journal article·2003-12

Long term oxidation of a SiC fiber-bonded composite in air at 1500 °C

Akihiko Otsuka, Yoshikazu Matsumura, Kazuya Hosono, Ryohei Tanaka

Publisher page

Abstract

Abstract The oxidation behavior of the SiC fiber-bonded composite (Tyrannohex™) was investigated at 1500 °C up to 4000 h in air. During heating of the samples, it was observed that an amorphous SiO 2 scale was formed and that bubbles of SiO 2 were generated due to the gaseous products upon oxidation. A large mass loss was also observed after 4000 h heating in spite of the condition of passive oxidation for SiC. The cause of large mass loss can be explained by destruction of oxidation protective scale due to bursting of the bubbles, and high oxidation rate due to high oxygen mobility in amorphous SiO 2 scale containing aluminum ions. To prevent this accelerated oxidation of the composite, a double-layered coating using a CVD-SiC process was developed. Although the samples coated with CVD-SiC were stable in this oxidation test, the cristobalite peaks observed by XRD suggest also an inherent problem of the SiO 2 scale spalling.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Synthesis of continuous SiC fibers with high tensile strength10.1111/j.1151-2916.1976.tb10975.x ↗
2. Conversion mechanisms of a polycarbosilane precursor into an SiC-based ceramic material10.1007/BF00544474 ↗
3. Precursor-derived covalent ceramics10.1002/adma.19950070903 ↗
4. Preceramic polymer routes to silicon carbide10.1021/cm00027a007 ↗
5. Reaction mechanisms of silicon carbide fiber synthesis by heat treatment of polycarbosilane fibers cured by radiation10.1111/j.1151-2916.1995.tb08898.x ↗
6. A model SiC-based fibre with low oxygen content prepared from a polycarbosilane precursor10.1023/A:1018597432067 ↗
7. High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C10.1038/35820 ↗
8. Ishikawa, T., Kajii, S., Hisayuki, T. and Kohtoku, Y., SiC polycrystalline fiber and the fiber-bonded ceramic. In Proceedings of the 6th Japan International SAMPE Symposium, ed. T. Tanimoto and T. Mori, Tokyo, 1999, 1, pp. 253–256.
9. The effects of an aggressive environment on subcritical crack growth of a continuous-fiber ceramic composites
10. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials10.1111/j.1151-2916.1994.tb07015.x ↗
11. Oxidation of the carbon interface in nicalon-fiber-reinforced silicon carbide composite10.1111/j.1151-2916.1997.tb02868.x ↗
12. Stress-rupture of nicalon/SiC continuous fiber ceramic composites in air at 950 °C10.1111/j.1151-2916.1997.tb03266.x ↗
13. Tensile stress rupture of SiCf/SiCm minicomposites with carbon and boron nitride interfaces at elevated temperatures in air10.1111/j.1151-2916.1997.tb03087.x ↗
14. A multi-layer CVD-SiC coating for oxidation protection of carbon/carbon composite
15. Improvement in oxidation resistance of a C/C composite by using CVD-SiC coating with SiC fiber-composite layer
16. Evidence for calcium and aluminum diffusion in SiO2 glass10.1111/j.1151-2916.1969.tb15855.x ↗
17. The mullite-corundum boundary in the systems MgO–Al2O3–SiO2 and CaO–Al2O3–SiO210.1111/j.1151-2916.1959.tb13589.x ↗