Thermal cycling and CMAS corrosion behavior of tri-layer Si/Yb2Si2O7/(Yb0.8Sc0.2)2SiO5 environmental barrier coatings
Source abstract
Abstract
A tri-layer Si/Yb2Si2O7/(Yb0.8Sc0.2)2SiO5 environmental barrier coating (EBC) is fabricated on the SiC substrate surface by air plasma spraying (APS) technology. Its thermal cycling and CMAS corrosion performance are investigated by experimental and first-principles calculation methods. During the thermal cycling between room temperature and 1350 ºC, the (Yb0.8Sc0.2)2SiO5 layer vertically cracks due to stress concentration caused by its mismatched coefficient of thermal expansion (CTE) with other layers, resulting in the spallation at the Yb2Si2O7/(Yb0.8Sc0.2)2SiO5 interface. Also, thermally grown oxide (TGO) growth stress and phase transition stress facilitate the coating cracking and even spallation at the Si/Yb2Si2O7 interface. Exposed to CMAS at 1300 ºC, garnet grains rapidly precipitate on the coating surface due to the existence of relatively small Sc3+ ion, effectively inhibiting the infiltration of CMAS melt. With the increase in either corrosion time or temperature, the size and number of garnet grains have an obvious increase without sacrificing phase stability. The introduction of Sc3+ ion not only lowers the reactivity of (Yb0.8Sc0.2)2SiO5 with CMAS melt, but also improves the structural stability of (Yb0.8Sc0.2)2SiO5, therefore enhancing the CMAS corrosion resistance of the Si/Yb2Si2O7/(Yb0.8Sc0.2)2SiO5 coating system.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. M. Van Roode, W.D. Brentnall, P.F. Norton, G.P. Pytanowski, Ceramic stationary gas turbine development, ASME 1993 Int Gas Turbine Aeroengine Congr Expo GT 1993. 3B, 1993.10.1115/93-GT-309 ↗
3. Comparisons of interface shear stress degradation rate between C/SiC and SiC/SiC ceramic-matrix composites under cyclic fatigue loading at room and elevated temperatures10.1080/09276440.2016.1196995 ↗
4. High-temperature oxidation of silicon carbide and silicon nitride10.2320/matertrans1989.38.821 ↗
5. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
6. New generation of plasma-sprayed mullite coatings on silicon carbide10.1111/j.1151-2916.1995.tb08236.x ↗
7. Development and environmental durability of mullite and mullite/YSZ dual layer coatings for SiC and Si3N4 ceramics10.1016/S0257-8972(96)03074-5 ↗
8. Current status of environmental barrier coatings for Si-based ceramics
9. Residual stresses and their effects on the durability of environmental barrier coatings for SiC ceramics10.1111/j.1551-2916.2005.00640.x ↗
10. Environmental degradation of high-temperature protective coatings for ceramic-matrix composites in gas-turbine engines10.1038/s41529-019-0075-4 ↗
11. Thermal expansion of rare-earth pyrosilicates10.1111/jace.12388 ↗
12. Mechanisms of ytterbium monosilicate/mullite/silicon coating failure during thermal cycling in water vapor10.1111/jace.13792 ↗
13. Response of ytterbium disilicate-silicon environmental barrier coatings to thermal cycling in water vapor10.1016/j.actamat.2015.12.053 ↗
14. Theoretical prediction and experimental investigation on the thermal and mechanical properties of bulk β-Yb2Si2O710.1111/jace.12618 ↗
15. Yttrium silicate coatings for oxidation protection of carbon-silicon carbide composites10.1111/j.1151-2916.2000.tb01392.x ↗
16. Thermal properties of rare-earth monosilicates for EBC on Si-based ceramic composites10.1111/jace.13982 ↗
17. Turbine airfoil degradation in the Persian Gulf war10.1007/BF03222663 ↗
18. Calcium-magnesium-aluminosilicate corrosion behaviors of rare-earth disilicates at 1400 ºC10.1016/j.jeurceramsoc.2013.05.030 ↗
19. Environmental barrier coating ceramics for resistance against attack by molten calcia-magnesia-aluminosilicate (CMAS) glass: Part II, β-Yb2Si2O7 and β-Sc2Si2O710.1016/j.jeurceramsoc.2018.03.010 ↗
20. The influence of calcium-magnesium-aluminosilicate deposits on internal stresses in Yb2Si2O7 multilayer environmental barrier coatings10.1016/j.actamat.2015.12.016 ↗
21. Resistance of ytterbium silicate environmental barrier coatings against molten calcium-magnesium-aluminosilicate (CMAS): a comprehensive study10.1016/j.surfcoat.2024.130540 ↗
22. Resistance of pure and mixed rare earth silicate against calcium-magnesium-aluminosilicate (CMAS): a comparative study10.1111/jace.17328 ↗
23. Interaction of ytterbium monosilicates environmental barrier coating material with molten calcium-magnesium-aluminosilicate (CMAS)10.1016/j.corsci.2022.110864 ↗
24. Corrosion behavior and mechanism of ytterbium monosilicates by molten calcium-magnesium-alumino-silicate melts at 1400 ºC and 1500 ºC10.1016/j.ceramint.2023.04.213 ↗
25. Reaction behaviors and mechanisms of tri-layer Yb2Si2O5/Yb2Si2O7/Si environmental barrier coatings with molten calcium-magnesium-alumino-silicate10.1016/j.corsci.2021.110069 ↗
