Effect of Alkaline-Earth Oxide Additives on Flexural Strength of Clay-Based Membrane Supports
Source abstract
Abstract
Low-cost ceramic membrane supports with pore sizes in the range of 0.52-0.62 μm were successfully prepared by uniaxial dry compaction method using inexpensive raw materials including kaolin, bentonite, talc, sodium borate, and alkaline-earth oxides in carbonate forms (e.g., MgCO₃, CaCO₃, and SrCO₃). The prepared green supports were sintered at 1000℃ for 8 hr in air. The effect of alkaline-earth oxide additives on the flexural strength of clay-based membrane supports was investigated. The porosity of the clay-based membrane supports was found to be in the range of 33-34%. The flexural strength of the clay-based membrane supports with 1% alkaline-earth carbonates was found to be in the range of 42.8-52.7 MPa. The addition of alkaline-earth carbonates to clay-based membrane supports resulted in large increases (47-80%) in the flexural strength of the membrane supports, compared to that of membrane supports without alkaline-earth carbonates. The typical flexural strength of the clay-based membrane support with 1% SrCO₃ was 52.7 MPa at 33.8% porosity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Grouting, Rheology, and Soil Mechanics · Microbial Applications in Construction Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.