article·2015-07-31Open access

A Surface Etching for Synthetic Diamonds with Nano-Thick Ni Films and Low Temperature Annealing

Jeongho Song, Yunyoung Noh, Ohsung Song

Abstract

Ni (100 nm thick) was deposited onto synthesized diamonds to fabricate etched diamonds. Next, those diamonds were annealed at varying temperatures (400 ~1200 o C) for 30 minutes and then immersed in 30 wt% HNO 3 to remove the Ni layers. The etched properties of the diamonds were examined with FE-SEM, micro-Raman, and VSM. The FE-SEM results showed that the Ni agglomerated at a low annealing temperature (~400 o C), and self-aligned hemisphere dots formed at an annealing temperature of 800 o C. Those dots became smaller with a bimodal distribution as the annealing temperature increased. After stripping the Ni layers, etch pits and trigons formed with annealing temperatures above 400 o C on the surface of the diamonds. However, surface graphite layers existed above 1000 o C. The B-H loop results showed that the coercivity of the samples increased to 320 Oe (from 37 Oe) when the annealing temperature increased to 600 o C and then, decreased to 150 Oe with elevated annealing temperatures. This result indicates that the coercivity was affected by magnetic domain pinning at temperatures below 600 o C and single domain behavior at elevated temperatures above 800 o C consistent with the microstructure results. Thus, the results of this study show that the surface of diamonds can be etched.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Graphene research and applications · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.