26. Reaction of Yb2SiO5 EBCs against CMAS melts with different composition10.1016/j.ceramint.2024.03.144 ↗
27. Influence of Gd doping on mechanical properties, thermal conductivity and microstructural evolution of (Yb1–xGdx)2SiO5 ceramics10.1016/j.ceramint.2024.11.225 ↗
28. Corrosion behavior of (Yb0.9Y0.1)2SiO5 environmental barrier coating material against CMAS and volcanic ash: Experimental and first-principles calculation10.1016/j.ceramint.2025.08.055 ↗
29. Interactions between rare-earth zirconates (RE2Zr2O7) and CMAS silicate melts10.1016/j.corsci.2023.111526 ↗
30. Corrosion behaviors and mechanisms of ytterbium silicate environmental barrier coatings by molten calcium-magnesium-alumino-silicate melts10.1016/j.corsci.2021.109718 ↗
31. Thermal cycle and water oxygen performance of multi-layered Y3Al5O12/Yb2SiO5/Yb2Si2O7 thermal/environmental barrier coatings10.1016/j.ceramint.2024.02.112 ↗
32. Zhong · 2018
33. Fracture mechanisms of ytterbium monosilicates environmental barrier coatings during cyclic thermal exposure10.1016/j.actamat.2015.10.019 ↗
34. Oxidation behavior and interface evolution of tri-layer Si/Yb2SiO5/LaMgAl11O19 thermal and environmental barrier coatings under isothermal heat treatment at 1300 ºC10.1016/j.surfcoat.2023.129554 ↗
35. Novel double ceramic coatings based on Yb2Si2O7/La2(Zr0.7Ce0.3)2O7 by plasma spraying on Cf/SiC composites and their thermal shock behavior10.1016/j.surfcoat.2012.07.070 ↗
36. Mg2Al4Si5O18 as a novel bond coat material for advanced thermal/environmental barrier coatings on SiCf/SiC composites10.1016/j.surfcoat.2024.130460 ↗
37. Corrosion of Yb2SiO5/Yb2Si2O7/Si EBCs against Na2SO4 + 25 wt% NaCl molten salt at 1350 ºC
38. Thermal shock resistance of tri-layer Yb2SiO5/Yb2Si2O7/Si coating for SiC and SiC-matrix composites10.1111/jace.15713 ↗
39. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
40. Volume change attending low-to-high inversion of cristobalite10.1111/j.1151-2916.1944.tb14471.x ↗
41. Local thermal conductivity measurements to determine the fraction of α-cristobalite in thermally grown oxides for aerospace applications10.1016/j.scriptamat.2019.10.027 ↗
42. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
43. Interaction and infiltration behavior between calcium-ferrum-alumina-silicate and Yb4Hf3O12 ceramics at various temperatures10.1111/jace.19413 ↗
44. Thermochemical interactions of (Yb0.7Gd0.3)4Hf3O12 ceramic with CMAS melts10.1016/j.jeurceramsoc.2024.116759 ↗
45. CMAS resistance of high-entropy (Dy0.2Ho0.2Er0.2Tm0.2Lu0.2)2Hf2O7 in-serviced as top TBC of Si-HfO2/Yb2Si2O7/Yb2SiO5 EBCs system: an experimental and atomistic modeling study10.1016/j.surfcoat.2025.132183 ↗
46. Interaction of high-entropy rare-earth monosilicates environmental barrier coatings subjected to corrosion by calcium-magnesium-alumino-silicate melts10.1016/j.corsci.2022.110564 ↗
47. High-temperature interactions of desert sand CMAS glass with yttrium disilicate environmental barrier coating material10.1016/j.ceramint.2018.09.058 ↗
48. CMAS corrosion behavior of dual-phase composite Gd2Si2O7/Sc2Si2O7 as a promising EBC material10.1016/j.jeurceramsoc.2023.06.026 ↗
49. Transport phenomena in materials processing
50. Effects of crystal structure and cation size on molten silicate reactivity with environmental barrier coating materials10.1111/jace.16694 ↗
51. Corrosion behavior of YxYb(2–x)Si2O7 environmental barrier coating materials against molten calcium-magnesium-aluminosilicate (CMAS) at 1475 ºC10.1016/j.corsci.2023.111770 ↗
52. 2ZrO2·Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: Part I, optical basicity considerations and processing10.1111/jace.13210 ↗
53. Mass spectrometric measurements of the silica activity in the Yb2O3-SiO2 system and implications to assess the degradation of silicate-based coatings in combustion environments10.1016/j.jeurceramsoc.2015.07.019 ↗
54. An interpretation of glass chemistry in terms of the optical basicity concept10.1016/0022-3093(76)90027-2 ↗
55. Insights into thermos-chemical attack of CMAS+NaVO3 mixtures on YSZ materials: an experimental and computational DFT study10.1038/s41529-025-00599-2 ↗
56. Hot corrosion of (Yb0.5Y0.5)2Si2O7 and (Yb0.25Y0.25Er0.25Tm0.25)2Si2O7 by CMAS at 1300 °C and 1500 °C10.1016/j.ceramint.2025.01.231 ↗
57. The corrosion behavior of Sc2O3-Y2O3 co-doped ZrO2 influenced by Sc2O3 content in CMAS at 1300 ºC10.1016/j.jeurceramsoc.2023.09.025 ↗
58. Molecular dynamics simulation: Elementary methods10.1063/1.4823234 ↗
59. CMAS resistance of high-entropy (Dy0.2Ho0.2Er0.2Tm0.2Lu0.2)2Hf2O7 in-serviced as top TBC of Si-HfO2/Yb2Si2O7/Yb2SiO5 EBCs system: an experimental and atomistic modeling study10.1016/j.surfcoat.2025.132183 ↗