Heat Treatment Effect on the Microstructure of 8YSZ Thick Film
Source abstract
Abstract
In order to fabricate 8YSZ thick film by silk screen printing, YSZ(yttria-stabilized zirconia) commercial powder was used as starting materials. Paste for screen printing was made by mixing 8YSZ powder and organic vehicles. 8YSZ thick film was formed on Al₂O₃ substrate. The crystal structure, and microstructure were investigated. Grain size of 8YSZ was increased with increasing calcination temperature and rapid grain growth was shown after calcination at 1300℃. Microstructure showed the mixture of large and small grain size after 1400℃ sintering. Shrinkage rate of 8YSZ thick film sintered at 1400℃ was more than 40%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.