Abstract
Ti 3 AlC 2 MAX phase is a premier candidate for high-temperature applications due to its ability to form a protective α-Al 2 O 3 layer. However, the influence of common synthesis byproducts, particularly TiC, on intrinsic oxidation resistance remains insufficiently understood. To this end, a series of samples was fabricated by reactive spark plasma sintering with precise stoichiometric control to systematically investigate the determinative effect of TiC secondary phase (0–21 wt%) on the isothermal oxidation of Ti 3 AlC 2 at 1200 °C, as assessed by thermogravimetric analysis (TGA) and microstructural examination. Results reveal that while phase-pure Ti 3 AlC 2 exhibited exceptional oxidation resistance through parabolic growth of a continuous, 3 µm-thick adherent α-Al 2 O 3 layer, the presence of TiC triggered a transition toward destructive linear kinetics. Notably, a 21 wt% TiC content resulted in a 46-fold increase in mass gain per unit area and the formation of a porous, non-protective TiO 2 -rich layer nearly 500 µm thick. Identical-location microstructural analysis of a TiC-rich sample at initial stages of oxidation demonstrated how TiC grains act as preferential nucleation and growth sites for TiO 2 , compromising the MAX phase inherent passivation and self-healing capabilities. These findings highlight the critical importance of phase purity in optimizing MAX phases for reliable oxidation resistance performance in demanding high-temperature environments.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: MXene and MAX Phase Materials · Intermetallics and Advanced Alloy Properties · 2D Materials and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. MAX phases – Past, present, and future10.1016/j.mattod.2023.11.010 ↗
2. The MAX Phases: Unique New Carbide and Nitride Materials: Ternary ceramics turn out to be surprisingly soft and machinable, yet also heat-tolerant, strong and lightweight10.1511/2001.28.334 ↗
3. On the Chemical Diversity of the MAX Phases10.1016/j.trechm.2019.02.016 ↗
4. Layered Machinable and Electrically Conductive Ti2AlC and Ti3AlC2 Ceramics: a Review10.1016/S1005-0302(10)60064-3 ↗
5. Elastic and Mechanical Properties of the MAX Phases10.1146/annurev-matsci-062910-100448 ↗
6. Oxidation behavior of Ti3AlC2 at 1000–1400 °C in air10.1016/S0010-938X(02)00177-4 ↗
7. A Critical Review of the Oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in Air10.1080/21663831.2013.806364 ↗
8. High-Temperature Oxidation Behavior of Ti2AlC in Air10.1023/A:1023092027697 ↗
9. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
10. Microstructures and Adhesion of the Oxide Scale Formed on Titanium Aluminum Carbide Substrates10.1111/j.1551-2916.2006.01141.x ↗
11. Cyclic oxidation of Ti3AlC2 at 1000–1300°C in air10.1016/j.corsci.2010.09.033 ↗
12. Isothermal oxidation of the Ti2AlC MAX phase coatings deposited by kerosene-fuelled HVOF spray10.1016/j.corsci.2018.04.022 ↗
13. MAX phase coatings: synthesis, protective performance, and functional characteristics10.1039/D4MH01001A ↗
14. Oxidation of Al2O3 Scale-Forming MAX Phases in Turbine Environments10.1007/s11661-017-4346-9 ↗
15. Ti3AlC2, a candidate structural material for innovative nuclear energy system: The microstructure phase transformation and defect evolution induced by energetic heavy-ion irradiation10.1016/j.actamat.2020.03.008 ↗
16. Oxidation of Cr2AlC Between 900 and 1200 °C in Air10.1007/s11085-007-9071-0 ↗
17. Synthesis and microstructure of layered-ternary Ti2AlC ceramic by high energy milling and hot pressing10.1016/j.msea.2008.01.017 ↗
18. Synthesis of Ti2AlC MAX phase and Ti2C MXene by activated combustion10.1016/j.ceramint.2024.01.130 ↗
19. High-throughput reaction engineering to assess the oxidation stability of MAX phases10.1038/s41524-020-00464-7 ↗
20. Synthesis of high-purity polycrystalline Ti3AlC2 through pulse discharge sintering Ti/Al/TiC powders10.1016/j.jallcom.2007.02.105 ↗
21. Low temperature synthesis of single-phase Ti3AlC2 through reactive sintering Ti/Al/C powders10.1016/j.msea.2007.04.009 ↗
22. Oxidation of Tin+1AlXn (n=1, 3 and X= C, N): II. Experimental Results10.1149/1.1380256 ↗
23. Oxidation of Tin+1AlXn (n= 1, 3 and X= C, N): I. Model10.1149/1.1380255 ↗
24. High-temperature oxidation of Ti3AlC2 between 1173 and 1473K in air10.1016/j.msea.2006.07.060 ↗
25. Breakaway oxidation of Ti3AlC2 during long-term exposure in air at 1100 °C10.1016/j.corsci.2015.12.001 ↗
26. Cyclic oxidation behavior of TiC/Ti3AlC2 composites at 550–950 °C in air10.1016/j.jallcom.2009.10.191 ↗
27. Effect of texture on oxidation resistance of Ti3AlC210.1016/j.jeurceramsoc.2018.03.009 ↗
28. Mechanical and oxidation behavior of textured Ti2AlC and Ti3AlC2 MAX phase materials10.1016/j.jeurceramsoc.2020.07.043 ↗
