Property of MgO with Different Sintering Temperatures under High Pressures

Jeongho Song, Yunyoung Noh, Ohsung Song

Abstract

We investigated the property changes of MgO powders sintered at temperatures ranging from 700 o C to 1900 o C for 5minutes at a pressure of 2.7 GPa for a high-pressure high-temperature(HPHT) diamond synthesis process. The physical properties of the sintered MgO powders were characterized by optical microscopy, field emission scanning electron microscopy (FE-SEM), Vickers hardness tests, and by the apparent density, and X-ray diffractometry. An optical micro-analysis showed that white MgO powders became black after sintering due to carbon contamination from the graphite heat source. FE-SEM revealed the growth in the grain size of the MgO powders from 0.3 m to 50 m after sintering at 1700 o C. The hardness and apparent density increased to 1800 o C while the samples were dedensified at 1900 o C due to the growth of isolated pores. According to the XRD analysis, no phase transformation occurred in the MgO powders. These results suggest that HPHT-sintered MgO powders can show an accelerated sintering process characterized by grain neck growth, pore connections, isolated pore growth and dedensification in 5 minutes, while these processes with the conventional sintering process take at least 5 hours.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-pressure geophysics and materials · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.