Influence of operating conditions on the degradation of co-annular Si₃N₄-MoSi₂ glow plugs
Source abstract
Abstract
Silicon-nitride-based composites are widely used in ceramic heaters for combustion engines due to their high strength and wear resistance. Recent developments in engine designs, focusing on using alternative jet fuels with lower auto-ignition tendencies, have increased the demand for ignition-assistance devices. However, extended operation of glow plugs at high temperatures, beyond their intended use, accelerates degradation processes, thereby reducing durability. To design improved materials for this application, investigating the degradation modes of state-of-the-art glow plugs is crucial. This paper presents experimental results on co-annular glow plugs tested in three operating environments: ambient air, constant airflow chambers, and combustion engines. XRD, SEM microscopy, and Micro-CT were used to characterize microstructural changes alongside resistance behavior. Observed degradation modes in co-annular designs included surface oxidation, volatilization, sintering aid migration, and internal cracks caused by thermal stress from CTE mismatch. The primary degradation mode of this glow plug design was surface oxidation, as the resistive heating occurred at the outermost surface, making it particularly susceptible to surface degradation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Thermomechanical characterization of hot surface ignition device using phenomenological heat flux model10.2514/1.B38662 ↗
2. Ignition sensitivity analysis for energy-assisted compression-ignition operation on jet fuels with varying cetane number10.4271/2022-01-0443 ↗
3. Development of a high-strength Si3N4 sintered body10.1016/0263-4368(91)90021-F ↗
4. Numerical investigations of combustion dynamics and thermo-mechanical stress in the ignition assistance system for small aircraft engines
5. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
6. Degradation of silicon nitride glow plugs in various environments part 1: DC electric field in ambient air10.1111/j.1744-7402.2010.02498.x ↗
7. Degradation of silicon nitride glow plugs in various environments part 2: gas burner rig10.1111/j.1744-7402.2011.02663.x ↗
8. Degradation of silicon nitride glow plugs in various environments part 3: NGDI engine10.1111/j.1744-7402.2011.0202724.x ↗
9. Karimi Sharif H.. Degradation of Silicon Nitride Glow Plugs in Electric Field-experiments and Modeling (Ph.D. thesis) University of British Columbia, 2015.
10. Baird B., Etemad S. Advanced Glow Plug for Heavy Fuels Applications, 2013, 2013-01–1716. https://doi.org/10.4271/2013-01-1716.10.4271/2013-01-1716 ↗
11. Mullite-mullite environmental barrier coatings on silicon nitride by composite sol-gel
12. Failure analysis of diesel engine glow plugs10.1016/j.engfailanal.2020.104394 ↗
13. Element redistribution in the oxide scale during air oxidation of Kanthal AF alloy10.1016/j.jmrt.2024.11.169 ↗
14. Key issues of MoSi2-UHTC ceramics for ultra high temperature heating element applications: Mechanical, electrical, oxidation and thermal shock behaviors10.1016/j.jallcom.2018.11.384 ↗
15. High temperature oxidation behavior of ZrB2-SiC added MoSi2 ceramics10.1016/j.ceramint.2018.08.144 ↗
16. Influence of different coating structures on the oxidation resistance of MoSi2 coatings10.1016/j.ceramint.2019.11.055 ↗
17. Oxidation behavior of plasma-sprayed MoSi2-Yb2O3 composite coating at 1700 °C10.1016/j.ceramint.2019.12.216 ↗
18. Potential of MoSi2 and MoSi2-Si3N4 composites for aircraft gas turbine engines
19. Precursor derived SiOC/MoSi2-composites for diesel glow plugs: preparation and high temperature properties10.2109/jcersj2.16108 ↗
20. Stafford · Combined Impacts of Engine Speed and Fuel Reactivity on Energy-assisted Compression-ignition Operation with Sustainable Aviation Fuels · 2023 · 2023
21. Thermal Characterization of an Ignition Assistant Device at Engine Relevant Conditions (MSc thesis)
22. Thermal performance of a ceramic heater ignition device for aircraft propulsion applications
23. Mechanism of liquid-phase sintering of silicon carbide and nitride with oxide activating additives10.1007/s10717-013-9557-y ↗
24. Factors influencing structural evolution in the oxide of hot-pressed Si3N4-Y2O3-SiO2 materials10.1007/BF02396923 ↗
25. The effect of different sintering additives on the electrical and oxidation properties of Si3N4–MoSi2 composites10.1016/j.jeurceramsoc.2006.07.009 ↗
26. Thermal agitation of electricity in conductors10.1103/PhysRev.32.97 ↗
27. Additive effects on Si3 N4 oxidation/volatilization in water vapor10.1111/j.1151-2916.2003.tb03462.x ↗
28. Temperature dependence mechanism of high-temperature oxidation of transition metal silicide10.1088/1361-648X/ad4b82 ↗
29. Preparation of MoSi2-SiC-Al2O3-SiO2 coating on mullite fibrous insulation with silica sol as binder by non-firing process10.1016/j.ceramint.2018.10.197 ↗
30. Factors inducing degradation of properties after long-term oxidation of electroconductive composites10.1557/JMR.2004.0210 ↗
31. Oxidation behavior of rare-earth disilicate–silicon nitride ceramics10.1111/j.1151-2916.1992.tb04463.x ↗
32. Development of a self-forming ytterbium silicate skin on silicon nitride by controlled oxidation10.1111/j.1151-2916.2002.tb00293.x ↗
33. Preparation and oxidation properties of tantalum-based Yb2O3 modified MoSi2 ceramic coating10.1016/j.jeurceramsoc.2025.117546 ↗
34. β- thermal expansion and stability in environmental barrier coating systems10.1111/jace.20214 ↗
35. Influence of temperature, oxygen partial pressure, and microstructure on the high-temperature oxidation behavior of the SiC Layer of TRISO particles10.1016/j.jeurceramsoc.2024.116913 ↗
36. Shackelford J.F., Alexander W., editors. CRC Materials Science and Engineering Handbook. 0 ed. CRC Press; 2000. https://doi.org/10.1201/9781420038408.10.1201/9781420038408 ↗
37. Stress development and fracture of surface nucleated cristobalite on silica glass10.1111/jace.13181 ↗
38. High oxidation resistance of hot pressed silicon nitride containing yttria and lanthania10.1016/S0955-2219(98)00237-4 ↗
39. Phase equilibria and crystal chemistry in the Y2 O3 –Al2 O3 –SiO2 system10.1557/JMR.1999.0064 ↗
40. Effect of sintering additives on the oxidation behavior of Si3N4 ceramics at 1300°C10.1016/j.jeurceramsoc.2004.03.023 ↗
41. Long-term stability of nonoxide ceramics in an oxidative environment at 1500 °C10.1016/S0955-2219(02)00267-4 ↗
42. Creep damage in an advanced self-reinforced silicon nitride: Part I, cavitation in the amorphous boundary phase10.1111/j.1151-2916.1999.tb01867.x ↗
43. Advanced ceramic materials for high temperature applications10.1002/adem.200500269 ↗
44. Thermochemical stability of Y2Si2O7 in high-temperature water vapor10.1111/jace.17114 ↗
45. Silica activity measurements in the Y2O 3 – SiO 2 system and applications to modeling of coating volatility10.1111/jace.12974 ↗
46. Silicon nitride for high-temperature applications10.1111/j.1551-2916.2010.03839.x ↗
47. Influence of rare-earth oxide additives on the oxidation resistance of Si3N4–SiC nanocomposites10.1016/j.jeurceramsoc.2013.01.008 ↗