Preparation of Ce0.8Gd0.2O1.9Powder by Milling of CeO2Slurry and Oxalate Precipitation
Source abstract
Abstract
CeO 2 Ce 0.8 Gd 0.2 O 1.9 (2009 11 5 ; 2010 1 8 ; 2010 1 25 ) ABSTRACT Ce 0.8 Gd 0.2 O 1.9 (GDC20) powder was synthesized by milling of CeO 2 slurry and Gd oxalate precipitation. The mixture of CeO 2 powder and Gd precipitates calcined at 600 o C for 2 h showed the particle size distribution similar to that of CeO 2 powder, which had been milled during the synthesis process. Attrition milling of the calcined powder with an average particle size of 0.36 m for 2 h resulted in a decrease in the particle size to 0.24 m. Although the milled powder consisted of small particles(<1 m), a small amount of fine platy Gd 2 O 3 particles, which had been survived in the milling process, was observed. Sintering of the powder compacts for 4 h showed relative densities of 80.7% at 1300 o C and 97% at 1400 o C, respectively. Densification was found to almost complete at 1500 o C, resulting in a dense and homogeneous microstructure with a relative density of 99.5%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.