journal article·2026-12

The role of fibre architecture in mechanisms of thermal shock induced damage in 2.5D and 3D Cf/SiC composites

Ramya Krishna, A. Udayakumar, Rahul Mitra

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (92)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. SiC-matrix composite materials for advanced jet engines10.1557/mrs2003.193 ↗
3. C/C-SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
4. Carbon fiber reinforced composites
5. Advances in SiC/SiC composites for aero-propulsion
6. Potential application of ceramic matrix composites to aero-engine components10.1016/S1359-835X(98)00139-0 ↗
7. Carbon fiber reinforced silicon carbide ceramic matrix composites
8. Ceramic matrix composite behavior enhancement for gas turbines hot sections
9. C/SiC and C/C-SiC composites
10. Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites10.1002/adem.200290001 ↗
11. Structure/oxidation behavior relationship in the carbonaceous constituents of 2D-C/PyC/SiC composites10.1016/0008-6223(93)90086-P ↗
12. Carbon fibre reinforced silicon carbide composites (C/SiC, C/C-SiC)10.1007/0-387-23986-3_6 ↗
13. Effects of loading rate and temperature on tensile behavior of orthogonal three-dimensional woven Si-Ti-C-O fiber/Si-Ti-C-O matrix composites10.1557/JMR.2004.0375 ↗
14. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs – a review10.1080/09506608.2019.1652006 ↗
15. 3D composites: opportunities & challenges
16. Noobing: a nonwoven 3D fabric-forming process explained10.1080/00405000208630552 ↗
17. Making the uniaxial noobing process industrially relevant
18. Thermal shock of ceramic matrix composites
19. Thermal shock and cyclic loading of ceramic parts in stationary gas turbines
20. Thermal shock behavior of ceramic matrix composites
21. Thermal shock behaviour of ceramics and ceramic composites10.1179/imr.1994.39.6.228 ↗
22. Towards structural design and thermal management of advanced 2D CMCs10.1016/j.ceramint.2020.10.056 ↗
23. Thermal shock resistance of SiC fibrerein-forced borosilicate glass and lithium aluminosilicate matrix composites10.1007/BF01151250 ↗
24. Damage characterisation of thermally shocked cross-ply ceramic composite laminates10.1007/s10853-006-6594-8 ↗
25. Thermal shock fracture in cross-ply fibre-reinforced ceramic-matrix composites10.1080/14786431003785621 ↗
26. Thermal shock fracture in unidirectional fibre-reinforced ceramic-matrix composites10.1016/j.compscitech.2005.04.004 ↗
27. Predicting the thermal shock resistance of fiber reinforced brittle matrix composites10.1016/S1359-6462(98)00031-1 ↗
28. Thermal shock damage of a 3D-SiC/SiC composite10.1002/adem.200500092 ↗
29. Microstructure and thermal shock property of liquid phase sintered C f/SiC composites10.1016/j.fusengdes.2012.03.039 ↗
30. Finite element simulation of stress distribution and development of C f/SiC ceramic-matrix composite coated with single layer SiC coating during thermal shock10.1016/j.compositesb.2013.03.028 ↗
31. Thermal shock properties of 3D-C/SiC composites prepared via polymer infiltration pyrolysis (PIP)10.1016/j.ceramint.2014.01.122 ↗
32. Micro-porosity as damage indicator for characterizing cyclic thermal shock-induced anisotropic damage in oxide/oxide ceramic matrix composites10.1016/j.engfracmech.2019.106669 ↗
33. Properties evolution and damage mechanism of SiC/SiC composites after thermal shock at 1300 °C10.1016/j.ceramint.2024.06.263 ↗
34. Thermal shock response behaviour of carbon fibre reinforced silicon carbide matrix composites prepared by chemical vapour infiltration at different heating rates10.1016/j.ceramint.2021.08.022 ↗
