Mechanical-property evaluation of thin corroded surface layers of ceramic materials by the microindentation technique
Source abstract
Abstract
Abstract An instrumented depth-sensitive microindentation technique was applied to evaluate mechanical properties of thin corroded layers of some ceramics which were immersed in boiling, highly condensed sulfuric acid up to 1000 h. Indentation load–depth curves were analyzed using a finite element model to systematically investigate the effect on the ceramics of film or corroded layer. The mechanical properties of both the oxide films and the corroded layers were evaluated through the combination between analytical and experimental results on the indentation curves. It was found that the relationship between thickness T of oxide films or corroded layers and the depth d determined by the slope change on the indentation load/depth–depth curve is described as T ≈10 d . The bending strengths of Si 3 N 4 and Al 2 O 3 after immersion were evaluated using the d associated with the corroded layer thickness and the K IC obtained before immersion. It was confirmed that the strength degradation of Si 3 N 4 and Al 2 O 3 due to the boiling sulfuric acid corrosion can be estimated using K IC and d -value.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques · Advanced machining processes and optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Onuki, K., Nakajima, H., Ioka, I., Futakawa, M. and Shimizu, S. IS-process for thermochemical hydrogen production. JAERI-Review 94-006, 1994.
2. Screening tests on materials of construction for the thermochemical IS process10.3323/jcorr1991.46.113 ↗
3. Lay · 1991
4. Frechette, V. D., Failure Analysis of Brittle Materials. Advances in Ceramics. The American Ceramic Society, Vol. 28, 1990.
5. Murakami, Y. et al., Stress Intensity Factors Handbook, Vols. 1 and 2. Pergamon, 1987.
6. Evaluation of material strength by ultra-micro-indentation
7. Hallquist, J. O., LS-DYNA Theoretical Manual. Livermore Software Technology Corporation, 1993.
8. Elastic/plastic properties of bilayered silica scales on SiC
9. Mechanism of strength degradation for hot corrosion of α-SiC10.1111/j.1151-2916.1986.tb07336.x ↗
10. Corrosion behavior of sintered silicon nitoride ceramics in acid and alkaline solutions10.3323/jcorr1991.44.276 ↗
11. Koiter · Trans. ASME, Ser. E · 1965 · 32 · 23710.1115/1.3625769 ↗
12. Corrosion resistance of oxide scale formed on SiSiC in boiling sulfuric acid