journal article·2003-08

The influence of oxidation on crack resistance in injection moulded Cr3C2/Al2O3 composites

Ching-An Jeng, Jow-Lay Huang

Publisher page

Abstract

Abstract The crack resistance (R-curve) of injection moulded Cr 3 C 2 /Al 2 O 3 composite was studied using the indentation-strength-in-bending technique. The influence of heat treatment on the crack resistance was investigated. The oxidation layer containing alumina and alumina/chromia solid solution was in a compression of −179 and −195 MPa as evaluated by X-ray analysis and indentation method, respectively. The results were slightly different from the thermal mismatch calculation (−139 MPa). The relatively compressive, low porous oxidation layer caused significant increase in crack resistance. Crack healing could contribute also partially to crack resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Injection Molding Process and Properties · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Microstructure and mechanical proterties of Cr3C2 particulate reinforced Al2O3 matrix composites10.1007/BF00356816 ↗
2. Effects of oxidation of Cr3C2 particle reinfroced Cr3C2 matrix composites on microstructure and mechanical structure properties10.1007/BF01352185 ↗
3. Effects of post-sinter hot isostatic pressing processes on microstructures and mechanical properties of Al2O3- Cr3C2 composites
4. Investigation of Al2O3/ Cr3C2 composites prepared by pressureless sintering (part 1)10.2109/jcersj.104.796 ↗
5. Investigation of Al2O3/ Cr3C2 composites prepared by pressureless sintering (part 2)10.1016/S0254-0584(97)80309-4 ↗
6. Investigation of Al2O3/ Cr3C2 composites prepared by pressureless sintering (part 3)10.1016/S0272-8842(98)00014-5 ↗
7. Strengthening glass-ceramics by application of compressive glazes10.1111/j.1151-2916.1968.tb11845.x ↗
8. Strengthening of oxide ceramics by tranformation-toughened stresses10.1111/j.1151-2916.1987.tb04952.x ↗
9. A Technique for introducing surface compression into zirconia ceramics10.1111/j.1151-2916.1983.tb10543.x ↗
10. Toughening of layered ceramic composites with residual surface compression10.1111/j.1151-2916.1996.tb07883.x ↗
11. Surface stress effects on indentation fracture sequences10.1111/j.1151-2916.1990.tb06737.x ↗
12. Strength rentention in SiC ceramics after long-term oxidation10.1111/j.1151-2916.1983.tb10101.x ↗
13. Oxidation-induced toughening and strengthening of Y2O3/SiC nanocomposites10.1111/j.1151-2916.1997.tb02903.x ↗
14. Effect of residual stress on the strength distribution of brittle materials10.1111/j.1151-2916.1989.tb05996.x ↗
15. Microstructure, strength and fracture characteristics of a free-standing plasma-sprayed alumina10.1016/S0955-2219(96)00242-7 ↗
16. Cohen, J. B., Dolle, H. and James, M. R., Stress Analysis from Powder Diffraction Patterns. NBS Special Publication 567, 1980, pp. 453–477.
17. Noyan · 1987
18. The interfacial reaction in Cr3C2/Al2O3 composites10.1557/JMR.1999.0108 ↗
19. Elastic properties of oxide solid solutions10.1111/j.1151-2916.1970.tb15982.x ↗
20. Migration of grain boundaries in alumina induced by chromia addition10.1016/0956-7151(94)00306-3 ↗
21. Formation of continuous series of solid solutions from powders prepared by hydrazine method10.1016/0025-5408(96)00064-5 ↗
22. Fabrication and mechanical properties of solid solution with low addition of Cr2O310.4028/www.scientific.net/KEM.161-163.161 ↗
23. Oxidation/vaporization kinectics of Cr2O310.1111/j.1151-2916.1971.tb12225.x ↗
24. An indentation technique for measuring strsses in tempered glass surfaces10.1111/j.1151-2916.1977.tb16106.x ↗
25. Measurement of thin-layer surface stresses by indentation fracture10.1007/BF00980772 ↗
26. Measurement of residual stresses in coating on brittle subsrates by indentation10.1111/j.1151-2916.1987.tb05006.x ↗
27. Kingery · 1976
28. Rising fracture toughness from the bending strength of indented alumina beams10.1111/j.1151-2916.1988.tb05051.x ↗
29. Crack stability and t-curve due to macroscopic residual compressive stress profiles10.1111/j.1151-2916.1991.tb07818.x ↗
30. Healing of surface cracks in SiC by oxidation10.1111/j.1151-2916.1970.tb12104.x ↗
31. Crack healing in a silicon nitride ceramics10.1111/j.1151-2916.1998.tb02558.x ↗
32. Influence of surface oxidation on thermal shock resistance and flexural strength of SiC/Cr3C2 composites10.1007/BF01154682 ↗