Indentation fracture resistance of silicon nitride measured on curved surfaces
Source abstract
Abstract
Silicon nitride balls utilised in bearing applications experience peak loads at their surface. Thus, knowledge of the indentation fracture resistance at this location is essential. However, the standard testing method requires flat surfaces, ignoring the spherical geometry. This study investigates an adaptation of the indentation fracture method for direct application on spherical surfaces (ball diameters > 5 mm to < 50 mm) and compares results against those from flat sections at various radial positions. Findings confirm that indentation loads ≥ 5 kg yield reliable results. Significant variations in the indentation fracture resistance were observed across different radial positions and ball sizes, which could be attributed to microstructural variability. Although results from curved surfaces differed from flat sections, no unique correlation with curvature was found. However, direct surface indentation with a systematic correction may serve as a robust, application relevant approach for the quality assessment of ceramic bearing balls.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. ASTM-F2094/F 2094M-08: Standard Specification for Silicon Nitride Bearing Balls, 2009.
2. ISO 26602:2017(E): Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics) - Silicon Nitride Materials for Rolling Bearing Balls and Rollers, 2017.
3. The crack propagation trend analysis in ceramic rolling element bearing considering initial crack angle and contact load effect
4. ISO 14627:2012(E): Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics) — Test Method for Fracture Resistance of Silicon Nitride Materials for Rolling Bearing Balls at Room Temperature by Indentation Fracture (IF) method, 2012.
5. ISO 21618:2019(E): Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics) — Test Method for Fracture Resistance of Monolithic Ceramics at Room Temperature by Indentation Fracture (IF) Method, 2019.
6. DIN EN ISO 15732:2005 Hochleistungskeramik – Prüfverfahren zur Bestimmung der Bruchzähigkeit monolithischer Keramik bei Raumtemperatur an einseitig gekerbten Biegeproben (SEPB-Verfahren) (ISO 15732:2003); Deutsche Fassung EN ISO 15732:2005, 2005.
7. DIN EN ISO 18756: Hochleistungskeramik – Bestimmung der Bruchzähigkeit monolithischer Keramik bei Raumtemperatur für Biegeproben mit Oberflächenriss (Knoop-Riss) (SCF-Verfahren) (ISO 18756:2003); Deutsche Fassung EN ISO 18756:2005, 2005.
8. ISO 23146:2012 Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics) — Test Methods for Fracture Toughness of Monolithic Ceramics — Single-edge V-notch Beam (SEVNB) method, 2012.
9. Intricacies involving the evaluation of fracture toughness obtained by the surface-crack-in-flexure method10.1111/jace.18667 ↗
10. Mechanical properties of silicon nitride rolling elements in dependence of size and shape10.1016/j.jeurceramsoc.2014.06.029 ↗
11. Equi-penetration grazing incidence X-ray diffraction method: stress depth profiling of ground silicon nitride10.1016/j.actamat.2014.06.015 ↗
12. Toughness measurement on ball specimens. Part I: theoretical analysis10.1016/j.jeurceramsoc.2011.12.003 ↗
13. Toughness measurement on ball specimens. Part II: experimental procedure and measurement uncertainties10.1016/j.jeurceramsoc.2013.12.052 ↗
14. Vickers indentation fracture toughness test Part 1 Review of literature and formulation of standardised indentation toughness equations10.1179/mst.1989.5.9.865 ↗
15. Vickers indentation fracture toughness test Part 2 Application and critical evaluation of standardised indentation toughness equations10.1179/mst.1989.5.10.961 ↗
16. Indentation crack profiles in silicon nitride10.1016/S0955-2219(00)00197-7 ↗
17. Crack profiles under a Vickers indent in silicon nitride ceramics with various microstructures10.1016/j.ceramint.2009.07.016 ↗
18. Light Microscopy
19. Beiträge zur Theorie des Mikroskops und der mikroskopischen Wahrnehmung10.1007/BF02956173 ↗
20. Influences of stress on the measurement of mechanical properties using nanoindentation: Part I. Experimental studies in an aluminum alloy10.1557/JMR.1996.0091 ↗
21. Application of X-Ray stress measuring technique to curved surfaces: residual stress on spherical surfaces
22. Production of sharp cracks in ceramic materials by three-point bending of sandwiched specimens10.1016/S0013-7944(97)00153-7 ↗
23. Surface crack in tension or in bending – a reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials10.1016/j.jeurceramsoc.2012.01.011 ↗
24. Corrigendum to“surface crack in tension or in bending – A reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials10.1016/j.jeurceramsoc.2017.05.008 ↗
25. Correlation between fracture toughness and microstructure of seeded silicon nitride ceramics10.1007/s10853-007-1679-6 ↗
26. Fünfschilling · 2009
27. J. Kübler, Fracture Toughness of Ceramics Using the SEVNB Method: round Robin, VAMAS Report No. 37 (ISSN 1016-2186) and ESIS Document D2-99, EMPA-Dübendorf, Switzerland (1999)., EMPA-Dübendorf, Switzerland (1999).
28. Keyence Deutschland GmbH, VK-X1000 Serie Benutzerhandbuch, 〈www.keyence.eu〉.
29. ISO-6507-1-2018: Metallic Materials - Vickers Hardness Test - Part 1: Test method, 2018.