Effect of composition and annealing temperature on the mechanical properties of a vitrified waste
Source abstract
Abstract
The microhardness and indentation fracture toughness of a vitrified industrial waste, in the form of ash, were characterized by the method of static indentation test. These properties were investigated as a function of composition and thermal treatment conditions. To further understand the influence of the constitutive oxides, additional measurements were made in a series of synthetic products, where a mixture of iron and lead oxides was used as a substitute for the ash. The underlying deformation mechanisms controlling the mechanical properties of such complex systems as determined by static indentation tests are discussed. It was found that plasticity, in the amorphous products, is mainly governed from the silica content, even in the cases where silica is not found in sufficient quantity in order to build an extended three-dimensional vitreous network. On the other hand, the morphology of the separated crystalline phases is the dominant factor affecting plasticity in the glass-ceramic products.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Glass properties and applications · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. LaGrega · 2001
2. Nazaroff · 2001
3. Corbitt · 1999
4. Characterization of a glass-ceramic produced from thermal power plant fly ashes10.1016/S0955-2219(00)00099-6 ↗
5. Crystallization behaviour of glasses produced from fly ashes10.1016/S0955-2219(01)00221-7 ↗
6. Relaxation in liquids, polymers and plastic crystals—strong/fragile patterns and problems10.1016/0022-3093(91)90266-9 ↗
7. Microhardness of phosphate glasses10.1016/0022-3093(94)90134-1 ↗
8. Brittleness of glass10.1016/S0022-3093(99)00348-8 ↗
9. Indentation of glass as a function of temperature10.1016/S0022-3093(00)00113-7 ↗
10. The brittle to ductile transition in a soda–lime–silica glass10.1016/S0022-3093(00)00109-5 ↗
11. Change in Vickers hardness at the glass transition region for fragile and strong glasses10.1016/S0022-3093(01)00521-X ↗
12. Vitrification of lead-rich solid ashes from incineration of hazardous industrial wastes10.1016/S0956-053X(02)00153-8 ↗
13. The crystallization kinetics of iron rich glass in different atmospheres10.1016/S0955-2219(00)00077-7 ↗
14. Iron-rich sintered glass-ceramics from industrial wastes10.1111/j.1151-2916.1999.tb02195.x ↗
15. Structural role of lead in lead silicate glasses derived from XPS spectra10.1016/0022-3093(95)00471-8 ↗
16. An XPS study of iron sodium silicate glass surfaces10.1016/S0022-3093(96)00523-6 ↗
17. Changes of the mechanical properties during the crystallization of bio-active glass–ceramics10.1023/A:1004855516457 ↗
18. Microstructural changes of processed vitrified solid waste products10.1016/S0955-2219(02)00289-3 ↗
19. Anderson · 1990
20. Shelby · 1997
21. Chemical durability of glasses obtained by vitrification of industrial wastes10.1016/S0956-053X(00)00077-5 ↗
22. Interpretation of the indentation size effect in Vickers microhardness measurements—absolute hardness of materials10.1016/0040-6090(89)90505-1 ↗
23. An explanation of the indentation size effect in ceramics10.1080/09500838908206356 ↗
24. A critical evaluation of indentation techniques for determining fracture toughness10.1111/j.1151-2916.1981.tb10320.x ↗
25. Amin, K. A. In Engineered Materials Handbook: Ceramics and Glasses, ed. S. J. Schneider Jr. ASM International, 2000, pp. 599–601.
26. A simple method for determining elastic-modulus-to-hardness ratios using Knoop indentation measurements10.1111/j.1151-2916.1982.tb10357.x ↗
27. Kavouras, P., Powder Processing for the Fabrication of Composite Materials for Technological Applications. PhD thesis, Aristotle University, Thessaloniki, 2003.
28. Doremus · 1994
29. The effect of indentation-induced cracking on the apparent microhardness10.1007/BF00352908 ↗
30. Microstructural dependence of relevant physical–mechanical properties on SiO2–Na2O–CaO–P2O5 biological glasses10.1016/S0142-9612(02)00189-8 ↗
31. Hardness and elastic properties of Bi2O3-based glasses10.1023/A:1017973830342 ↗
32. Indentation deformation and fracture toughness of densified silicate glass10.1007/BF00369689 ↗
33. Densification of magnesium and calsium metaphosphate glasses10.1016/0022-3093(91)90158-3 ↗
34. Effect of contact residual stress relaxation on fracture strength of indented soda–lime glass10.1111/j.1151-2916.1985.tb16167.x ↗
35. Flaw characteristics in dynamic fatigue10.1111/j.1151-2916.1980.tb10759.x ↗
36. Theory of fatigue for brittle flaws originating from residual stress concentrations10.1111/j.1151-2916.1983.tb10039.x ↗
37. Fracture toughness measurement of glass and ceramic materials using chevron-notched specimens10.1111/j.1151-2916.1988.tb05911.x ↗
38. Reliability of the chevron-notch technique for fracture toughness determination in glass10.1016/S0921-5093(02)00612-3 ↗