Ultra high molecular weight polyethylene: Mechanics, morphology, and clinical behavior
Source abstract
Abstract
Ultra high molecular weight polyethylene (UHMWPE) is a semicrystalline polymer that has been used for over four decades as a bearing surface in total joint replacements. The mechanical properties and wear properties of UHMWPE are of interest with respect to the in vivo performance of UHMWPE joint replacement components. The mechanical properties of the polymer are dependent on both its crystalline and amorphous phases. Altering either phase (i.e., changing overall crystallinity, crystalline morphology, or crosslinking the amorphous phase) can affect the mechanical behavior of the material. There is also evidence that the morphology of UHMWPE, and, hence, its mechanical properties evolve with loading. UHMWPE has also been shown to be susceptible to oxidative degradation following gamma radiation sterilization with subsequent loss of mechanical properties. Contemporary UHMWPE sterilization methods have been developed to reduce or eliminate oxidative degradation. Also, crosslinking of UHMWPE has been pursued to improve the wear resistance of UHMWPE joint components. The 1st generation of highly crosslinked UHMWPEs have resulted in clinically reduced wear; however, the mechanical properties of these materials, such as ductility and fracture toughness, are reduced when compared with the virgin material. Therefore, a 2nd generation of highly crosslinked UHMWPEs are being introduced to preserve the wear resistance of the 1st generation while also seeking to provide oxidative stability and improved mechanical properties.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Orthopedic Infections and Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Anon, 2007. Canadian joint replacement registry report. Canadian Institute for Health and Information
2. AAOS (Ed.) 2008. Burden of musculoskeletal disease in the united states: Prevalence, societal and economic cost. American Academy of Orthopaedic Surgeons, Rosemount, IL
3. Influence of election beam irradiation dose on the properties of crosslinked UHMWPE
4. Aseptic loosening of total joint replacements: Mechanisms underlying osteolysis and potential therapies10.1186/ar2170 ↗
5. The performance of gamma- and EtO-sterilised UHMWPE acetabular cups tested under severe simulator conditions. Part 2: Wear particle characteristics with isolation protocols10.1016/S0142-9612(03)00264-3 ↗
6. A three-dimensional constitutive model for the large stretch behaviour of rubber elastic materials10.1016/0022-5096(93)90013-6 ↗
7. The porous-coated anatomic total hip prosthesis: Failure of the metal-backed acetabular component
8. ASTM, 2000. D 4020-00a: Standard specification for ultra-high-molecular-weight polyethylene molding and extrusion materials
9. The effects of degree of crosslinking on the fatigue crack initiation and propagation resistance of orthopedic-grade polyethylene10.1002/jbm.a.10606 ↗
10. Jumbo femoral head for the treatment of recurrent dislocation following total hip replacement10.2106/00004623-200202000-00013 ↗
11. Constitutive modeling of the large strain time-dependent behaviour of elastomers10.1016/S0022-5096(97)00075-6 ↗
12. Deformation of elastomeric networks: Relation between molecular level deformation and classical statistical mechanics models of rubber elasticity
13. An augmented hybrid constitutive model for simulation of unloading and cyclic loading behavior of conventional and highly crosslinked UHMWPE10.1016/j.biomaterials.2003.08.065 ↗
14. Prediction of multiaxial mechanical behavior for conventional and highly crosslinked UHMWPE using a hybrid constitutive model10.1016/S0142-9612(02)00514-8 ↗
15. Molecular chain stretch is a multiaxial failure criterion for conventional and highly crosslinked UHMWPE10.1016/j.orthres.2004.08.014 ↗
16. Constitutive Modeling of ultra-high molecular weight polyethylene under large-deformation and cyclic loading conditions10.1016/S0142-9612(01)00367-2 ↗
