570 MPa (0°/0°), 120 MPa (0°/90°), and 40 MPa (90°/90°). The results facilitated modeling the material’s non-linear tensile response, characterized by a remarkably prolonged plateau with pseudo-plastic behavior, followed by stiffness recovery before ultimate failure. A simplified analytical model was developed to predict this behavior originated by residual thermal stresses and inelastic phenomena. A complete constitutive law was then developed and implemented in a FE model, utilizing a bi-phasic approach including Drucker-Prager plasticity and orthotropic ductile damage. Two-step analyses were performed, starting with a thermal step to represent the buildup of a self-equilibrating RTS state in the material phases, followed by a mechanical simulation. This demonstrated the model's efficacy in capturing the non-linear response in both homogeneous and cross-ply lay-ups, contributing to advancements in materials engineering and the design of UHTCMCs-based hot structures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Qualification and reusability of long and short fibre-reinforced ultra-refractory composites for aerospace thermal protection systems10.1016/j.corsci.2021.109955 ↗
2. Cost estimating of commercial smallsat launch vehicles10.1016/j.actaastro.2018.11.054 ↗
3. Operational limits for reusable space transportation systems due to physical boundaries of C/SiC materials10.1016/S1270-9638(03)00054-3 ↗
4. On-orbit service (OOS) of spacecraft: A review of engineering developments10.1016/j.paerosci.2019.01.004 ↗
5. 3D microstructure characterization of 2D Cf-ZrB2-SiC ultra-high temperature ceramic matrix composites using X-ray microscopy10.1016/j.ceramint.2023.11.183 ↗
6. Enhanced fracture properties of continuous Cf/ZrB2-based composites with polydopamine-derived carbon boundary layer
7. Local indentation response of carbon fibers embedded in a harsh environment: The sintered ultra-high temperature ceramic matrix
8. Long-term oxidation and ablation behavior of Cf/ZrB2–SiC composites at 1500, 2000, and 2200°C10.1111/ijac.14299 ↗
9. Temperature-dependent oxidation kinetics and mechanical properties degradation of Cf/ZrB2-SiC composites
10. Effects of multilayer hydrothermal carbon interphases on mechanical properties and thermal shock resistance of CF/ZrB2-SiCBN10.1016/j.jeurceramsoc.2022.05.029 ↗
11. Characterization of carbon fiber-reinforced ultra-high temperature ceramic matrix composites fabricated via Zr-Ti alloy melt infiltration10.1016/j.jeurceramsoc.2022.06.040 ↗
12. A systematic approach for horizontal and vertical scale up of sintered Ultra-High Temperature Ceramic Matrix Composites for aerospace – Advances and perspectives10.1016/j.compositesb.2022.109709 ↗
13. Retained strength of UHTCMCs after oxidation at 2278 K
14. Insight into microstructure and flexural strength of ultra-high temperature ceramics enriched SICARBON™ composite10.1016/j.matdes.2021.109888 ↗
15. Ablation behavior and mechanisms of 3D Cf/ZrB2-SiC composite applied in long-term temperature up to 2400 °C10.1016/j.corsci.2021.109706 ↗
16. Advances in ultra-high temperature ceramics, composites, and coatings
17. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs–a review10.1080/09506608.2019.1652006 ↗
18. Processing of fiber-reinforced ultra-high temperature ceramic composites: a review10.1002/ces2.10033 ↗
19. Long-term ablation behavior and mechanisms of 2D-Cf/ZrB2-SiC composites at temperatures up to 2400 °C10.1016/j.corsci.2020.108967 ↗
20. Oxidation behavior and ablation mechanism of Cf/ZrB2-SiC composite fabricated by vibration-assisted slurry impregnation combined with low-temperature hot pressing10.1016/j.corsci.2019.108181 ↗
