journal article·2024-09Open access

Advances and challenges in zirconia-based materials for dental applications

Mi-Kyung Han

Abstract

Abstract Zirconia ceramics, as a category of metal oxide ceramics, stand out due to their impressive physicochemical and mechanical properties. Recognized for being bioinert, these ceramics are non-toxic, exhibit excellent biocompatibility, and offer superior mechanical strength. Moreover, zirconia’s natural aesthetic qualities enable it to closely mimic the appearance of natural teeth, making it an optimal choice for dental restorations, such as crowns, bridges, and veneers. This review examines the complex relationship between zirconia’s microstructure, including aspects like grain size, porosity, and phase composition, and how these factors impact its translucency and mechanical durability. A specific focus is on the critical role of the tetragonal phase in zirconia, spotlighting its contribution to the material’s superior mechanical strength and esthetic qualities. The stabilization of this phase, primarily through the use of yttria, is discussed for its dual influence on enhancing both the material’s strength and esthetic properties. Challenges such as low-temperature degradation (LTD) and discoloration are highlighted, along with potential solutions like advanced surface modifications and novel manufacturing techniques. The potential of flash sintering and 3D printing to further improve zirconia’s properties is also explored.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. E. Marin, History of dental biomaterials: biocompatibility, durability and still open challenges. Herit. Sci. 11, 207 (2023). https://doi.org/10.1186/s40494-023-01046-810.1186/s40494-023-01046-8 ↗
2. I. Denry, J.R. Kelly, State of the art of zirconia for dental applications. Dent. Mater. 24, 299–307 (2008). https://doi.org/10.1016/j.dental.2007.05.00710.1016/j.dental.2007.05.007 ↗
3. Y. Zhang, B.R. Lawn, Novel zirconia materials in dentistry. J. Dent. Res. 97, 140–147 (2018). https://doi.org/10.1177/002203451773748310.1177/0022034517737483 ↗
4. A. Siddiqi, A.S. Khan, S. Zafar, Thirty years of translational research in zirconia dental implants: a systematic review of the literature. J. Oral Implant. 43, 314–326 (2017). https://doi.org/10.1563/aaid-joi-D-17-0001610.1563/aaid-joi-D-17-00016 ↗
5. G. Marchesi, A.C. Piloni, V. Nicolin, G. Turco, R.D. Lenarda, Chairside CAD/CAM materials: current trends of clinical uses. Biology 10, 1170 (2021). https://doi.org/10.3390/biology1011117010.3390/biology10111170 ↗
6. E. Kontonasaki, P. Giasimakopoulos, A.E. Rigos, Strength and aging resistance of monolithic zirconia: an update to current knowledge. Jpn. Dental. Sci. Rev. 56, 1–23 (2020). https://doi.org/10.1016/j.jdsr.2019.09.00210.1016/j.jdsr.2019.09.002 ↗
7. Y. Yin, J. Xu, M. Ji, L. Li, M. Chen, A critical review on sintering and mechanical processing of 3Y-TZP ceramics. Ceram. Int. 49, 1549–1571 (2023). https://doi.org/10.1016/j.ceramint.2022.10.15910.1016/j.ceramint.2022.10.159 ↗
