Study on the Synthesis by Milling and Solid-State Reaction Method and Electrochemical Properties of LiNiO2
Source abstract
Abstract
LiNiO₂ was synthesized by the solid-state method after mixing LiOHㆍH₂O and Ni(OH)₂ with SPEX milt. The optimum condition for the synthesis of LiNiO₂ was the calcination at 750℃ for 30 h in O₂ stream after milling for 1 h. The LiNiO₂ synthesized under this condition showed relatively large value of I 003 /I 104 and relatively small value of R-factor. When LiNiO₂ was cycled in 2.7~4.15 V at 0.1C-rate, the first discharge capacity was not very large (145.8 mAh/g) but it showed good cycling performance. When LiNiO₂ was cycled in 2.7~4.2 V at 0.1 C-rate, the first discharge capacity was large but it showed poor cycling performance probably because of the transition of H2 hexagonal structure to H3 hexagonal structure. In addition, when LiNiO₂ was cycled in 1.0~4.8 V at 1/24C-rate, the first discharge capacity was very large (257.7 mAh/g) and the discharge capacity increased with the number of cycles.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Supercapacitor Materials and Fabrication
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.