17. Catastrophic failure of the polyethylene liner of uncemented acetabular components
18. Biomet Inc., 2008. Arcom XL revised v3. Retrieved May 9, 2008, from www.biomet.com
19. Cracking and impingement in ultra-high-molecular-weight polyethylene acetabular liners10.1016/j.arth.2005.05.001 ↗
20. Oxidation behaviour in prosthetic UHMWPE components sterilised with high-energy radiation in the presence of oxygen10.1016/j.polymdegradstab.2006.08.002 ↗
21. Time resolved simultaneous small- and wide-angle x-ray scattering during polyethylene deformation-II. Cold drawing of linear polyethylene10.1016/S0032-3861(97)00226-7 ↗
22. Fracture of the polyethylene tibial post in a NexGen posterior-stabilized knee prosthesis10.1016/j.arth.2004.04.013 ↗
23. Impact of gamma sterilization on clinical performance of polyethylene in the knee10.1016/S0883-5403(96)80026-X ↗
24. Mechanisms of failure of modular prostheses
25. Mechanisms of crosslinking and oxidative degradation of UHMWPE
26. Courtney · 2000
27. Crane, D.J., Pruitt, L., et al. 1999. Plasticity induced damage layer and lamellar alignment detected in UHMWPE: A comparison of retrievals and simulator components. In: Transactions of the 25th Society for Biomaterials
28. Shelf life and in vivo duration. Impacts on performance of tibial bearings
29. In vivo oxidation of gamma-barrier-sterilized ultra-high-molecular-weight polyethylene bearings10.1016/j.arth.2006.07.006 ↗
30. Five-year experience with crossfire highly cross-linked polyethylene10.1097/00003086-200512000-00024 ↗
31. The effect of patient gait on the material properties of UHMWPE in hip replacements10.1016/j.biomaterials.2005.01.007 ↗
32. Highly cross-linked polyehtylene in total hip arthroplasty10.1097/01.blo.0000150314.70919.e3 ↗
33. Clinical performance of a durasul highly cross-linked polyethylene acetabular liner for total hip arthroplasty at five years
34. Dowling · 1999
35. Basis for a second generation highly crosslinked UHMWPE10.1097/01.blo.0000238856.61862.7d ↗
36. Degradation of mechanical behavior in UHMWPE after natural and accelerated aging10.1016/S0142-9612(00)00021-1 ↗
37. Edidin, A.A., Kurtz, S.M., 2000. The evolution of paradigms for wear in total joint arthroplasty; the role of design, material, and mechanics
38. A randomized, prospective evaluation of outcome after total hip arthroplasty using cross-linked marathon and non-cross-linked enduron polyethylene10.1016/j.arth.2006.02.012 ↗
39. The obesity epidemic: Its effect on total joint arthroplasty10.1016/j.arth.2007.04.014 ↗
40. Effect of annealing and temperature on the morphological structure of polymers10.1351/pac197231010113 ↗
41. Morphological alteration during texture-producing plastic plane strain compression of high-density polyethylene10.1021/ma00047a023 ↗
42. Large diameter femoral heads on highly cross-linked polyethythlene10.1097/01.blo.0000218742.61624.80 ↗
43. Fatigue crack propagation resistance of virgin and highly crosslinked, thermally treated ultra-high molecular weight polyethylene10.1016/j.biomaterials.2005.09.010 ↗
44. Failure micromechanisms during uniaxial tensile fracture of conventional and highly crosslinked ultra-high molecular weight polyethylenes used in total joint replacement10.1016/S0142-9612(03)00277-1 ↗
45. The effects of gamma radiation sterilization and ageing on the structure and morphology of medical grade ultra high molecular weight polyethylene10.1016/0032-3861(96)89386-4 ↗
46. J-integral fracture toughness and tearing modulus measurement of radiation cross-linked UHMWPE10.1016/S0736-0266(02)00073-6 ↗
47. The effects of raw material, irradiation dose, and irradiation source on crosslinking of UHMWPE
48. Recurrent dislocation after revision total hip replacement with a large prosthetic femoral head–A case report10.2106/00004623-200404000-00025 ↗
49. A constitutive model for the nonlinear viscoplastic behavior of glassy polymers10.1002/pen.760350407 ↗
50. Hearle · 1982
51. Fracture of the central polyethylene tibial spine in posterior stabilized total knee arthroplasty10.1016/S0883-5403(03)00192-X ↗
