A Study on the Thermal Stability of an Al2O3/SiON Stack Structure for c-Si Solar Cell Passivation Application
Source abstract
Abstract
We investigated the influence of blistering on Al 2 O 3 /SiON stacks and Al 2 O 3 /SiNx:H stacks passivation layers. Al 2 O 3 film provides outstanding Si surface passivation quality. Al 2 O 3 film as the rear passivation layer of a p-type Si solar cell is usually stacked with a capping layer, such as SiO 2 , SiNx, and SiON films. These capping layers protect the thin Al 2 O 3 layer from an Al electrode during the annealing process. We compared Al 2 O 3 /SiON stacks and Al 2 O 3 /SiNx:H stacks through surface morphology and minority carrier lifetime after annealing processes at 450 o C and 850 o C. As a result, the Al 2 O 3 /SiON stacks were observed to produce less blister phenomenon than Al 2 O 3 /SiNx:H stacks. This can be explained by the differences in the H species content. In the process of depositing SiNx film, the rich H species in NH 3 source are diffused to the Al 2 O 3 film. On the other hand, less hydrogen diffusion occurs in SiON film as it contains less H species than SiNx film. This blister phenomenon leads to an increase insurface defect density. Consequently, the Al 2 O 3 /SiON stacks had a higher minority carrier lifetime than the Al 2 O 3 /SiNx:H stacks.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.