Ti–6Al–4V triply periodic minimal surface structures for bone implants fabricated via selective laser melting
Source abstract
Abstract
Triply periodic minimal surface (TPMS) structures have already been shown to be a versatile source of biomorphic scaffold designs. Therefore, in this work, Ti-6Al-4V Gyroid and Diamond TPMS lattices having an interconnected high porosity of 80-95% and pore sizes in the range of 560-1600 μm and 480-1450 μm respectively were manufactured by selective laser melting (SLM) for bone implants. The manufacturability, microstructure and mechanical properties of the Ti-6Al-4V TPMS lattices were evaluated. Comparison between 3D micro-CT reconstructed models and original CAD models of the Ti-6Al-4V TPMS lattices shows excellent reproduction of the designs. The as-built Ti-6Al-4V struts exhibit the microstructure of columnar grains filled with very fine and orthogonally oriented α' martensitic laths with the width of 100-300 nm and have the microhardness of 4.01 ± 0.34 GPa. After heat treatment at 680°C for 4h, the α' martensite was converted to a mixture of α and β, in which the α phase being the dominant fraction is present as fine laths with the width of 500-800 nm and separated by a small amount of narrow, interphase regions of dark β phase. Also, the microhardness is decreased to 3.71 ± 0.35 GPa due to the coarsening of the microstructure. The 80-95% porosity TPMS lattices exhibit a comparable porosity with trabecular bone, and the modulus is in the range of 0.12-1.25 GPa and thus can be adjusted to the modulus of trabecular bone. At the same range of porosity of 5-10%, the moduli of cortical bone and of the Ti-6Al-4V TPMS lattices are in a similar range. Therefore, the modulus and porosity of Ti-6Al-4V TPMS lattices can be tailored to the levels of human bones and thus reduce or avoid "stress shielding" and increase longevity of implants. Due to the biomorphic designs, and high interconnected porosity and stiffness comparable to human bones, SLM-made Ti-6Al-4V TPMS lattices can be a promising material for load bearing bone implants.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
2. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
3. Medical design: direct metal laser sintering of Ti–6Al–4V10.1016/j.matdes.2010.02.050 ↗
4. Solid-state foaming of titanium by superplastic expansion of argon-filled pores10.1557/JMR.2001.0210 ↗
5. Phase transformation dynamics during welding of Ti–6Al–4V10.1063/1.1737476 ↗
6. Osteoinduction of porous bioactive titanium metal10.1016/S0142-9612(03)00551-9 ↗
7. Fiber metal composites in the fixation of skeleta1 prosthesis10.1002/jbm.820070305 ↗
8. Gibson · 1997
9. Gong · 2013
10. In situ characterization of the deformation and failure behavior of non-stochastic porous structures processed by selective laser melting10.1016/j.msea.2011.07.026 ↗
11. Design and additive manufacturing of cellular lattice structures
12. Compression-compression fatigue of selective electron beam melted cellular titanium (Ti–6Al–4V)10.1002/jbm.b.31901 ↗
13. Direct metal fabrication of titanium implants with tailored materials and mechanical properties using electron beam melting technology10.1016/j.msec.2007.04.022 ↗
14. Cellular Ti–6Al–4V structures with interconnected macro porosity for bone implants fabricated by selective electron beam melting10.1016/j.actbio.2008.03.013 ↗
15. The relationship between stress shielding and bone resorption around total hip stems and the effects of flexible materials10.1097/00003086-199201000-00014 ↗
16. Minimal surface scaffold designs for tissue engineering10.1016/j.biomaterials.2011.06.012 ↗
17. Evaluation of titanium alloys fabricated using rapid prototyping technologies-electron beam melting and laser beam melting10.3390/ma4101776 ↗
18. Study of laser-sinterability of ferro-based powders10.1108/13552540510623594 ↗
19. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
20. A novel porous Ti6Al4V: characterization and cell attachment10.1002/jbm.a.30278 ↗
21. Mathematically defined tissue engineering scaffold architectures prepared by stereolithography10.1016/j.biomaterials.2010.05.068 ↗
22. Effects of the architecture of tissue engineering scaffolds on cell seeding and culturing10.1016/j.actbio.2010.06.012 ↗
23. Characterization of Ti–6Al–4V open cellular foams fabricated by additive manufacturing using electron beam melting10.1016/j.msea.2009.11.015 ↗
24. Selective laser melting: a regular unit cell approach for the manufacture of porous, titanium, bone in-growth constructs, suitable for orthopedic applications10.1002/jbm.b.31219 ↗
25. Mechanical properties of porous titanium compacts prepared by powder sintering10.1016/j.scriptamat.2003.08.018 ↗
26. Mechanical evaluation of porous titanium (Ti6Al4V) structures with electron beam melting (EBM)10.1016/j.jmbbm.2009.10.006 ↗
27. Schwarz meets Schwann: design and fabrication of biomorphic and durataxic tissue engineering scaffolds10.1016/j.media.2006.06.001 ↗
28. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
29. Microstructure and mechanical behavior of porous Ti–6Al–4V parts obtained by selective laser melting10.1016/j.jmbbm.2013.05.011 ↗
30. Hot working of commercial Ti–6Al–4V with an equiaxed α–β microstructure: materials modeling considerations10.1016/S0921-5093(00)00741-3 ↗
31. Comparison of the mechanical properties between tantalum and nickel-titanium foamsimplant materials for bone ingrowth applications10.1016/j.jallcom.2006.08.069 ↗
32. Schoen, A.H., 1970. Infinite Periodic Minimal Surfaces Without Self-Intersections. NASA Technical Report TN D-5541, Washington, DC.
33. Schwarz · 1885
34. Biomaterials and bone mechanotransduction10.1016/S0142-9612(01)00002-3 ↗
35. Simonelli · 2014
36. Osteoblast and Chondrocyte interactions during coculture on scaffolds10.1109/MEMB.2003.1256269 ↗
37. A study of the micro structural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
38. Macropore tissue ingrowth: quantitative and qualitative hydroxyapatite ceramic10.1016/0142-9612(86)90071-2 ↗
39. Selective laser melting of Ti6Al4V alloy for biomedical applications: Temperature monitoring and microstructural evolution10.1016/j.jallcom.2013.08.183 ↗
40. Evaluations of cellular lattice structures manufactured using selective laser melting10.1016/j.ijmachtools.2012.06.002 ↗
41. Using electroactive substrates to pattern the attachment of two different cell populations10.1073/pnas.101112898 ↗
42. Micro-CT-based improvement of geometrical and mechanical controllability of selective laser melted Ti6Al4V porous structures10.1016/j.msea.2011.06.045 ↗
43. Pore throat size and connectivity determine bone and tissue ingrowth into porous implants: three-dimensional micro-CT based structural analyses of porous bioactive titanium implants10.1016/j.biomaterials.2006.08.013 ↗
44. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