35. Damage analysis of CVI SiCf/SiCm ceramic matrix composites under thermal shock10.1016/j.ijfatigue.2025.108842 ↗
36. Thermal shock behavior of two-dimensional woven fiber-reinforced ceramic composites10.1111/j.1151-2916.1996.tb07996.x ↗
37. Thermal shock damage in a two-dimensional woven-fiber-reinforced-CVI SiC-matrix composite10.1111/j.1151-2916.1996.tb08719.x ↗
38. Oxidation and thermal shock resistant properties of Al-modified environmental barrier coating on SiCf/SiC composites10.1016/j.ceramint.2017.06.167 ↗
39. Thermal shock properties of a 2D-C/SiC composite prepared by chemical vapor infiltration10.1007/s11665-012-0465-z ↗
40. Thermal shock behavior of 3-dimensional C/SiC composite10.1016/S0008-6223(01)00225-1 ↗
41. Revealing thermal shock behaviors and damage mechanism of 3D needled C/C–SiC composites based on multi-scale analysis10.1016/j.jmrt.2024.01.260 ↗
42. Thermal shock resistance of a 2D-C/SiC composite and its damage mechanisms10.1179/1743676113Y.0000000120 ↗
43. Preparation of 3D orthogonal woven C-SiC composite and its characterization for thermo-mechanical properties10.1016/j.msea.2011.04.063 ↗
44. Tensile strength degradation of a 2.5D-C/SiC composite under thermal cycles in air10.1016/j.jeurceramsoc.2015.12.007 ↗
45. Evaluation of elastic constants and high temperature tensile behaviour with damage assessment of the SiC seal-coated 2.5D Cf/SiC composites having multilayered interphase and Si-B-C added matrix10.1016/j.jeurceramsoc.2022.12.066 ↗
46. Effect of CVI-induced porosity on elastic properties and mechanical behaviour of 2.5D and 3D Cf/SiC composites with multilayered interphase10.1016/j.jeurceramsoc.2024.02.039 ↗
47. Resistance to cyclic oxidation and evolution of oxide scale in 2.5D and 3D Cf/SiC composites with Si-B-C added matrix10.1016/j.jeurceramsoc.2025.117666 ↗
48. Complete determination of elastic moduli of interpenetrating metal/ceramic composites using ultrasonic techniques and micromechanical modelling10.1016/j.msea.2011.07.029 ↗
49. Standard test method for flexural properties of continuous fiber-reinforced advanced ceramic composites
50. The structure of chemical vapor deposited silicon carbide10.1016/0040-6090(77)90103-1 ↗
51. Nondestructive determination of thickness and refractive index of transparent films10.1147/rd.81.0043 ↗
52. Strength and fracture behavior of two-, three- and four-dimensionally reinforced carbon/carbon composites10.1016/j.msea.2009.11.010 ↗
53. The future of carbon-carbon composites10.1016/0008-6223(87)90116-3 ↗
54. Comparison of 2D and 3D carbon/carbon composites with respect to damage and fracture resistance10.1016/S0008-6223(02)00442-6 ↗
55. Chawla · 2003
56. Overview no. 85 The mechanical behavior of ceramic matrix composites10.1016/0001-6160(89)90291-5 ↗
57. Thermal shock behaviour of angle-ply and woven dense ceramic-matrix composites10.1007/s10853-007-2314-2 ↗
58. Thermal expansion of the cubic (3C) polytype of SiC10.1007/BF01106557 ↗
59. Transverse and longitudinal coefficient of thermal expansion of carbon fibers at high temperatures (300–2500 K)10.1016/j.carbon.2008.07.035 ↗
60. Thermal shock behavior of fiber-reinforced ceramic matrix composites10.1016/0961-9526(95)00051-N ↗
61. The oxidation behaviour of carbon fibres10.1007/BF01154706 ↗
62. Oxidation kinetics and stress effects for the oxidation of continuous carbon fibers within a microcracked C/SiC ceramic matrix composite10.1111/j.1551-2916.2007.02170.x ↗
63. Oxidation kinetics of SiC deposited from CH3SiCl3/H2 under CVI conditions10.1007/BF01116033 ↗
64. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: II, modeling10.1111/j.1151-2916.1994.tb07016.x ↗
