Dependence of Crosslinking Temperature on Swelling Behavior of Hyaluronic Acid Porous Microbeads Synthesized by a Modified Spray Method

Younghun Kim, In‐Kyu Lee, Jintae Kim, Ju-Hyun Park, Deuk Yong Lee

Abstract

Hyaluronic acid (HA) microbeads were synthesized by dropping 0.5 wt% of sodium hyaluronate dissolved in NaOH into 0.2 vol% of divinyl sulfone dissolved in 2-methyl-1propanol at a speed of 0.005 ml/min. HA microbeads were collected from a divinyl sulfone crosslinker solution stirred at 200 to 400 rpm for 5 h at temperatures from room temperature to 60 o C at intervals of 10 o C. The crosslinked microbeads were then cleaned thoroughly using distilled water and ethanol. SEM results revealed that the microbeads were white-colored spheres. The 3-D porous network structure of the microbeads became dense with an increase in the crosslinking temperature; however, no dependence of the crosslinking temperature on the microbead size was detected. The extent of swelling decreased from 970% to 670% with an increase in the crosslinking temperature from room temperature to 60 o C, most likely due to the increase in the degree of crosslinking.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogels: synthesis, properties, applications · Collagen: Extraction and Characterization · Proteoglycans and glycosaminoglycans research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.