journal article·2025-11Open access

High-temperature Si-Pr eutectic filler for brazing RBSiC composites: Wettability and bonding mechanisms

Xiaoqian Xue, Fugang Lu, Jia Yang, Yibo Fu, Qianrun Zhang, Tong Wu, Mengchun Fu, Panpan Lin, Ce Wang, Yongkang Dong, Tiesong Lin, Zhanguo Liu, Peng He

Abstract

This study investigates the brazing of Si-Pr eutectic filler with Reaction-bonded Silicon Carbide (RBSiC), offering a comprehensive analysis of the wetting mechanism, microstructural evolution , mechanical properties, and fracture behavior of the joints . The results demonstrate that the Si-Pr eutectic filler achieves exceptional wettability with RBSiC, with no new phases formed at the interface, indicating stable and reliable interfacial interactions . Notably, the joint shear strength reaches 62.6 MPa at 1290 °C, with fracture occurring within the substrate, highlighting the superior mechanical properties of the brazed joints . The bonding mechanism involves Si adsorption and atomic bond formation facilitated by the diffusion of the filler and interface reconstruction. This work not only enhances our understanding of Si-Pr eutectic brazing alloys but also provides valuable insights for advancing composite material joining technologies, paving the way for more robust and efficient material connections in high-performance applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. 1300°C–1900 °C heat treatment and mechanical properties optimization of RB-SiC ceramics10.1016/j.ceramint.2023.12.338 ↗
2. Microstructure and mechanical-properties of reaction-formed silicon-carbide (RFSiC) ceramics10.1016/0921-5093(94)90346-8 ↗
3. Key parameters in the manufacture of SiC-based composite materials by reactive melt infiltration10.3390/ma12152425 ↗
4. Progress in tribological research of SiC ceramics in unlubricated sliding-a review10.1016/j.matdes.2020.108528 ↗
5. Nanomechanical characterization of RB-SiC ceramics based on nanoindentation and modelling of the ground surface roughness10.1016/j.ceramint.2019.11.094 ↗
6. High efficiency abrasive waterjet dressing of diamond grinding wheel10.4028/www.scientific.net/AMR.1017.243 ↗
7. Subsurface deformation and crack propagation between 3C -SiC/6H-SiC interface by applying in-situ laser-assisted diamond cutting RB-SiC10.1016/j.matlet.2023.133878 ↗
8. Advances in modifications and high-temperature applications of silicon carbide ceramic matrix composites in aerospace: a focused review10.1016/j.jeurceramsoc.2021.03.051 ↗
9. Radiation effects in SiC for nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
10. Additive manufacturing of silicon carbide for nuclear applications10.1016/j.jnucmat.2020.152577 ↗
11. Review of silicon carbide power devices and their applications10.1109/TIE.2017.2652401 ↗
12. Mechanical and tribological properties of electrically conductive SiC based cermets10.1016/j.ijrmhm.2016.12.017 ↗
13. Vat photopolymerization-based additive manufacturing of high-strength RB-SiC ceramics by introducing quasi-spherical diamond10.1016/j.jeurceramsoc.2023.05.016 ↗
14. A comprehensive review of the photopolymerization of ceramic resins used in stereolithography
15. Pressureless joining of SiC by molten Si infiltration to the SiC/C filler tape and residual stress analysis10.1016/j.jeurceramsoc.2023.11.021 ↗
16. Development of SiC-SiC joint by reaction bonding method using SiC/C tapes as the interlayer10.1016/j.jeurceramsoc.2012.04.049 ↗
17. Ablation behavior and mechanism of (PyC-Csf)/ZrB2-SiC-ZrC ceramics sintered by reactive spark plasma sintering at low temperature10.1016/j.corsci.2024.111873 ↗
18. A heat-resistant preceramic polymer with broad working temperature range for silicon carbide joining10.1016/j.jeurceramsoc.2017.08.033 ↗
19. Reaction mechanism and mechanical properties of a SiCf/SiC joint affected by Cu/Ni/Ti elements and inhomogeneous composites10.1016/j.jeurceramsoc.2023.10.049 ↗
20. Joining of ceramics demonstrated by the example of SiC/Ti10.1016/0955-2219(90)90012-5 ↗
21. Solid-state joining of SiC using a thin Ti3AlC2, TiC, or Ti filler10.1016/j.jeurceramsoc.2019.09.031 ↗
22. Ceramic–metal composites for heat exchangers in concentrated solar power plants10.1038/s41586-018-0593-1 ↗
23. Solid state reactions between SiC and Ir10.1016/j.jeurceramsoc.2019.06.009 ↗
24. Survey on wetting of SiC by molten metals10.1016/j.ceramint.2010.01.001 ↗
25. Wetting and interfacial behavior of Ni-Si alloy on different substrates10.1007/s10853-009-3858-0 ↗
26. Towards optimization of SiC/CoSi2 composite material manufacture via reactive infiltration: wetting study of Si–Co alloys on carbon materials10.1016/j.jeurceramsoc.2015.07.016 ↗
27. Eutectoid transformations in Fe-Si alloys for thermoelectric applications10.1016/j.jallcom.2017.06.023 ↗
28. The wettability of silicon carbide by Au-Si alloys10.1016/S0921-5093(97)00718-1 ↗
29. Bonding and wetting in non-reactive metal/SiC systems: weak or strong interfaces10.1016/S0921-5093(99)00274-9 ↗
30. Studies of the joining-relevant interfacial properties in the Si-Ti/C and Si-Ti/SiC systems10.1007/s11665-020-04655-7 ↗
31. Design of refractory SiC/ZrSi2 composites: Wettability and spreading behavior of liquid Si-10Zr alloy in contact with SiC at high temperatures10.1016/j.jeurceramsoc.2019.12.027 ↗
32. Pr-Si Binary Phase Diagram 0-100 at% Si: Datasheet from "PAULING FILE Multinaries Edition – 2022" in SpringerMaterials (〈https://materials.springer.com/isp/phase-diagram/docs/c_0905747〉).
33. Competitive growth of Si and YSi2 phases in a eutectic Si-Y alloy prepared by the Bridgeman method10.1016/j.ceramint.2018.04.150 ↗
34. Reactive infiltration of porous graphite by NiSi alloys10.1016/j.actamat.2008.01.011 ↗
35. The role of the chemical reaction in the infiltration of porous carbon by NiSi alloys10.1016/j.scriptamat.2006.02.015 ↗
36. Fundamental issues of reactive wetting by liquid metals10.1007/s10853-009-4128-x ↗
37. Wetting and spreading behavior of liquid Si-Ti eutectic alloy in contact with glassy carbon and SiC at T = 1450 °C10.1007/s11661-019-05382-y ↗
38. Wetting behavior and reactivity of liquid Si-10Zr alloy in contact with glassy carbon10.1016/j.jallcom.2020.153643 ↗
39. Wetting of ceramics by molten silicon and silicon alloys: a review10.1007/s10853-012-6663-0 ↗
40. Atomic Mechanism of Diffusion
41. SiC-IrSi 3 for high oxidation resistance
42. New advanced SiC-based composite materials for use in highly oxidizing environments: synthesis of SiC/IrSi310.1016/j.jeurceramsoc.2019.10.018 ↗
43. Thermodynamic descriptions of the light rare-earth elements in silicon carbide ceramics10.1111/jace.17031 ↗
44. Brazing of AlN to SiC by a Pr silicide: physicochemical aspects10.1016/j.msea.2007.11.092 ↗