29. Synthesis, sintering, and effect of surface roughness on oxidation of submicron Ti2AlC ceramics10.1111/jace.17582 ↗
30. Mechanism for breakaway oxidation of the Ti2AlC MAX phase10.1016/j.actamat.2021.117025 ↗
31. Oxidation mechanisms in bulk Ti2AlC: Influence of the grain size10.1016/j.jeurceramsoc.2020.01.042 ↗
32. Microstructure-oxidation resistance relationship in Ti3AlC2 MAX phase10.1016/j.jallcom.2020.154062 ↗
33. J.L. Smialek, Unusual Oxidative Limitations for Al-MAX Phases, NASA/TM–2017-219444, Cleveland, OH, 2017.
34. Oxidation behavior of TiC-containing Ti3AlC2 based material at 500–900 °C in air10.1007/s10019-003-0278-7 ↗
35. Oxidation behavior of Ti3AlC2 powders in flowing air10.1039/b203644d ↗
36. Mechanical properties of materials based on MAX phases of the Ti-Al-C system10.3103/S1063457612020049 ↗
37. Mechanical properties of porous Ti3SiC2/TiC, Ti3AlC2/TiC, and Ti4AlN3/TiN nanolaminates at 20–1300°C10.1007/s11106-010-9252-2 ↗
38. Tungsten in Ti3AlC2 MAX phase composites: Reactions during sintering and mechanical properties10.1016/j.jeurceramsoc.2025.118016 ↗
39. An optimized method for synthesizing phase-pure Ti3AlC2 MAX-phase through spark plasma sintering10.1016/j.jeurceramsoc.2021.10.030 ↗
40. Kinetic Aspects of Ti2AlC MAX Phase Oxidation10.1007/s11085-015-9526-7 ↗
41. Recent advances in magnetic structure determination by neutron powder diffraction10.1016/0921-4526(93)90108-I ↗
42. Effects of Co-doping and Microstructure on Charge Carrier Energy Filtering in Thermoelectric Titanium-Doped Zinc Aluminum Oxide10.1021/acsami.1c20300 ↗
43. Tailoring electronic and thermal transport properties of CaO(CaMnO3)m-based (m=1 and m=∞) composites for thermoelectric power generation10.1016/j.actamat.2018.10.052 ↗
44. Y and La Doping in CaMnO3 Compounds: Effects of Dopant Identity and Amount on Charge Transport Kinetics10.1002/aesr.202300191 ↗
45. Synthesis reactions for Ti3AlC2 through pulse discharge sintering Ti/Al4C3/TiC powder mixture10.1016/j.scriptamat.2006.07.018 ↗
46. Synthesis and Characterization of a Remarkable Ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
47. Ripplocations: A universal deformation mechanism in layered solids
48. Synthesis and Characterization of Ti3 AlC210.1111/j.1151-2916.2000.tb01281.x ↗
49. Dove · 1993
50. Ziman · 1960
51. Thermal Conductivity: XI, Conductivity bf Some Refractory Carbides and Nitrides10.1111/j.1151-2916.1954.tb14059.x ↗
52. Solid state properties of group IVb carbonitrides10.1016/0925-8388(94)01315-9 ↗
53. Thermal Conductivity of Titanium Carbide, Zirconium Carbide, and Titanium Nitride at High Temperatures10.1111/j.1151-2916.1964.tb15657.x ↗
54. Electronic and thermal properties of Ti3Al(C0.5,N0.5)2, Ti2Al(C0.5,N0.5) and Ti2AlN10.1063/1.2979326 ↗
55. Electrical properties of hard materials10.1016/S0263-4368(99)00005-0 ↗
56. Rud’, Yu.V. Rud’, T. El-Raghy, Electrical conductivity, thermopower, and Hall effect of Ti3AlC2, Ti4AlN3, and Ti3SiC210.1103/PhysRevB.62.10194 ↗
57. High-temperature oxidation of titanium carbide in oxygen10.1007/BF00613231 ↗
58. V.B. Voitovich, Mechanism of the High Temperature Oxidation of Titanium Carbide10.1515/HTMP.1997.16.4.243 ↗
59. A conceptual study into the potential of Mn+1AXn-phase ceramics for self-healing of crack damage10.1016/j.jeurceramsoc.2014.08.046 ↗
60. High temperature healing of Ti2AlC: On the origin of inhomogeneous oxide scale10.1016/j.scriptamat.2011.03.031 ↗
61. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
62. Effect of temperature on the healing capacity and mechanical properties of Ti2AlC MAX phase ceramics10.1111/ijac.14704 ↗
63. Self-Healing Performance of Ti2AlC Ceramic10.1039/c2jm16123k ↗
64. Self-healing behavior of Ti2AlC at a low oxygen partial pressure10.1007/s40145-022-0640-0 ↗