journal article·2026-02Open access

High temperature interlaminar tensile strength of a SiCf/SiC ceramic matrix composite determined through diametrical compression testing up to 1200°C

S.P. Jeffs, C.D. Newton, S. John, M.R. Bache, L. Gale, S. Pattison, A.L. Chamberlain

Abstract

The diametrical compression test method was used in this study to determine the high temperature interlaminar tensile strength of a SiC f /SiC Ceramic Matrix Composite. Two disk geometries are employed (Φ4.5 mm and Φ9 mm) with tests performed up to 1200°C, building upon previous room temperature investigations conducted by the authors [1]. For all tests, disks failed parallel to the loading axis spanning between the upper and lower contact points, ensuring repeatability and reliability even at high temperatures. Digital image correlation was applied to selected tests to measure the full-field strain and observe damage progression to ultimate failure. Weibull distribution was implemented to determine the characteristic strength and distribution, to understand the influence of specimen volume and high temperature oxidation. High temperature results were revealed to have a higher characteristic strength and Weibull modulus owing to the associated oxidation mechanisms, whether the formation of silica rich regions or degradation of the interphase.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Determining the interlaminar tensile strength of a SiCf/SiC ceramic matrix composite through diametrical compression testing10.1016/j.jeurceramsoc.2022.11.014 ↗
2. Ceramic matrix composites taking flight at GE aviation
3. J.A. DiCarlo, Advances in SiC/SiC Composites for Aero-Propulsion, Sep. 26, 2014. doi:https://doi.org/10.1002/9781118832998.ch7.10.1002/9781118832998.ch7 ↗
4. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
5. G. Gardiner, A new era for ceramic matrix composites. Accessed: Oct. 31, 2024. [Online]. Available: 〈https://www.compositesworld.com/articles/a-new-era-for-ceramic-matrix-composites〉.
6. “Ceramic Matrix Composites: High value composites for extreme environments to transform net zero engineering solutions.” Accessed: Oct. 31, 2024. [Online]. Available: 〈https://www.nccuk.com/what-we-do/technologies/ceramic-matrix-composites/〉.
7. Fatigue of ceramic matrix composites10.1016/0956-7151(94)00304-Z ↗
8. Degradation of a SiC-SiC composite in water vapor environments10.1111/jace.16838 ↗
9. Matrix cracking onset stress and strain as a function of temperature, and characterisation of damage modes in SiCf/SiC ceramic matrix composites via acoustic emission10.1016/j.jeurceramsoc.2022.10.042 ↗
10. Effect of oxidation on the bending fatigue behavior of an advanced SiC/SiC CMC component at 1000 °C in air10.1016/j.jeurceramsoc.2022.03.061 ↗
11. Multiphysics model of thermomechanical oxidative degradation in SiC/SiC ceramic matrix composite microstructures10.1016/j.jeurceramsoc.2025.117335 ↗
12. Elevated-temperature stress rupture in interlaminar shear of a Hi-Nic SiC/SiC ceramic matrix composite10.1016/j.compscitech.2008.12.006 ↗
13. The interlaminar tensile and shear behavior of a unidirectional C-C composite10.1016/0022-3115(96)80018-3 ↗
14. S. Kane, A. Stanley, L. Sanchez, D. Faucett, and S. Choi, Life Limiting Aspects of an MI SiC/SiC Ceramic Matrix Composite (CMC) in Interlaminar Shear at Elevated Temperature, in Proceedings of the ASME Turbo Expo 2021: Turbomachinery Technical Conference and Exposition., ASME, 2021, p. V006T02A009.10.1115/GT2021-60277 ↗
15. In-plane and interlaminar shear strength of a unidirectional Hi-Nicalon fiber-reinforced celsian matrix composite10.1016/S0272-8842(02)00006-8 ↗
16. Characterization of interlaminar shear strength of ceramic matrix composites10.1111/j.1151-2916.1993.tb03979.x ↗
17. Interlaminar tensile strength of alumina-based oxide/oxide ceramic matrix composite at room temperature and 1200 °C using diametral compression test method10.1016/j.compositesa.2024.108420 ↗
18. J.T. Mattison, D. Calvin, and S.R. Choi, Development of High-Temperature, Interlaminar Tension (ILT) Test Methodology for Ceramic Matrix Composites (CMCs), in Proceedings of the ASME Turbo Expo 2024: Turbomachinery Technical Conference and Exposition. Volume 2, London, United Kingdom: ASME, Jun. 2024, p. V002T02A004. doi:10.1115/GT2024-123432.10.1115/GT2024-123432 ↗
19. ASTM C1468-19a, Standard Test Method for Transthickness Tensile Strength of Continuous Fiber-Reinforced Advanced Ceramics at Ambient Temperature, 2019, ASTM International: West Conshohocken.
20. A modified test for measuring the interlaminar tensile strength of fiber-reinforced ceramic composites10.1016/j.compscitech.2007.06.002 ↗
21. High-temperature diametral compression strength of microwave-sintered mullite10.1016/j.jeurceramsoc.2011.07.034 ↗
22. Diametral compression test: validation using finite element analysis10.1007/s00170-011-3328-0 ↗
23. Strength anisotropy of NITE-SiC/SiC composite by various failure modes10.2320/matertrans.M2012182 ↗
24. Determination and prediction of axial/off-axial mechanical properties of SiC/SiC composites10.1016/j.fusengdes.2012.02.026 ↗
25. Size effect assessment by Weibull’s approach and the coupled criterion10.1016/j.engfracmech.2021.107979 ↗
26. T. Hinoki, E. Lara-Curzio, and L.L. Snead, Evaluation of Transthickness Tensile Strength of SiC/SiC Composites, in 27th Annual Cocoa Beach Conference on Advanced Ceramics and Composites: B: Ceramic Engineering and Science Proceedings, in Ceramic Engineering and Science Proceedings., 2003, pp. 401–406. doi:https://doi.org/10.1002/9780470294826.ch58.10.1002/9780470294826.ch58 ↗
27. On weakest link theory and weibull statistics10.1111/jace.14665 ↗
28. Size and scale effects in composites: I. Literature review10.1016/S0266-3538(98)00065-7 ↗
29. Characteristic strength, weibull modulus, and failure probability of fused silica glass10.1117/1.3265716 ↗
30. Size effect of carbon fiber-reinforced silicon carbide composites (C/C-SiC): part 2 - tensile testing with alignment device10.1016/j.jeurceramsoc.2021.11.044 ↗
31. Oxidation of SiC/BN/SiC ceramic matrix composites in dry and wet oxygen at intermediate temperatures10.1016/j.jeurceramsoc.2022.04.003 ↗
32. Wilson · 2018
33. Modeling environmentally induced property degradation of SiC/BN/SiC ceramic matrix composites10.1111/jace.15325 ↗