journal article·2006-01

Reclamation of used SiC grinding powder and its sintering characteristics

Ningfeng Gao, Koji Watari, Shoichi Kume, Yukari Ando, Sasai Ryo, Hideaki Itoh

Publisher page

Abstract

Abstract A process of recycling used abrasive SiC powder after grinding Si wafer was proposed to raw powder for sintering. The used SiC powder could be successfully converted to composite powders consisting of SiC particle and Si 3 N 4 whisker via a heat treatment in N 2 atmosphere, in which iron oxide acted as a catalyst in the vapor–liquid–solid (VLS) formation of Si 3 N 4 . With the addition of 3 mass% Al 2 O 3 and 1 mass% Y 2 O 3 , the composite powders sintered at 1900 °C for 2 h exhibited a 3-point bending strength of 626 ± 48 MPa and a fracture toughness of 3.9 ± 0.1 MPa m 1/2 , which were significantly enhanced as compared with those of using recovered powder merely composed of SiC particle. The strength and fracture toughness of the sintered material could be improved by optimization of chemical and heat treatment parameters and controlling the amount of sintering additives and hot pressing conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Suzuki · 2001
2. New refractories made from reused silicon carbide10.2109/jcersj.112.428 ↗
3. Industrial trend and statistics of artificial abrasives
4. Recycling of used abrasive powder of SiC by hydrothermal treatment
5. Effects of whisker distribution and sintering temperature on friction and wear of Si3N4-whisker-reinforced Si3N4-composites10.1016/S0043-1648(99)00058-7 ↗
6. Alloy phase diagrams
7. The assessment of thermodynamic parameters in the Fe–O and Fe–Si–O systems10.1016/S0016-7037(97)00256-1 ↗
8. Crystal growth of silicon nitride whiskers through a VLS mechanism using SiO2–Al2O3–Y2O3 oxides as liquid phase10.1016/S0272-8842(97)00042-4 ↗
9. Production of SiC and Si3N4 whisker in C+SiO2 solid mixtures10.1016/S0254-0584(01)00332-7 ↗
10. A simple method to synthesize Si3N4 and SiO2 nanowires from Si or Si/SiO2 mixture10.1016/S0022-0248(01)01650-5 ↗
11. Low-temperature pressurless sintering of β-silicon carbide with aluminum oxide and yttrium oxide additions
12. Effects of intergranular phase chemistry on the microstructure and mechanical properties of silicon carbide ceramics densified with rare-earth oxide and alumina additions10.1111/j.1151-2916.2001.tb00891.x ↗
13. Formation behavior of multi-cation α-sialons containing calcium and magnesium10.1016/S0167-577X(98)00155-4 ↗
14. Mechanical properties of AlN-polytypoids—15R, 12H and 21R10.1016/S0921-5093(99)00500-6 ↗