Synthesis of the Nano-sized SrAl2O4Phosphors by Wet Processing and its Photoluminescence Properties
Source abstract
Abstract
and co-doped strontium aluminate, long phosphorescent phoshor was fabricated and its photoluminescence was characterized. The phosphor, was synthesized by a coprecipitation in which metal salts of , , were dissolved in solution with adding and as a activator and co-activator, respectively. The coprecipitated products were separated from solution, washed, and dried in a vacuum dry oven. The dried powders were then mixed with 3 wt% as a flux and heated at for 3 h under the reducing ambient atmosphere of 95%Ar+ gases. For the synthesized , properties of photoluminescence such as emission, excitation and decay time were examined. The emission intensity increased as the annealing temperature increased and showed a maximum peak intensity at 510 nm with a broad band from . Monitored at 520 nm, the excitation spectrum showed a maximum peak intensity at wavelength with a broad band from wavelength. The decay time of increased as the annealing temperature increased.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.