Fatigue behaviour of mullite studied by the indentation flexure method
Source abstract
Abstract
A systematic study has been performed of the use of the Indentation Flexure Fatigue (IFF) method to study crack growth in mullite at room temperature and high temperature (1300°C). The results obtained for a mullite have been compared with previous data generated on the same material, but using the more direct compact tension method. The material produces transgranular crack growth and consequently does not show R-curve behaviour, which considerably simplifies the comparison of the data generated by both methods. The IFF method can significantly overestimate the crack tip stress intensity factor because of the way in which the residual stress intensity produced by the indentation is estimated. The experimental details that influence the test results were investigated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Effects of water and other dielectrics on crack growth10.1007/BF00752191 ↗
2. Crack propagation and fracture in silicon carbide10.1007/BF00554926 ↗
3. A method for evaluating the time-dependent failure characteristics of brittle materials and its application to polycrystalline alumina10.1007/BF00550196 ↗
4. Influence of water vapour on crack propagation in soda-lime glass10.1111/j.1151-2916.1967.tb15145.x ↗
5. Stress corrosion of ionic and mixed ionic/covalent solids10.1111/j.1151-2916.1986.tb07332.x ↗
6. Cyclic fatigue-crack propagation in magnesia-partially-stabilized zirconia ceramics10.1111/j.1151-2916.1990.tb05132.x ↗
7. Fatigue crack growth from indentation flaw in ceramics10.1007/BF00017822 ↗
8. Controlled surface flaws in hot pressed SiC10.1111/j.1151-2916.1976.tb09381.x ↗
9. Controlled indentation-induced cracks for the determination of fracture toughness in alumina
10. Controlled surface flaws in hot-pressed Si3N410.1111/j.1151-2916.1975.tb19571.x ↗
11. Static and cyclic fatigue behaviour of polycrystalline alumina10.1111/j.1151-2916.1972.tb11260.x ↗
12. Cyclic fatigue crack propagation in alumina under direct tension-compression loading10.1111/j.1151-2916.1989.tb06133.x ↗
13. Crack propagation in ceramic materials under cyclic loading conditions10.1007/BF02642921 ↗
14. High frequency cyclic crack propagation in ceramic materials10.1007/BF00036978 ↗
15. Crack-interface grain bridging as a fracture resistance mechanism in ceramics10.1111/j.1151-2916.1987.tb04982.x ↗
16. Crack- interface grain bridging as a fracture resistance mechanism in ceramics10.1111/j.1151-2916.1987.tb04983.x ↗
17. Role of interfacial grain bridging sliding friction in the crack-resistance and strength properties of nontransforming ceramics10.1016/0001-6160(89)90299-X ↗
18. Determination of crack- bridging forces in alumina10.1111/j.1151-2916.1988.tb05908.x ↗
19. Fatigue and static crack propagation in yttria-stabilized tetragonal polycrystals10.1111/j.1151-2916.1997.tb03192.x ↗
20. Cyclic fatigue crack growth behaviour in β-(Si–Al–O–N) at ambient and elevated temperatures10.1023/A:1004620023312 ↗
21. Subcritical crack propagation under cyclic and static loading in mullite and mullite-zirconia10.1016/S0955-2219(97)00118-0 ↗
22. Development of High Temperature Fatigue, Creep and Thermal Shock Resistant Zircon and Mullite Zirconia Ceramics, Final Technical Report for Brite-Euram Project No. BRE2-CT94-0613, QMW, London, 1997.
23. Suitability of mullite for high temperature applications10.1016/S0955-2219(99)00116-8 ↗
24. Kübler J., Fracture Toughness of Ceramics Using the SEVNB Method; Round Robin. VAMAS Report No37, ISSN 1016-2186, published by EMPA Dübendorf, Switzerland, May 1999.
25. Srawley J. E., Gross B., In Cracks in Fracture, Am. Soc. Test. Mater., Spec. Tech. Publ., No.601, ASTM, Philadelphia, PA, 1976, pp. 559-579.10.1520/STP28664S ↗
26. Elastic/plastic indentation damage in ceramics10.1111/j.1151-2916.1980.tb10768.x ↗
27. A critical evaluation of indentation techniques for measuring fracture toughness10.1111/j.1151-2916.1981.tb10320.x ↗
28. ASTM Standard E 740-80, Standard recommended practice for fracture testing with surface-crack tension specimens. In ASTM Annual Book of Standards, Vol. 301, American Society of Testing and Materials, Philadelphia, PA, 1983, pp. 740-750.
29. Newman, Jr., J. C. and Raju I. S., Analysis of Surface Cracks in Finite Plates under Tension or Bending Loads, NASA Technical paper 1578, NASA December 1979.
30. Repeated indentation method10.1111/j.1151-2916.1990.tb05149.x ↗
31. VAMAS round robin on fracture toughness of silicon nitride10.1111/j.1151-2916.1995.tb08891.x ↗
32. Cronins, A., unpublished work at Queen Mary and Westfield College.