Conductivity of La0.95Sr0.05Ga0.90Mg0.10O3−δ obtained by mechanical activation
Source abstract
Abstract
Abstract Dense ceramics of La 0.95 Sr 0.05 Ga 0.90 Mg 0.10 O 3− δ (LSGM) were obtained from La 2 O 3 , SrO, Ga 2 O 3 and MgO precursors activated by dry grinding in a high-energy planetary ball-mill. Samples sintered at 1450 °C for 4 h have an average grain size of ca. 250 nm. This value increases to 5 μm when the sample is annealed for 40 h at the same temperature. Samples prepared by a conventional ceramic route were also obtained with a grain size of 13.5 and 20.5 μm, after sintering at 1550 °C for 4 and 40 h, respectively. Impedance spectroscopy data revealed similar grain conductivities for both materials. However, a significant degradation was observed on ageing the LSGM prepared by the conventional ceramic route, probably due to compositional alterations at the grain boundaries. This degradation was not present in the material prepared from mechanically activated precursors. Grain size effects on the electrical conductivity were analysed to determine the effective grain boundary conductivity and the brick-layer model is assumed to estimate the grain boundary thickness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. A superior oxide-ion electrolyte
2. Doped LaGaO3 perovskite type oxide as a new oxide ionic conductor10.1021/ja00088a016 ↗
3. Superior oxygen ion conductivity of lanthanum gallate doped with strontium and magnesium10.1149/1.1836692 ↗
4. Superior perovskite oxide-ion conductor; strontium- and magnesium-doped LaGaO3. II. ac Impedance spectroscopy10.1111/j.1151-2916.1998.tb02663.x ↗
5. The effect of doping and processing conditions on properties of La1−xSrxGa1−yMgyO310.1016/S0955-2219(01)00203-5 ↗
6. Chemical preparation of pure and strontium and/or magnesium-doped lanthanum gallate powders10.1111/j.1151-2916.2000.tb01666.x ↗
7. Formation of CaTiO3 by grinding from mixtures of CaO or Ca(OH)2 with anatase or rutile at room temperature10.1016/S0032-5910(98)00012-6 ↗
8. Mechanochemical synthesis of lanthanum aluminate by grinding lanthanum oxide with transition alumina10.1111/j.1151-2916.2000.tb01215.x ↗
9. Piezoelectric PMN-PT ceramics from mechanochemically activated precursors10.1016/S0955-2219(03)00598-3 ↗
10. Anderwood · 1970
11. Average grain size in polycrystalline ceramics10.1111/j.1151-2916.1969.tb11975.x ↗
12. Dopant substitution and ion migration in the LaGaO3-based oxygen ion conductor10.1021/jp972819d ↗
13. Conductivity of CGO and CSO ceramics obtained from freeze-dried precursors10.1016/S0013-4686(03)00027-6 ↗