Effect of Silicate Ions on the Hydration of 4CaO · Al2O3· Fe2O3with Gypsum
Source abstract
Abstract
Na₂Si₂O 5 added to the solution affects the hydration of 4CaO·Al₂O₃·Fe₂O₃ with calcium sulfate. The reaction between 4CaO·Al₂O₃·Fe₂O₃ and CaSO₄·2H₂O decrease with increasing amount of Na₂Si₂O 5 in solution, owing to low hydraulic reactivity of 4CaO·Al₂O₃·Fe₂O₃ by the adsorption of silicate ions on the surface of 4CaO·Al₂O₃·Fe₂O₃ particles. The dissolution rate of 4CaO·Al₂O₃·Fe₂O₃ particles deceased with the increase of the concentration of silicate ion in solution. When the 4CaO·Al₂O₃·Fe₂O₃ particles was hydrated in gypsum - Na₂Si₂O 5 solution, the hydration was retarded and the rate could not discriminate between formation of ettringite and that of monosulfate, and it stopped in high concentration of silicate ions. However, silicate ion did not any effect on the dissolution rate of gypsum.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Grouting, Rheology, and Soil Mechanics · Concrete and Cement Materials Research · Mine drainage and remediation techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.