Properties of Al2O3-SiCwComposites Fabricated by Three Preparation Methods
Source abstract
Abstract
Al 2 O 3 -SiC composites reinforced with SiC whisker (SiC w ) were fabricated using three different methods. In the first, Al 2 O 3 -SiC w starting materials were used. In the second, Al 2 O 3 -SiC w -SiC particles (SiC p ) were used, which was intended to enhance the mechanical properties by SiC p reinforcement. In the third method, reaction-sintering was used with mullite-Al-C-SiC w starting materials. After hotpressing at 1750 o C and 30 MPa for 1 h, the composites fabricated using Al 2 O 3 -SiC w and Al 2 O 3 -SiC w -SiC p showed strong mechanical properties, by which the effects of reinforcement by SiC w and SiC p were confirmed. On the other hand, the mechanical properties of the composite fabricated by reaction-sintering were found to be inferior to those of the other Al 2 O 3 -SiC composites owing to its relatively lower density and the presence of -Al 2 O 3 and -Al 2.67 O 4 . The greatest hardness and K 1C were 20.37 GPa for the composite fabricated using Al 2 O 3 -SiC w , and 4.9 MPam 1/2 using Al 2 O 3 -SiC w -SiC p , respectively, which were much improved over those from the monolithic Al 2 O 3 .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.