8. J.D.M. Matos, G.R.S. Lopes, D.A. Queiroz, L.J.N. Nakano, N.C.R. Ribeiro, A.B. Barbosa, L.C. Anami, M.A. Bottino, Dental ceramics: fabrication methods and aesthetic characterization. Coatings 12, 1228 (2022). https://doi.org/10.3390/coatings1208122810.3390/coatings12081228 ↗
9. S. Kongkiatkamon, D. Rokaya, S. Kengtanyakich, C. Peampring, Current classification of zirconia in dentistry: an updated review. Peer J. 11, e15669 (2023). https://doi.org/10.7717/peerj.1566910.7717/peerj.15669 ↗
10. A. Warreth, Y. Elkareimi, All-ceramic restorations: a review of the literature. Saudi Dent. J. 32, 365–372 (2020). https://doi.org/10.1016/j.sdentj.2020.05.00410.1016/j.sdentj.2020.05.004 ↗
11. H.Y. Shi, R. Pang, J. Yang, D. Fan, H. Cai, H.B. Jiang, J. Han, E.S. Lee, Y. Sun, Overview of several typical ceramic materials for restorative dentistry. Biomed. Res. Int. (2022). https://doi.org/10.1155/2022/845144510.1155/2022/8451445 ↗
12. M. Talibi, K. Kaur, H.S. Patanwala, H. Parmar, Do you know your ceramics? Part 1: classification. Br. Dent. J. 232, 27–32 (2022). https://doi.org/10.1038/s41415-021-3818-x10.1038/s41415-021-3818-x ↗
13. J. Emsley, In your element: the A–Z of zirconium. Nat. Chem. 6, 254 (2014). https://doi.org/10.1038/nchem.187510.1038/nchem.1875 ↗
14. Y. Zhang, H.-X. Chen, L. Duan, J.-B. Fan, L. Ni, V. Ji, A comparison study of `the structural and mechanical properties of cubic, tetragonal, monoclinic, and three orthorhombic phases of ZrO2. J. Alloys Compd. 749, 283–292 (2018). https://doi.org/10.1016/j.jallcom.2018.03.25310.1016/j.jallcom.2018.03.253 ↗
15. J. Chevalier, L. Gremillard, The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends. J. Am. Ceram. Soc. 92, 1901–1920 (2009). https://doi.org/10.1111/j.1551-2916.2009.03278.x10.1111/j.1551-2916.2009.03278.x ↗
16. ISO 13356, Implants for surgery—ceramic materials based on yttria-stabilized tetragonal zirconia (Y-TZP). (2016) (see www.iso.org/patents)
17. H. Hayashi, T. Saitou, N. Maruyama, H. Inaba, K. Kawamura, M. Mori, Thermal expansion coefficient of yttria stabilized zirconia for various yttria contents. Solid State Ion. 176, 613–619 (2005). https://doi.org/10.1016/j.ssi.2004.08.02110.1016/j.ssi.2004.08.021 ↗
18. R.H.J. Hannink, P.M. Kelly, B.C. Muddle, Transformation toughening in zirconia-containing ceramics. J. Am. Ceram. Soc. 83, 461–487 (2000). https://doi.org/10.1111/j.1151-2916.2000.tb01221.x10.1111/j.1151-2916.2000.tb01221.x ↗
19. F. Kern, R. Gadow, Alumina toughened zirconia from yttria coated powders. J. Eur. Ceram. Soc. 32, 3911–3918 (2012). https://doi.org/10.1016/j.jeurceramsoc.2012.03.01410.1016/j.jeurceramsoc.2012.03.014 ↗
20. F. Zhang, K. Vanmeensel, M. Inokoshi, M. Batuk, J. Hadermann, B. Van Meerbeek, I. Naert, J. Vleugels, Critical influence of alumina content on the low temperature degradation of 2–3 mol% yttria-stabilized TZP for dental restorations. J. Eur. Ceram. Soc. 35, 741–750 (2015). https://doi.org/10.1016/j.jeurceramsoc.2014.09.01810.1016/j.jeurceramsoc.2014.09.018 ↗
