Grain boundary corrosion of highly porous ceramic TiO 2 foams is reduced by annealing and quenching
Source abstract
Abstract
Abstract Porous bioceramics, such as scaffolds, can be used for bone regeneration. Bioceramics are instantly attacked by body fluids, macrophages and osteoclasts during stages of bone repair. Acidic microenvironments generated by these cells may amplify the well-known effect of grain boundary dissolution. Grain boundary corrosion in such porous scaffolds can have significant impact on the mechanical strength due to the high surface area of the scaffold. Corrosive media were found to significantly affect the mechanical strength of highly porous TiO2 scaffolds. Compressive strength decreased significantly after 12 h in an aqueous acidic solution with a reduction to 35 ± 10% after 8 weeks immersion time. Following post-sintering heat treatments by combining air quenching and annealing, the strength was maintained throughout a corrosion period of 8 weeks in acidic environment. Impurity segregation to the grain boundaries and thus, susceptibility to grain boundary corrosion was reduced by the synergistic effect of both heat treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Ceramic TiO2-foams: characterisation of a potential scaffold10.1016/S0955-2219(03)00255-3 ↗
2. Ultra-porous titanium oxide scaffold with high compressive strength10.1007/s10856-010-4142-1 ↗
3. Bone formation in TiO2 bone scaffolds in extraction sockets of minipigs10.1016/j.actbio.2012.02.020 ↗
4. Bone resorption by osteoclasts10.1126/science.289.5484.1504 ↗
5. The influence of dissolved calcium salts on the degradation of hard-tissue collagens by lysosomal cathepsins10.1016/S0174-173X(87)80009-2 ↗
6. Microelectrode studies on the acid microenvironment beneath adherent macrophages and osteoclasts10.1016/0014-4827(88)90191-7 ↗
7. Fracture repair
8. Microstructure design of HIPed TiO2 ceramics for improved corrosion resistance10.1023/A:1018568101522 ↗
9. Corrosion of ceramics in aqueous hydrofluoric acid10.1111/j.1151-2916.2000.tb01348.x ↗
10. Corrosion behavior of alumina ceramics in aqueous HCl and H2SO4 solutions10.1016/j.corsci.2007.10.008 ↗
11. Devitrification of the grain boundary glassy phase in a high-alumina ceramic substrate10.1111/j.1151-2916.1994.tb04647.x ↗
12. Grain boundary chemistry of alumina by high-resolution imaging SIMS10.1016/S1359-6454(99)00263-3 ↗
13. Corrosion behavior of alumina ceramics in caustic alkaline solutions at high temperatures10.1111/j.1151-2916.1991.tb04304.x ↗
14. Microstructure and chemistry of intergranular glassy films in liquid-phase-sintered alumina10.1111/j.1151-2916.1998.tb02343.x ↗
15. Structure and composition of grain boundaries in ceramics10.1016/S0955-2219(98)00294-5 ↗
16. Corrosion of alumina ceramics in acidic aqueous solutions at high temperatures and pressures10.1023/A:1026714218522 ↗
17. Microstructure of 96% alumina ceramics: III, crystallization of high-calcia boundary glasses10.1111/j.1151-2916.1990.tb04276.x ↗
18. Dissolution kinetics of crystalline and amorphous silica in hydrofluoric-hydrochloric acid mixtures10.1111/j.1151-2916.1987.tb05708.x ↗
19. Theory of corrosion of glass and ceramics
20. Bisen · 2014
21. How useful is SBF in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
22. Pelleg · 2014 · 351
23. Effect of microstructure on toughness and strength
24. Creep and fracture of a vitreous-bonded aluminium oxide10.1007/BF01117359 ↗
25. Grain- boundaries in polycrystalline ceramics10.1146/annurev.ms.17.080187.000421 ↗
26. Dopant distribution in grain-boundary films in calcia-doped silicon nitride ceramics10.1111/j.1151-2916.1998.tb02747.x ↗
27. Structure of grain boundaries in ceramics10.1016/0304-3991(84)90104-9 ↗
28. Solubility and dissolution rate of silica in acid fluoride solutions10.1016/j.gca.2009.08.027 ↗
29. Boon and bane of metal ions in medicine10.1126/science.1083004 ↗
30. A comparative study on the in vivo behavior of hydroxyapatite and silicon substituted hydroxyapatite granules10.1023/A:1021114710076 ↗
31. Silicon: a possible factor in bone calcification10.1126/science.167.3916.279 ↗
32. Influences of ionic dissolution products of dicalcium silicate coating on osteoblastic proliferation, differentiation and gene expression10.1016/j.actbio.2008.10.011 ↗
33. Aluminum stimulates the proliferation and differentiation of osteoblasts in vitro by a mechanism that is different from fluoride10.1007/BF00227749 ↗
34. Effects of metal ions on osteoblast-like cell metabolism and differentiation10.1002/(SICI)1097-4636(199701)34:1<29::AID-JBM5>3.0.CO;2-P ↗
35. Crystallization of small quantities of glass (or a liquid) segregated in grain boundaries10.1016/0001-6160(81)90036-5 ↗
36. Plausible concepts necessary and sufficient for interpretation of ceramic grain-boundary phenomena: II, solute segregation, grain-boundary diffusion, and general discussion10.1111/j.1151-2916.1974.tb10818.x ↗
37. Role of interfacial grain-bridging sliding friction in the crack-resistance and strength properties of nontransforming ceramics10.1016/0001-6160(89)90299-X ↗
38. Methods for improving the mechanical properties of oxide glasses10.1007/BF00544488 ↗
39. Influence of grain size and degree of crystallization of intergranular glassy phase on the mechanical behaviour of a debased alumina10.1007/BF02387741 ↗
40. Carter · 2015
41. Crystallization and structure of a MgO–Al2O3–SiO2–TiO2 glass-ceramic10.1007/BF00550667 ↗
42. Improved flaw tolerance in alumina containing 1 vol% anorthite via crystallization of the intergranular glass10.1111/j.1151-2916.1992.tb07210.x ↗
43. Effect of annealing treatments on microstructure and mechanical properties of liquid-phase-sintered silicon carbide10.1016/S0955-2219(00)00254-5 ↗
44. Influence of powder characteristics on liquid phase sintering of silicon carbide10.2109/jcersj.103.257 ↗
45. Walther · 2009