21. Disclosing residual thermal stresses in UHT fibre-reinforced ceramic composites and their effect on mechanical behaviour and damage evolution10.1016/j.compositesb.2022.110369 ↗
22. Elevated temperature tensile and bending strength of ultra-high temperature ceramic matrix composites obtained by different processes10.1016/j.jeurceramsoc.2023.03.055 ↗
23. Development of damage in a 2D woven C/SiC composite under mechanical loading: I. Mechanical characterization10.1016/S0266-3538(96)00094-2 ↗
24. Cyclic loading of a SiC-fiber reinforced ceramic matrix composite reveals damage mechanisms and thermal residual stress state10.1016/j.compositesa.2012.06.011 ↗
25. Chemical reactions and thermal stress induced microstructure evolution in 2D-Cf/ZrB2-SiC composites10.1016/j.jmst.2020.12.054 ↗
26. Propulsion tests on ultra-high-temperature ceramic matrix composites for reusable rocket nozzles10.26599/JAC.2023.9220759 ↗
27. Study on toughening mechanisms of pyrolytic carbon interface layer in Cf/ZrB2-SiC composites using in-situ tensile experimental and numerical methods
28. Off-axis damage tolerance of fiber-reinforced composites for aerospace systems10.1016/j.jeurceramsoc.2019.12.038 ↗
29. Impact of residual stress on thermal damage accumulation, and Young’s modulus of fiber-reinforced ultra-high temperature ceramics10.1016/j.matdes.2018.10.019 ↗
30. A binary model of textile composites—I. Formulation10.1016/0956-7151(94)90479-0 ↗
31. A binary model of textile composites--II. The elastic regime10.1016/0956-7151(95)00057-3 ↗
32. Evaluation of Macroscopic and Local Strains in a Three-Dimensional Woven C/SiC Composite10.1111/j.1551-2916.2005.00156.x ↗
33. Treating matrix nonlinearity in the binary model formulation for 3D ceramic composite structures10.1016/j.compositesa.2009.10.020 ↗
34. A bi-phasic modelling approach for interlaminar and intralaminar damage in the matrix of composite laminates10.1016/j.compstruct.2019.111747 ↗
35. Is spark plasma sintering suitable for the densification of continuous carbon fibre - UHTCMCs?10.1016/j.jeurceramsoc.2019.12.004 ↗
36. Effect of PAN-based and pitch-based carbon fibres on microstructure and properties of continuous Cf/ZrB2-SiC UHTCMCs10.1016/j.jeurceramsoc.2020.05.032 ↗
37. Tough salami-inspired Cf/ZrB2 UHTCMCs produced by electrophoretic deposition10.1016/j.jeurceramsoc.2017.09.047 ↗
38. In-plane thermal expansion behavior of M55J carbon fiber reinforced SiC matrix composite
39. In-plane thermal expansion behavior of dense ceramic matrix composites containing SiBC matrix10.1016/j.jeurceramsoc.2020.03.006 ↗
40. Measurement and calculation of thermal residual stress in fiber reinforced ceramic matrix composites10.1016/j.compscitech.2008.08.015 ↗
41. Residual stress-related common intersection points in the mechanical behavior of ceramic matrix composites undergoing cyclic loading10.1007/s11340-012-9709-y ↗
42. Strength evolution of cyclic loaded LSI-based C/C-SiC composites10.1016/j.ceramint.2016.06.061 ↗
43. Fibre-matrix interphases and interfaces in ceramic matrix composites processed by CVI10.1163/156855493X00112 ↗
44. Preparation of C/SiC Composites by Hot Pressing, Using Different C Fiber Content as Reinforcement10.1111/j.1551-2916.2005.00872.x ↗
45. Modeling of residual stress-induced stress–strain behavior of unidirectional brittle fiber/brittle matrix composite with weak interface10.1016/S0266-3538(03)00015-0 ↗
46. On the thermal shock resistance and mechanical properties of novel unidirectional UHTCMCs for extreme environments10.1038/s41598-018-27328-x ↗