21. A.A. Dmitrievskii, D.G. Zhigacheva, N.Y. Efremova, A.V. Umrikhin, Phase composition stability of nanostructured composite ceramics based on CaO–ZrO2 under hydrothermal impact. Nanotechnol. Russ. 14, 125–131 (2019). https://doi.org/10.1134/S199507801902005810.1134/S1995078019020058 ↗
22. J.-D. Lin, J.-G. Duh, C.-L. Lo, Mechanical properties and resistance to hydrothermal aging of ceria- and yttria-doped tetragonal zirconia ceramics. Mater. Chem. Phys. 77, 808–818 (2002). https://doi.org/10.1016/S0254-0584(02)00161-X10.1016/S0254-0584(02)00161-X ↗
23. D. Tovar-Vargas, E. Roitero, M. Anglada, E. Jiménez-Piqué, H. Reveron, Mechanical properties of ceria-calcia stabilized zirconia ceramics with alumina additions. J. Eur. Ceram. Soc. 41, 5602–5612 (2021). https://doi.org/10.1016/j.jeurceramsoc.2021.05.00610.1016/j.jeurceramsoc.2021.05.006 ↗
24. R.K. Govila, Strength characterization of MgO-partially stabilized zirconia. J. Mater. Sci. 26, 1545–1555 (1991). https://doi.org/10.1007/BF0054466310.1007/BF00544663 ↗
25. M. Yoshimura, M. Yashima, T. Noma, S. Somiya, Formation of diffusionlessly transformed tetragonal phases by rapid quenching of melts in ZrO2-RO1.5 systems (R = rare earths). J. Mater. Sci. 25, 2011–2016 (1990). https://doi.org/10.1007/BF0104575710.1007/BF01045757 ↗
26. A. Eichler, Tetragonal Y-doped zirconia: structure and ion conductivity. Phys. Rev. B 64, 174103 (2001). https://doi.org/10.1103/PhysRevB.64.17410310.1103/PhysRevB.64.174103 ↗
27. C. Piconi, G. Maccauro, Zirconia as a ceramic biomaterial. Biomaterials 20, 1–25 (1999). https://doi.org/10.1016/S0142-9612(98)00010-610.1016/S0142-9612(98)00010-6 ↗
28. E. Jerman, N. Lümkemann, M. Eichberger, C. Zoller, S. Nothelfer, A. Kienle, B. Stawarczyk, Evaluation of translucency, Marten’s hardness, biaxial flexural strength and fracture toughness of 3Y-TZP, 4Y-TZP and 5Y-TZP materials. Dent. Mater. 37, 212–222 (2021). https://doi.org/10.1016/j.dental.2020.11.00710.1016/j.dental.2020.11.007 ↗
29. L. Jiang, S. Guo, Y. Bian, M. Zhang, W. Ding, Effect of sintering temperature on mechanical properties of magnesia partially stabilized zirconia refractory. Ceram. Int. 42, 10593–10598 (2016). https://doi.org/10.1016/j.ceramint.2016.03.13610.1016/j.ceramint.2016.03.136 ↗
30. A. Vichi, C. Louca, G. Corciolani, M. Ferrari, Color related to ceramic and zirconia restorations: a review. Dent. Mater. 27, 97–108 (2011). https://doi.org/10.1016/j.dental.2010.10.01810.1016/j.dental.2010.10.018 ↗
31. W.M. Johnston, Color measurement in dentistry. J. Dent. 37, e2-6 (2009). https://doi.org/10.1016/j.jdent.2009.03.01110.1016/j.jdent.2009.03.011 ↗
32. J. Yan, M.R. Kaizer, Y. Zhang, Load-bearing capacity of lithium disilicate and ultra-translucent zirconias. J. Mech. Behav. Biomed. Mater. 88, 170–175 (2018). https://doi.org/10.1016/j.jmbbm.2018.08.02310.1016/j.jmbbm.2018.08.023 ↗
33. M. Yousry, I. Hammad, M.E. Halawani, M. Aboushelib, Translucency of recent zirconia materials and material-related variables affecting their translucency: a systematic review and meta-analysis. BMC Oral Health 24, 309 (2024). https://doi.org/10.1186/s12903-024-04070-710.1186/s12903-024-04070-7 ↗