65. Oxidation behaviour of silicon carbide – a review
66. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
67. Long-term oxidation behaviors and strength retention properties of self-healing SiCf/SiC-SiBCN composites10.1016/j.jeurceramsoc.2022.12.009 ↗
68. Oxidation resistance and evolution of multi-layered oxide scale during isothermal and cyclic exposure of ZrB2–SiC–LaB6 composites at 1300 °C to 1500 °C10.1007/s11661-021-06501-4 ↗
69. Oxidation of carbon fibers and films in ceramic matrix composites: a weak link process10.1016/0008-6223(95)00034-B ↗
70. Oxidation and corrosion of non-oxide ceramics
71. A comparison of the oxidation kinetics of SiC and Si3 N 410.1149/1.2048559 ↗
72. Thermal shock behavior of a three-dimensional SiC/SiC composite10.1007/s11661-006-1053-3 ↗
73. Broadband laser-ultrasonic spectroscopy for quantitative characterization of porosity effect on acoustic attenuation and phase velocity in CFRP laminates
74. Elastic modulus measurements of extremely porous ceramic materials by ultrasonic phase spectroscopy10.1016/S0921-5093(98)00524-3 ↗
75. Effect of thermal cycling on creep behavior of powder-metallurgy-processed and hot-rolled Al and Al-SiC particulate composites10.1007/s11661-009-9982-2 ↗
76. Lemaitre · 1996
77. Evaluation and extension of physical property-porosity models based on minimum solid area10.1007/BF00355133 ↗
78. Impact of residual stress on thermal damage accumulation, and Young’s modulus of fiber-reinforced ultra-high temperature ceramics10.1016/j.matdes.2018.10.019 ↗
79. Influence of fibre architecture on the tensile, compressive and flexural behaviour of 3D woven composites10.1016/j.compositesa.2014.11.012 ↗
80. Mechanical behaviour of 2D and 3D weaved SiC-matrix, carbon continuous-fibre-reinforced composites: Part 1. Flexural strength under static loading conditions10.1007/s12666-016-0922-8 ↗
81. M. Li, R. Matsuyama, M. Sakai, 1999, Interlaminar shear strength of C/C-composites: the dependence on test methods, vol. 37, 1999, pp. 1749–57.10.1016/S0008-6223(99)00049-4 ↗
82. Insight into microstructure and flexural strength of ultra-high temperature ceramics enriched SICARBON™ composite10.1016/j.matdes.2021.109888 ↗
83. Measurement of interfacial mechanical properties in fiber-reinforced ceramic composites10.1111/j.1151-2916.1987.tb05702.x ↗
84. Strong interface in CMC s, a condition for efficient multilayered interphases10.1557/PROC-365-371 ↗
85. Influence of Interfaces and Interphases on the mechanical behavior of fiber-reinforced ceramic matrix composites
86. Oxidation of C/SiC composites in reduced oxygen partial pressures10.1149/MA2009-02/19/1857 ↗
87. Disclosing residual thermal stresses in UHT fibre-reinforced ceramic composites and their effect on mechanical behaviour and damage evolution10.1016/j.compositesb.2022.110369 ↗
88. Influence of fiber architecture on the fracture behavior of Cf-ZrB2-SiC UHTCMCs: a 3D image analysis10.1111/jace.20659 ↗
89. Effects of multilayer hydrothermal carbon interphases on mechanical properties and thermal shock resistance of CF/ZrB2-SiCBN10.1016/j.jeurceramsoc.2022.05.029 ↗
90. Enhanced mechanical properties and thermal shock resistance of Cf/ZrB2-SiC composite via an efficient slurry injection combined with vibration-assisted vacuum infiltration10.1016/j.jeurceramsoc.2020.07.003 ↗
91. Mechanical and thermal shock properties of Cf/SiBCN composite: Effect of sintering densification and fiber coating10.1111/jace.18364 ↗
92. Microstructure, mechanical properties and thermal shock resistance of ZrB2-SiC-Cfcomposite with inhibited degradation of carbon fibers10.1016/j.jallcom.2017.02.227 ↗