journal article·2016-12

Effects of processing temperature on microstructures and mechanical behaviours of reactive hot-pressed SiC(SCS-6)/Ti/ZrB2–ZrC hybrid composites

Shuqi Guo

Publisher page

Abstract

Abstract In this study, hybrid composites comprising SiC(SCS-6)/Ti composite and ZrB 2 –ZrC ceramics were prepared by sandwiching Ti/SiC(SCS-6)/Ti sheets and Zr + B 4 C powder layers, followed by reactive hot pressing (RHPing) between 1250 °C and 1400 °C. The effects of RHPing temperature on the microstructures and the mechanical behaviours of the composites were examined. For the samples prepared at 1250 °C and 1300 °C, a Ti-rich zone was observed in the matrix and around the fibres. However, for the sample prepared at 1400 °C, no Ti-rich zone was observed. In addition, the hybrid composites show noncatastrophic fracture behaviour, irrespective of RHPing temperature. Compared to the sample processed at 1400 °C, the samples processed at 1250 °C and 1300 °C exhibited higher flexural strength and greater damage tolerance. The lower strength and damage tolerance for the composite processed at 1400 °C are attributed to stronger interface bonding via significant degradation of the C-rich coating and to strength degradation of the fibres.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Materials for ultrahigh temperature structural applications
2. UHTCs: Ultra-high temperature ceramic materials for extreme environment applications
3. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
4. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
5. Thermophysical properties of ZrB2 and ZrB2–SiC ceramics10.1111/j.1551-2916.2008.02268.x ↗
6. Thermal and electrical transport of spark plasma-sintered HfB2 and ZrB2 ceramics10.1111/j.1551-2916.2011.04411.x ↗
7. Electrical resistivity of titanium diboride and zirconium diboride10.1111/j.1151-2916.1995.tb08498.x ↗
8. Some characteristics and applications of ZrB2 ceramics
9. J. Bull, M.J. White, L. Kaufman, Ablation resistant zirconium and hafnium ceramics, United States Patent, No. 5750450 (1998).
10. Oxidation of ultra-high temperature transition metal diboride ceramics10.1179/1743280411Y.0000000012 ↗
11. Strong ZrB2–SiC–WC ceramics at 1600°C10.1111/j.1551-2916.2011.05062.x ↗
12. UHTS composites for hypersonic applications
13. A low risk reentry: looking backward to step forward10.1016/j.ast.2005.10.006 ↗
14. Aerothermodynamic study of ultra-high temperature ceramic winglet for atmospheric reentry test10.2514/1.33296 ↗
15. Tensile tests of ceramic-matrix composites: theory and experiment10.1111/j.1151-2916.1990.tb05273.x ↗
16. Damage and failure in unidirectional ceramic-matrix composites10.1111/j.1151-2916.1992.tb05495.x ↗
17. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
18. Effect of hot pressing time and temperature on the microstructure and mechanical properties of ZrB2–SiC10.1007/s10853-006-1274-2 ↗
19. Improved processing and oxidation-resistance of ZrB2 ultra-high temperature ceramics containing SiC nanodispersoids10.1016/j.msea.2007.03.002 ↗
20. Effect of thermal exposure on strength of ZrB2-based composites with nano-sized SiC particles10.1016/j.compscitech.2008.06.021 ↗
21. S.Q. Guo, SiC fibres-containing hybrid composites and their fabrication method, Japan Patent, No. 2015-167721 (Patent pending).
22. S.Q. Guo, Reactive hot-pressed hybrid ceramic composites comprising SiC(SCS-6)/Ti composite and ZrB2–ZrC ceramic, J. Am. Ceram. Soc., http://dx.doi.org/10.1111/jace.14372.10.1111/jace.14372 ↗
23. Reactive hot-pressing of platelet-like ZrB2–ZrC–Zr cermets: processing and microstructure10.1016/j.ceramint.2014.04.117 ↗
24. The microstructure of SCS-6 SiC fibre10.1557/JMR.1991.2234 ↗
25. Microstructure and role of outermost coating for tensile strength of SiC fibre10.1016/S1359-6454(98)00181-5 ↗
26. Continuous silicon carbide fibre MMCs
27. Allotropic transformation in titanium-zirconium alloys
28. Low-temperature processing ZrB2–ZrC composites by reactive hot pressing10.1007/s11661-008-9500-y ↗
29. Transient plastic phase processing of titanium-boron-carbon composites10.1111/j.1151-2916.1993.tb03924.x ↗
30. Improvement of mechanical properties of SiC(SCS-6) fibre-reinforced Ti3AlC2 matrix composites with Ti barrier layer10.1016/j.jeurceramsoc.2015.12.039 ↗
31. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
32. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
33. Residual stresses, strength and toughness of laminates with different layer thickness ratios10.1016/j.actamat.2006.06.008 ↗
34. Strength-degrading mechanisms for chemically-vapor-deposited SCS-6 silicon carbide fibres in an argon environment10.1111/j.1151-2916.1998.tb02433.x ↗