A Study on the Electrical Properties of Al2O3/La2O3/Al2O3Multi-Stacked Films Using Tunnel Oxide Annealed at Various Temperatures
Source abstract
Abstract
The structural and electrical properties of Al 2 O 3 /La 2 O 3 /Al 2 O 3 (ALA) films using a tunnel oxide annealed at various temperatures were investigated. The program/erase properties of the ALA films using the tunnel oxide annealed at 600 o C were superior to others. The program/erase voltage and time of the ALA films using the tunnel oxide annealed at 600 o C were 11 V for 10 ms (program) and -11 V for 100 ms (erase), respectively, and the corresponding memory window was about 1.59 V. In the retention test, the V th distributions of all films were not changed up to about 10 4 cycles. In this study, all data showed sufficient characteristics to be used in flash memory devices.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.