journal article·2026-01Open access

Steam corrosion behavior of rare earth multi-component glass ceramics modified SiCf/SiC composites

Pinxiao Chen, Yawen Ma, Yongsheng Liu, Jingxin Li, Litong Xi, Jing Wang, Yuyu Song, Qiaomu Liu, Yejie Cao

Abstract

In this work, SiC f /SiC composites are modified by (Y 0.25 Yb 0.25 Er 0.25 Ho 0.25 ) 2 Si 2 O 7 ((4RE 0.25 ) 2 Si 2 O 7 ), and compacted by RE 2 O 3 -Al 2 O 3 -SiO 2 -B 2 O 3 -Cr 2 O 3 glass (or simply RBCAS glass. RE=Y, Yb, Er, Ho, equimolar ratios), which can separate out mullite and (4RE 0.25 ) 2 Si 2 O 7 after infiltration. After being corroded in steam environment for 100 h at 1300 ºC, the internal morphology of modified SiC f /SiC composites remained excellent stability due to the blocking effect of the modified phase. In particular, there is no new phase was formed in the modified matrix of SS-R and SS-HR composites, only the (4RE 0.25 ) 2 Si 2 O 7 and mullite crystals grew. The strength retention rate of modified SiC f /SiC composites after high-temperature steam corrosion was about 82.8 %, which is higher than that of SiC f /SiC composites prepared by CVI process (70.7 %). This rare earth multi-component microcrystalline glass has excellent resistance to steam corrosion and can be used as modified material of SiC f /SiC composites.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Current research art of rare earth compound modified SiC-CMCs for enhanced wet-oxygen corrosion resistance10.1016/j.ceramint.2022.03.210 ↗
3. Potential application of ceramic matrix composites to aero-engine components10.1016/S1359-835X(98)00139-0 ↗
4. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
5. Degradation mechanism of SiCf/SiC composites after long-time water vapor and oxygen corrosion at 1300 ºC10.1016/j.corsci.2022.110099 ↗
6. Accelerated oxidation of SiC CMC’s by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
7. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
8. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
9. Variation of the oxidation rate of silicon carbide with watervapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
10. Protective coatings for gas turbines, the gas turbine handbook
11. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
12. Effect of heat treatment on the microstructure and strength of yttrium silicate matrix-modified SiCf/SiC composites10.1016/j.jeurceramsoc.2021.09.031 ↗
13. The impact of water and oxygen contents on the corrosion performance of yttrium silicate modified SiCf/SiC composites under high temperature conditions10.1016/j.jeurceramsoc.2023.11.049 ↗
14. Preparation and properties of SiC/SiC-SiYC with excellent water-oxygen corrosion resistance10.1016/j.jeurceramsoc.2023.06.007 ↗
15. Significant improvement of resistance to dry/water oxygen corrosion at medium and high temperatures of SiC/SiC composites upon matrix modification by Ca-Y-Al-Si-O microcrystalline glass10.1016/j.jeurceramsoc.2023.04.016 ↗
16. Current status of environmental barrier coatings for Si-based ceramics
17. Mechanisms of ytterbium monosilicate/mullite/silicon coating failure during thermal cycling in water vapor10.1111/jace.13792 ↗
18. Thermal properties of single-phase Y2SiO510.1016/j.jeurceramsoc.2008.07.026 ↗
19. Silicon nitride for high-temperature applications10.1111/j.1551-2916.2010.03839.x ↗
20. Recent progress in high-entropy alloys10.3166/acsm.31.633-648 ↗
21. Alloyed pleasures: multimetallic cocktails
22. High-entropy ceramics: present status, challenges, and a look forward10.1007/s40145-021-0477-y ↗
23. Entropy-stabilized oxides10.1038/ncomms9485 ↗
24. High-entropy environmental barrier coating for the ceramic matrix composites10.1016/j.jeurceramsoc.2019.02.022 ↗
25. Excellent CMAS resistance of a newly developed equiatomic high entropy (Dy1/4Ho1/4Tm1/4Yb1/4)2Si2O7 ceramic pyrosilicate10.1016/j.ceramint.2023.03.101 ↗
26. High-entropy rare-earth disilicate (Lu0.2Yb0.2Er0.2Tm0.2Sc0.2)2Si2O7: a potential environmental barrier coating material10.1016/j.jeurceramsoc.2022.03.006 ↗
