Abstract

Abstract YBa2Cu3O7−x thin films were deposited by pulsed laser deposition (PLD) using differently preablated targets. The effect of the total number of laser pulses on the morphology and composition of the YBa2Cu3O7−x target was investigated and the induced modification of the irradiated surface was found to affect the characteristics of the produced films. It is shown that both the particle density and the particle size in the prepared c-axis oriented films have been greatly reduced using a target preablated with a low number of pulses. The optimum conditions for the preparation of high quality YBa2Cu3O7−x thin films with reduced particles and high critical current density are established.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Plasma Diagnostics and Applications · Physics of Superconductivity and Magnetism

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Smooth YBa2Cu3O7−x thin films prepared by pulsed laser deposition in O2/Ar atmosphere10.1063/1.111331 ↗
2. Growth of high-Tc thin films10.1088/0953-2048/12/6/202 ↗
3. Particulates on pulsed-laser deposited Y–Ba–Cu–O films10.1016/0921-4534(95)00678-8 ↗
4. Thin-film multilayer interconnect technology for YBa2Cu3O7−x10.1063/1.356469 ↗
5. Off-axis laser deposition of YBa2Cu3O7−x thin films10.1063/1.107951 ↗
6. Laser wavelength dependent properties of YBa2Cu3O7−x thin films deposition by laser ablation10.1063/1.101999 ↗
7. Laser ablated thin films of YBa2Cu3O7−x: the nature and origin of the particulates10.1016/0921-4534(91)90693-S ↗
8. Origin of surface roughness for c-axis oriented Y–Ba–Cu–O superconducting films10.1063/1.104143 ↗
9. Effects of target microstructure on pulsed laser deposited YBa2Cu3O7-thin films10.1016/S0040-6090(99)00717-8 ↗
10. Congruent laser ablation due to pre-irradiation of target10.1016/S0921-4534(00)00327-0 ↗
11. Reduction of droplet emission and target roughening in laser ablation and deposition of metals10.1063/1.354763 ↗
12. Optimization of KrF laser ablation parameters for in-situ growth of YBa2Cu3O7−x10.1016/0921-4534(92)90445-I ↗
13. Crossed fluxes technique for pulsed laser deposition of smooth YBa2Cu3O7−x films and multilayers10.1063/1.110773 ↗
14. Target modification in the excimer laser deposition of YBa2Cu3O7−x10.1063/1.106386 ↗
15. Laser ablation threshold of YBa2Cu3O7−x10.1063/1.112921 ↗
16. Steady state pulsed laser deposition target scanning for improved plume stability and reduced particle density10.1063/1.113261 ↗
17. Synthesis of HTSC Re(Y)Ba2Cu3Ox powders: the role of ionic radius10.1016/S0921-4534(97)01636-5 ↗
18. Processing effect on microstructure and superconducting properties of sintered ReBa2Cu3Oy ceramics—the role of ionic radius10.1016/S0955-2219(00)00074-1 ↗
19. Modelling of the hysteresis loop for YBa2Cu3O7 thin films10.1016/0921-4534(94)02347-6 ↗
20. Influence of target composition on the quality of YBCO films fabricated by Nd:YAG pulsed laser deposition10.1016/S0921-4534(00)01578-1 ↗
21. Deposition angle-dependent morphology of laser deposited YBa2Cu3O7 thin films10.1063/1.112223 ↗
22. Pulsed laser deposition and characterization of high-Tc YBa2Cu3O7−x superconducting thin films10.1016/S0927-796X(97)00019-3 ↗