34. E.R. Khattab, S.S. Abd El Rehim, W.M.I. Hassan, T.S. El-Shazly, Band structure engineering and optical properties of pristine and doped monoclinic zirconia (m-ZrO2): density functional theory theoretical prospective. ACS Omega 6, 30061–30068 (2021). https://doi.org/10.1021/acsomega.1c0475610.1021/acsomega.1c04756 ↗
35. C.H. Lim, S. Vardhaman, N. Reddy, Y. Zhang, Composition, processing, and properties of biphasic zirconia bioceramics: relationship to competing strength and optical properties. Ceram. Int. 48, 17095–17103 (2022). https://doi.org/10.1016/j.ceramint.2022.02.26510.1016/j.ceramint.2022.02.265 ↗
36. H.-K. Kim, S.-H. Kim, Optical properties of pre-colored dental monolithic zirconia ceramics. J. Dent. 55, 75–81 (2016). https://doi.org/10.1016/j.jdent.2016.10.00110.1016/j.jdent.2016.10.001 ↗
37. F. Zhang, H. Reveron, B.C. Spies, B.V. Meerbeek, J. Chevalier, Trade-off between fracture resistance and translucency of zirconia and lithium-disilicate glass ceramics for monolithic restorations. Acta Biomater. 91, 24–34 (2019). https://doi.org/10.1016/j.actbio.2019.04.04310.1016/j.actbio.2019.04.043 ↗
38. L. Wang, K. Wang, Y. Sheng, Z. Hao, W. Tang, R. Dou, The effect of phase contents on the properties of yttria stabilized zirconia dental materials fabricated by stereolithography-based additive manufacturing. J. Mech. Behav. Biomed. Mater. 150, 106313 (2024). https://doi.org/10.1016/j.jmbbm.2023.10631310.1016/j.jmbbm.2023.106313 ↗
39. F. Zhang, B.V. Meerbeek, J. Vleugels, Importance of tetragonal phase in high-translucent partially stabilized zirconia for dental restorations. Dent. Mater. 36, 491–500 (2020). https://doi.org/10.1016/j.dental.2020.01.01710.1016/j.dental.2020.01.017 ↗
40. E. Roitero, H. Reveron, L. Gremillard, V. Garnier, C. Ritzberger, J. Chevalier, Ultra-fine Yttria-stabilized zirconia for dental applications: a step forward in the quest towards strong, translucent and aging resistant dental restorations. J. Eur. Ceram. Soc. 43, 2852–2863 (2023). https://doi.org/10.1016/j.jeurceramsoc.2022.11.04810.1016/j.jeurceramsoc.2022.11.048 ↗
41. S.N. Dokuzlu, M.G. Subaşı, Effect of sintering programs and surface treatments on monolithic zirconia. J. Adv. Prosthodont. 16, 25–37 (2024). https://doi.org/10.4047/jap.2024.16.1.2510.4047/jap.2024.16.1.25 ↗
42. H. Liu, M. Inokoshi, K. Xu, W. Tonprasong, S. Minakuchi, B.V. Meerbeek, J. Vleugels, F. Zhang, Does speed-sintering affect the optical and mechanical properties of yttria-stabilized zirconia? a systematic review and meta-analysis of in-vitro studies. Jpn. Dent. Sci. Rev. 59, 312–332 (2023). https://doi.org/10.1016/j.jdsr.2023.08.00710.1016/j.jdsr.2023.08.007 ↗
43. F.F. Lange, Transformation toughening. Pt.3. Experimental-observations in the ZrO2–Y2O3 system. J. Mater. Sci. 17, 240–246 (1982). https://doi.org/10.1007/Bf0080905910.1007/Bf00809059 ↗
44. A.M. Alshahrani, C.H. Lim, M.S. Wolff, M.N. Janal, Y. Zhang, Current speed sintering and high-speed sintering protocols compromise the translucency but not strength of yttria-stabilized zirconia. Dent. Mater. (2024). https://doi.org/10.1016/j.dental.2024.02.012. (in press)10.1016/j.dental.2024.02.012 ↗
