article·2013-11-30Open access

Hot Corrosion Behavior of Plasma Sprayed 4 mol% Y2O3-ZrO2Thermal Barrier Coatings with Volcanic Ash

Wonjun Lee, Byung-Koog Jang, Dae‐Soon Lim, Yoon‐Suk Oh, Seong-Won Kim, Hyung-Tae Kim, Hiroshi Araki, Hideyuki Murakami, Seiji Kuroda

Abstract

The hot corrosion behavior of plasma sprayed 4 mol% Y 2 O 3 -ZrO 2 (YSZ) thermal barrier coatings (TBCs) with volcanic ash is investigated.Volcanic ash that deposited on the TBCs in gas-turbine engines can attack the surface of TBCs itself as a form of corrosive melt.YSZ coating specimens with a thickness of 430-440 µm are prepared using a plasma spray method.These specimens are subjected to hot corrosion environment at 1200 o C with five different duration time, from 10 mins to 100 h in the presence of corrosive melt from volcanic ash.The microstructure, composition, and phase analysis are performed using Field emission scanning electron microscopy, including Energy dispersive spectroscopy and X-ray diffraction.After the heat treatment, hematite (Fe 2 O 3 -TiO 2 ) and monoclinic YSZ phases are found in TBCs.Furthermore the interface area between the molten volcanic ash layers and YSZ coatings becomes porous with increases in the heat treatment time as the YSZ coatings dissolved into molten volcanic ash.The maximum thickness of this a porous reaction zone is 25 µm after 100 h of heat treatment.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.