Low Temperature Sintering Additives for Mullite Ceramics

Chang-Bin Lim, DongHun Yeo, Hyo-Soon Shin, Yong Soo Cho

Publisher page

Abstract

Additives for low temperature sintering of mullite ceramics were investigated for matching Mo-Cu conducting paste with that ceramics at 1,400℃. SiO 2 , MgO and Y 2 O 3 were chosen as the additives for low temperature sintering, and the amounts of those additives were varied with sintering temperature of 1,400℃ to 1,500℃. With additives of 1.0 wt% of SiO 2 , 1.0 wt% of MgO, and 1.5 wt% of Y 2 O 3 , the densest sintered body of 3.12 g/㎤ was obtained at 1,400℃ in reducing atmosphere. The flexural strength of that was 325 MPa and the CTE (Coefficient of thermal expansion) was 4.33 ppm/℃.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.