27. Water vapor corrosion behaviors of high-entropy pyrosilicates
28. High temperature corrosion of (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 environmental barrier coating material subjected to water vapor and molten calcium-magnesium-alumino-silicate (CMAS)10.1016/j.corsci.2020.108881 ↗
29. A multicomponent γ-type (Gd1/6Tb1/6Dy1/6Tm1/6Yb1/6Lu1/6)2Si2O7 disilicate with outstanding thermal stability10.1080/21663831.2020.1783007 ↗
30. Preparation and corrosion resistance of high-entropy disilicate (Y0.25Yb0.25Er0.25Sc0.25)2Si2O7 ceramics10.1016/j.corsci.2021.109786 ↗
31. Preparation and water vapor corrosion behavior of high entropy rare earth disilicate (Y0.25Yb0.25Ho0.25Er0.25) 2Si2O710.1016/j.ceramint.2023.11.182 ↗
32. Microstructure and properties of SiCf/SiC joint brazed by Y-Al-Si-O glass10.1016/j.ceramint.2018.02.092 ↗
33. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics
34. Current status of environmental barrier coatings for Si-based ceramics
35. Thermal properties of single-phase Y2SiO510.1016/j.jeurceramsoc.2008.07.026 ↗
36. Mechanisms of ytterbium monosilicate/mullite/silicon coating failure during thermal cycling in water vapor10.1111/jace.13792 ↗
37. Phase equilibria in the system MgO-Cr2O3-SiO210.1111/j.1151-2916.1954.tb13981.x ↗
38. Phase equilibria in the system Cr2O3-SiO210.6028/jres.005.021 ↗
39. The system Al2O3-Cr2O3-SiO210.1111/j.1151-2916.1968.tb13328.x ↗
40. PerezJ · High. Lev. Waste melter Study Rep. · 2001
41. Kinetics of ion-exchange-induced vitrification of glass-ceramics10.1111/jace.16253 ↗
42. Structure and performance of glass-ceramics obtained by bayan obo tailing and Fly ash10.1016/j.jnoncrysol.2013.09.012 ↗
43. Physical and spectroscopic properties of multi-component Na2O-PbO-Bi2O3-SiO2 glass ceramics with Cr2O3 as nucleating agent10.1016/j.optmat.2015.05.048 ↗
44. Recent progress in high-entropy alloys10.3166/acsm.31.633-648 ↗
45. Degradation of silicon carbide in combustion gasflow at high temperature and high speed10.1299/jsmea.44.520 ↗
46. SiC recession caused by SiO2 scale volatility under combustion conditions: I, experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
47. SiC recession caused by SiO2 scale volatility under combustion conditions: II, thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
48. A comparison of the oxidation kinetics of SiC and Si3N410.1149/1.2048559 ↗
49. Mass spectrometric identification of Si-O-H(g) species from the reaction of silica with water vapor at atmospheric pressure10.1111/j.1151-2916.1997.tb02935.x ↗
50. The effect of microstructure and chromia content on the properties of zirconia toughened alumina10.1016/j.ceramint.2017.10.146 ↗
51. Anomalous densification behavior of Al2O3-Cr2O3 system10.1016/j.matchar.2015.11.005 ↗
52. Densification behavior and properties of alumina-chrome ceramics: effect of TiO210.1016/j.ceramint.2012.06.013 ↗
53. Microstructure and mechanical properties of CaAl12O19 reinforced Al2O3-Cr2O3 composites10.1016/j.jeurceramsoc.2021.08.024 ↗
54. Effects of Cr2O3 addition on the mechanical properties, microstructure and wear performance of zirconia-toughened-alumina (ZTA) cutting inserts10.1016/j.jallcom.2011.09.092 ↗
55. Development and environmental durability of mullite and mullite/YSZ dual layer coatings for SiC and Si3N4 ceramics10.1016/S0257-8972(96)03074-5 ↗
56. Observations of accelerated silicon carbide recession by oxidation at high water-vapor pressures10.1111/j.1151-2916.2000.tb01172.x ↗
57. Effects of moisture on tensile stress rupture behavior of a SiC/SiC composite at elevated temperatures10.1016/j.compscitech.2007.03.005 ↗
58. Enhanced water-oxygen corrosion resistance of SiC/SiC composites at 1350 ºC via a single-layer Y-Al-Si-O glass-ceramics environmental barrier coating10.1016/j.jeurceramsoc.2024.116728 ↗
59. Water and oxygen corrosion resistance of SiCf/SiC-SiYBC composites prepared by reactive melt infiltration at 1300 ºC-1500 ºC10.1111/ijac.14597 ↗