Preparation of Ce0.8Gd0.2O1.9 Powder Using CeO2 Powder and Gd Precipitation and Effect of CoO doping on Sintering
Source abstract
Abstract
Ce 0.8 Gd 0.2 O 1.9 (GDC20) powder was prepared from a mixture of submicron-sized CeO 2 powder and Gd precipitates using ammonium carbonate ((NH 4 ) 2 CO 3 ) as a precipitant. The mixture was calcined at 700 o C for 4 h followed by ball-milling that resulted in the GDC powder with an average particle size of 0.46 m. The powder had a very uniform particle size distribution with particle sizes ranging from 0.3 m to 1 m. Sintering of undoped GDC samples did not show a relative density of 99.2% until the temperature was increased to 1500 o C, whereas GDC samples doped with 5 mol% CoO exhibited a significant densification at lower temperature reaching a relative density of 97.6% at 1100 o C and of 98.8% at 1200 o C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.