Abstract

Abstract Tensile fracture properties of directionally solidified chromia-doped c -axis sapphire fibers have been studied in a range of temperature (room temperature up to 1400 °C) and dopant content (0, 300 ppm and 1% of Cr 2 O 3 ). Delayed failure of the fibers was studied by measuring the dependence of the tensile strength on the loading rate and by fractographic studies on the fracture surfaces of the fibers. In all the temperature range, the fibers doped with 300 ppm of Cr 2 O 3 are slightly stronger than the pure sapphire fibers. The least strong fibers are those containing 1% of Cr 2 O 3 . For this badge of material, the beneficial effect of solution hardening is counterweighted by increasing amount of defects caused by a faster fabrication. Slow crack growth appears to be the process controlling delayed failure at higher temperature. Little contribution of slow crack growth to delayed failure is found at the lower temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · Textile materials and evaluations · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Haggerty, S., Growth of titanium and chromium strengthened sapphire fibers. Technical Report AFML-TR-73-2. Air Force Materials Laboratory, WPAFB, OH, 1972.
2. Crane, R. L., An investigation of the mechanical properties of silicon carbide and sapphire filaments. Technical Report AFML-TR-72-180. Air Force Materials Laboratory, WPAFB, OH, 1972.10.21236/AD0753711 ↗
3. Sayir, H., Farmer, S. C., Lagerlof, K. P. D. and Sayir, A., Temperature dependent fracture strength of doped single-crystal alumina fibers. In Advances in Ceramic-Matrix Composites II, ed. J. P. Singh and N. P. Bansal, pp. 53–63. Ceramic Transactions, Vol 46. The American Ceramic Society, Westerville, OH, 1994.
4. Slow crack growth in sapphire fibers at 800° to 1500°C10.1111/j.1151-2916.1993.tb03973.x ↗
5. Sayir, A., Time dependent strength of sapphire fibers at high temperatures. In Advanced Ceramic-Matrix Composites, ed. N. P. Bansal, pp. 691–703. Ceramic Transactions, Vol 38. The American Ceramic Society, Westerville, OH, 1993.
6. Heydt, P. E., Tressler, R. E. and Sayir, A., Delayed failure of Cr3+-doped sapphire fibers. In Advances in Ceramic-Matrix Composites III, ed. N. P. Bansal and J. P. Singh, pp. 67–75. Ceramic Transactions, Vol 74. The American Ceramic Society, Westerville, OH, 1996.
7. McClellan, K. J., Sayir, H., Heuer, A. H., Sayir, A., Haggerty, J. S. and Sigalovsky, J., High-temperature creep-resistant Y2O3-stabilized cubic ZrO2 single-crystal fibers. In Advances in Ceramic-Matrix Composites II, ed. J. P. Singh and N. P. Bansal, pp. 63–73. Ceramic Transactions, Vol 46. The American Ceramic Society, Westerville, OH, 1994.
8. High-temperature creep deformation of directionally solidified Al2O3/Er3Al5O1210.1016/S1359-6454(02)00571-2 ↗
9. Wachtman · 1996
10. High-temperature mechanical properties of directionally solidify Cr3+ sapphire fibers
11. The mechanical properties of impurity-doped alumina single crystal
12. Pletka, M. L., Mitchell, T. E. and Heuer, A. H., Strengthening mechanisms in sapphire. In Fracture Mechanics of Ceramics (Vol 2), ed. R. Bradt et al. Plenum Press, New York, 1974, pp. 181–194.10.1007/978-1-4613-4431-5_8 ↗
13. Review of solid-solution hardening10.1007/BF00356192 ↗
14. Barsoum · 1997
15. System grows single-srystal fiber
16. Phase diagrams Al2O3–Cr2O310.6028/jres.006.059 ↗
17. CRC Handbook of Materials Science (Vol I), ed. C. T. Lynch. CRC Press, 1986.
18. Indication of chromium-oxide hydroxide evaporation during oxidation of 304L at 873K in the presence of 10-percent water-vapor10.1023/A:1018875024306 ↗
19. Growth of controlled profile crystals from the melt. Part II: Edge-defined, film-fed growth10.1016/0025-5408(71)90007-9 ↗
20. Heydt, P. E., Master Thesis. Pennsylvania State University, 1996.
21. Quispe Cancapa, J. J., de Arellano Lopez, A. R. and Sayir, A., Room- and high-temperature tensile fracture of directionally solidified chromia-doped sapphire fibers. Ceram. Eng. Sci. Proc., 2003, 24, 135–142.10.1002/9780470294826.ch20 ↗
22. Quispe Cancapa, J. J., Master Thesis. Universidad de Sevilla, 2002.
23. Kotchick, D. M., Ph.D. Thesis, Pennsylvania State University, 1978.
24. Rice, R. W, Fractography of Glasses and Ceramics, ed. J. R. Varner and V. D. Frechette. Adv. Ceram., 1986, 22, 3–56.
25. Comment of creep deformation of 0° sapphire10.1111/j.1151-2916.1977.tb15512.x ↗
26. Brittleness dependence of crack branching in ceramics10.1111/j.1151-2916.1986.tb04743.x ↗
27. Creep deformation of 0° sapphire10.1111/j.1151-2916.1976.tb09379.x ↗
28. Solution hardening—a comparison of two models10.1016/S0921-5093(00)01721-4 ↗
29. Wiederhorn, S. E., Fracture Mechanics of Ceramics (Vol 2), ed. R. Bradt et al. Plenum Press, New York, 1974, pp. 613–646.10.1007/978-1-4615-7014-1_12 ↗
30. A diffusive crack-growth model for creep fracture10.1111/j.1151-2916.1982.tb10365.x ↗
32. Lattice trapping of fracture cracks10.1063/1.1660699 ↗
33. Basal slip in sapphire (α-Al2O3)10.1016/S0921-5093(97)00056-7 ↗