Characteristics of PZT Powders Synthesized by Hydrothermal Process

Beom-Seok Yang, Huk-Hee Lee, Chang-Whan Won, Beom-Seok Yang, Huk-Hee Lee, Chang-Whan Won

Abstract

Conditions for formation of perovskite Pb(Zr 0.52 Ti 0.48 )O₃ phase by the hydrothermal synthesis are investigated. Pb(Zr 0.52 Ti 0.48 )O₃ ceramics were synthesized by hydrothermal process above 180℃ for 2 h reaction using 5~30 M KOH solution as a mineralizer. Particle size increases in proportion to the mineralizer concentration. As a result of EDX analysis, PZT powders synthesized using 50 M of KOH as a mineralizer were considered as 2.42 mol% K doped-PZT powders. And 2.42 mol% K doped-PZT has much higher mechanical quality factor than undoped PZT ceramics. The sintering properties showed 7.987 g/㎤ of sintered density and 3~4 ㎛ of grain size.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.