45. P.V. Steyern, E. Bruzell, L. Vos, F.S. Andersen, A. Ruud, Sintering temperature accuracy and its effect on translucent yttria-stabilized zirconia: flexural strength, crystal structure, tetragonality and light transmission. Dent. Mater. 38, 1099–1107 (2022). https://doi.org/10.1016/j.dental.2022.04.02310.1016/j.dental.2022.04.023 ↗
46. T.D.C. Too, M. Inokoshi, K. Nozaki, M. Shimizubata, H. Nakai, H. Liu, S. Minakuchi, Influence of sintering conditions on translucency, biaxial flexural strength, microstructure, and low-temperature degradation of highly translucent dental zirconia. Dent. Mater. J. 40, 1320–1328 (2021). https://doi.org/10.4012/dmj.2020-44810.4012/dmj.2020-448 ↗
47. W. Du, Y. Ai, W. He, W. Chen, B. Liang, C. Lv, Formation and control of “intragranular” ZrO2 strengthened and toughened Al2O3 ceramics. Ceram. Int. 46, 8452–8461 (2020). https://doi.org/10.1016/j.ceramint.2019.12.08010.1016/j.ceramint.2019.12.080 ↗
48. W. Qian, Z. Zhang, S. Wang, Z. Guo, Y. Chen, M.A. Islam, Q. Zhao, H. Li, Y. Liu, H. Zhan, Enhancing the toughness of nano-composite coating for light alloys by the plastic phase transformation of zirconia. Int. J. Plast. 163, 103555 (2023). https://doi.org/10.1016/J.IJPLAS.2023.10355510.1016/J.IJPLAS.2023.103555 ↗
49. M. Trunec, P. Stastny, J. Kastyl, P. Roupcova, Z. Chlup, 2Y-TZP ceramics with high strength and toughness by optimizing the microstructure. J. Eur. Ceram. Soc. 44, 3258–3266 (2024). https://doi.org/10.1016/j.jeurceramsoc.2023.12.05710.1016/j.jeurceramsoc.2023.12.057 ↗
50. B. Osswald, F. Kern, Ytterbia—praseodymia co-stabilized TZP with high toughness and transformation limited strength. Open Ceram. 17, 100515 (2024). https://doi.org/10.1016/j.oceram.2023.10051510.1016/j.oceram.2023.100515 ↗
51. S. Lawson, Environmental degradation of zirconia ceramics. J. Eur. Ceram. Soc. 15, 485–502 (1995). https://doi.org/10.1016/0955-2219(95)00035-S10.1016/0955-2219(95)00035-S ↗
52. B. Deng, R. Zou, Y. Huang, L. Feng, Y. Chen, Effect of grain boundary segregation on aging resistance and mechanical properties of tetravalent element-doped 3YTZP ceramics for dental restoration. Int. J. Smart Nano Mater. (2023). https://doi.org/10.1080/19475411.2023.219786610.1080/19475411.2023.2197866 ↗
53. K. Matsui, K. Nakamura, M. Saito, A. Kuwabara, H. Yoshida, Y. Ikuhara, Low temperature degradation in yttria-stabilized tetragonal zirconia polycrystal: effect of Y3+ distribution in grain interiors. Acta Mater. 227, 117659 (2022). https://doi.org/10.1016/j.actamat.2022.11765910.1016/j.actamat.2022.117659 ↗
54. J. Chevalier, L. Gremillard, S. Deville, Low-temperature degradation of zirconia and implications for biomedical implants. Annu. Rev. Mater. Res. 37, 1–32 (2007). https://doi.org/10.1146/annurev.matsci.37.052506.08425010.1146/annurev.matsci.37.052506.084250 ↗
55. K. Matsui, H. Yoshida, Y. Ikuhara, Nanocrystalline, ultra-degradation-resistant zirconia: Its grain boundary nanostructure and nanochemistry. Sci. Rep. 4, 1–6 (2014). https://doi.org/10.1038/srep0475810.1038/srep04758 ↗
