journal article·2006-01

Electrophoretic deposition and sintering of zirconia layers on microstructured steel substrates

A. Pfrengle, H. von Both, R. Knitter, J. Haußelt

Publisher page

Abstract

A method is developed to electrophoretically deposit homogeneous zirconia layers with a thickness of about 5 μm on microstructured steel substrates. To realize layers in this range of thickness, the use of fine to submicron zirconia powder is necessary. To determine the electrokinetic behavior of the powder particles during electrophoresis, their electrophoretic mobility (EM) is measured. Special attention is drawn to the dependence of the mobility on particle size, where Henry theory can be applied. After depositing the layer on the substrate, it is sintered at 1000 °C and investigated by optical microscopy and SEM.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrophoretic Deposition in Materials Science · TiO2 Photocatalysis and Solar Cells · Advanced Photocatalysis Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Fabrication of ceramic composite coatings using electrophoretic deposition, reaction bonding and low temperature sintering10.1016/S0955-2219(01)00254-0 ↗
2. Laser processing of yttria stabilised zirconi/alumina coatings on Fecralloy substrates10.1016/j.surfcoat.2004.01.040 ↗
3. Electrophoretic deposition EPD: mechanisms. kinetics and application to ceramics10.1111/j.1151-2916.1996.tb08929.x ↗
4. Müller · 1996
5. Lagaly · 1997
6. Israelachvili · 2000
7. Malvern Instruments, Documentation for Zetasizer 1000/2000/3000: Principles of operation, Manual Number MAN 0152, Issue 1.1, 1996.
8. Modified booth equation for the calculation of zeta potential10.1007/s003960050218 ↗
9. Electrophoretic deposition of aqueous nano-γ-Al2O3 suspensions10.1016/S0025-5408(02)00693-1 ↗
10. The conductivity of aqueous Al2O3 slips for electrophoretic deposition10.1016/0167-577X(96)00075-4 ↗
11. Effect of the slurry properties on the homogeneity of alumina deposits obtained by aqueous electrophoretic deposition10.1016/S0025-5408(00)00288-9 ↗
12. Sintering behavior and grain structure development of ZrO2- and Al2O3-compacts fabricated from different nanosized powders