journal article·2009-08

Reaction of TiC with SiCl4 vapor with formation of SiC–TiC composites

S. Shimada, A. Onuma

Publisher page

Abstract

Abstract The reaction of TiC grains with SiCl 4 vapor was carried out in Ar at 1000–1600 °C to produce TiC–SiC composite powders. The compositions of these powders were controlled by controlling the conversion to SiC, which depends on the reaction temperature. The phases formed by the solid–gas reaction were identified by X-ray analysis (XRD) and the molar ratio of SiC to TiC in the powder was estimated from the area ratios of the respective XRD peaks. The reaction begins at about 1100 °C and its rate increases with temperature to 1600 °C, at which 92% SiC is formed. The morphology of the TiC–SiC composites was observed by scanning electron microscopy and transmission electron microscopy and a reaction mechanism is deduced from the above results and thermodynamic considerations. TiC–SiC composites were densified by spark plasma sintering at 1750 °C and 40 MPa to the relative density 92–96% and a Vickers hardness of 1700–1900 Hv.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. The oxidation of TiC at low temperatures10.1007/BF01107214 ↗
2. Improvements in mechanical properties in SiC by the addition of TiC particles10.1111/j.1151-2916.1984.tb19174.x ↗
3. Effects of initial α-phase content of SiC on microstructure and mechanical properties of SiC–TiC composites10.1016/S0955-2219(00)00160-6 ↗
4. The influence of processing parameters on microstructure and mechanical properties of SiC–TiCp ceramics10.1016/0272-8842(95)99798-G ↗
5. Fabrication and mechanical evaluation of SiC–TiC nanocomposites by SPS10.1016/S0167-577X(03)00434-8 ↗
6. Rapid reactive synthesis and sintering of submicron TiC/SiC composites through spark plasma sintering10.1111/j.1551-2916.2004.01157.x ↗
7. Field assisted sintering of electro-conductive ZrO2-based composites10.1016/j.jeurceramsoc.2006.04.142 ↗
8. Preparation and microstructure of a ZrB2–SiC composite fabricated by the spark plasma sintering-reactive synthesis (SPS-RS) method10.1111/j.1551-2916.2007.02050.x ↗
9. Densification of SiC by SPS-effects of time, temperature and pressure10.1016/j.jeurceramsoc.2006.10.005 ↗
10. Role of impurities on the spark plasma sintering of ZrCx–ZrB2 composites10.1016/j.jeurceramsoc.2007.07.013 ↗
11. Fracture toughness of TiC–SiC composites fabricated by CVD and the mechanism of toughening10.2109/jcersj.100.835 ↗
12. The growth and characterization of CVD SiC–TiC in-situ composites10.1016/S0272-8842(97)00008-4 ↗
13. Effect of CH4 and H2 on CVD of SiC and TiC for possible fabrication of SiC/TiC/C FGM10.1016/S0167-577X(96)00221-2 ↗
14. Microstructure of chemically vapour codeposited SiC–TiC–C nanocomposites10.1016/0921-5093(93)90725-T ↗
15. Growth and stability of CVD codeposited nanocomposite SiC–TiC–C10.1016/0965-9773(94)90080-9 ↗
16. Design, fabrication and properties of layered SiC/TiC ceramic with graded thermal residual stress10.1016/S0955-2219(02)00306-0 ↗
17. Synthesis of β-SiC whiskers from silica black ore10.2109/jcersj.104.992 ↗
18. Hack, H., GTT (Version 4.14) Gtt-Technologies, Germany, 1998.
19. Oxidation of HfC and TiC single crystals with formation of carbon at high temperature and low oxygen pressures10.1111/j.1151-2916.2000.tb01265.x ↗
20. Weak interaction of oxygen with some refractory carbides10.1149/1.1354606 ↗