56. V. Koenig, T. Douillard, J. Chevalier, F. Amiard, M. Lamy de la Chapelle, S. Le Goff, A. Vanheusden, N. Dardenne, C. Wulfman, A. Mainjot, Intraoral low-temperature degradation of monolithic zirconia dental prostheses: 5-year results of a prospective clinical study with ex vivo monitoring. Dent. Mater. 40, 198–209 (2024). https://doi.org/10.1016/j.dental.2023.11.00810.1016/j.dental.2023.11.008 ↗
57. L. Gremillard, J. Chevalier, T. Epicier, G. Fantozzi, Improving the durability of a biomedical-grade zirconia ceramic by the addition of silica. J. Am. Ceram. Soc. 85, 401–407 (2002). https://doi.org/10.1111/j.1151-2916.2002.tb00103.x10.1111/j.1151-2916.2002.tb00103.x ↗
58. F. Zhang, J. Chevalier, C. Olagnon, B. Van Meerbeek, J. Vleugels, Slow crack growth and hydrothermal aging stability of an alumina-toughened zirconia composite made from La2O3-doped 2Y-TZP. J. Eur. Ceram. Soc. 37, 1865–1871 (2017). https://doi.org/10.1016/j.jeurceramsoc.2016.11.00310.1016/j.jeurceramsoc.2016.11.003 ↗
59. A.A. Nogiwa-Valdez, W.M. Rainforth, P. Zeng, I.M. Ross, Deceleration of hydrothermal degradation of 3Y-TZP by alumina and lanthana co-doping. Acta Biomater. 9, 6226–6235 (2013). https://doi.org/10.1016/j.actbio.2012.11.02710.1016/j.actbio.2012.11.027 ↗
60. F. Zhang, K. Vanmeensel, M. Batuk, J. Hadermann, M. Inokoshi, B. Van Meerbeek, I. Naert, J. Vleugels, Highly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation. Acta Biomater. 16, 215–222 (2015). https://doi.org/10.1016/j.actbio.2015.01.03710.1016/j.actbio.2015.01.037 ↗
61. A. Kurihara, K. Nakamura, S. Shishido, R. Inagaki, A. Harada, T. Kanno, H. Egusa, Mechanism underlying ultraviolet-irradiation-induced discoloration of dental zirconia ceramics stabilized with 3 and 5 mol% yttria. Ceram. Int. 50, 12136–12145 (2024). https://doi.org/10.1016/j.ceramint.2024.01.11710.1016/j.ceramint.2024.01.117 ↗
62. Z. Xiaoqing, J. Yu, D. Cao, R. Yang, T. Wu, W. Ye, W. Zhou, M. Xu, M. Yang, X. Xu, X. Yu, X. Cui, Reversible discoloration mechanism of irradiated blue cubic zirconia single crystals. Opt. Mater. 149, 114958 (2024). https://doi.org/10.1016/j.optmat.2024.11495810.1016/j.optmat.2024.114958 ↗
63. J. Wang, J. Li, Y. Li, L. Li, X. Su, Y. Hu, X. Xu, One-step synthesis and low-temperature rapid sintering of alumina-zirconia ceramics by flash sintering combined with phase transformation. Mater Charact 209, 113771 (2024). https://doi.org/10.1016/j.matchar.2024.11377110.1016/j.matchar.2024.113771 ↗
64. Y. Lu, L. Wang, A.M.O.D. Piva, J.P.M. Tribst, S.M. Čokić, F. Zhang, A. Werner, C.J. Kleverlaan, A.J. Feilzer, Effect of printing layer orientation and polishing on the fatigue strength of 3D-printed dental zirconia. Dent. Mater. 40, 190–197 (2024). https://doi.org/10.1016/j.dental.2023.11.00710.1016/j.dental.2023.11.007 ↗
65. Y.S. Romario, C. Bhat, M. Ramezani, T. Pasang, Z. Chen, C.-P. Jiang, Fabrication of translucent graded dental crown using zirconia-yttrium multi-slurry tape casting 3D printer. J. Mech. Behav. Biomed. Mater. 152, 106406 (2024). https://doi.org/10.1016/j.jmbbm.2024.10640610.1016/j.jmbbm.2024.106406 ↗