52. The role of macrophages in osteolysis of total joint replacement10.1016/j.biomaterials.2004.04.035 ↗
53. ISO, 2001. 11542-1: Plastics–Ultra-high-molecular-weight polyethylene (PE-UHMW) moulding and extrusion materials–Part 1: Designation system and basis for specifications
54. The effect of protein adsorption on the friction behavior of UHMWPE10.1007/s11249-006-9078-8 ↗
55. Early femoral head penetration of a highly cross-linked polyethylene liner vs a conventional polyethylene liner: A case-controlled study10.1016/j.arth.2005.05.008 ↗
56. 2004
57. Kurtz, S., Bergstrom, J., et al. 2007. Validation of hybrid model and ultimate chain stretch criterion for a second-generation highly crosslinke UHMWPE. In: 6th Combined Meeting of the ORS, Orthopaedic Research Society, Honolulu, Hawaii, Poster 498
58. Mechanical properties of retrieved highly cross-linked crossfire liners after short-term implantation10.1016/j.arth.2005.07.015 ↗
59. Kurtz, S., Lau, E., et al. 2008a. Future young patient demand for primary and revision joint replacement: National projections from 2010 to 2030. In: 54th Annual Meeting of the Orthopedic Research Society, San Francisco, Poster 175410.1007/s11999-009-0834-6 ↗
60. Kurtz, S., MacDonald, D., et al. 2008b. In vivo oxidation, oxidation potential, and clinical performance of first and second-generation highly crosslinked acetabular bearings for THA. In: 54th Annual Meeting of the Orthopedic Research Society, San Francisco, Poster 1790
61. Kurtz, S., MacDonald, D., et al. 2008c. In vivo oxidation and oxidation potential for polyethylene in total disc replacement following gamma sterilization in air and first-generation barrier packaging. In: 54th Annual Meeting of the Orthopedic Research Society, San Francisco, Poster 1324
62. Anisotropy and oxidative resistance of highly crosslinked UHMWPE after deformation processing by solid-state ram extrusion10.1016/j.biomaterials.2005.05.102 ↗
63. Projections of primary and revision hip and knee arthroplasties in the united states from 2005 to 203010.2106/00004623-200704000-00012 ↗
64. In vivo degradation of polyethylene liners after gamma sterilization in Air10.2106/JBJS.D.02111 ↗
65. Polyethylene wear and rim fracture in total disc arthroplasty10.1016/j.spinee.2006.05.012 ↗
66. Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty10.1016/S0142-9612(99)00053-8 ↗
67. Relationship between the clinical performance and large deformation mechanical behavior of retrieved UHMWPE tibial inserts10.1016/S0142-9612(99)00178-7 ↗
68. Thermomechanical behavior of virgin and highly crosslinked ultra-high molecular weight polyethylene used in total joint replacements10.1016/S0142-9612(02)00102-3 ↗
69. Simulation of large strain plastic deformation and texture evolution in high density polyethylene10.1016/0032-3861(93)90039-D ↗
70. Wear of shelf-aged UHMWPE acetabular liners
71. Properties of crosslinked ultra-high-molecular-weight polyethylene
72. Current concepts review: Ultra high molecular weight polyethylene
73. Structure and plastic deformation of polyethylene10.1007/BF01162485 ↗
74. In vivo comparative wear study of traditional and highly cross-linked polyethylene in total hip arthroplasty10.1016/j.arth.2005.03.033 ↗
75. Fracture of posterior-stablized tibial insert in a genesis knee prosthesis10.1054/arth.2000.4810 ↗
76. Fracture of the polyethylene tibial post in a posterior cruciate-substituting total knee arthroplasty mimicking patellar clunk syndrome10.1016/S0883-5403(03)00333-4 ↗
77. Wear of gamma-crosslinked polyethylene acetabular cups against roughened femoral balls10.1097/00003086-199912000-00008 ↗
78. Development of an extremely wear-resistant ultra High molecular weight polyethylene for total hip replacement10.1002/jor.1100170203 ↗
79. Effect of sterilization method and other modifications on the wear resistance of acetabular cups made of ultra-high molecular weight polyethylene
80. Comparative fatigue behavior and toughness of remelted and annealed highly crosslinked polyethylenes10.1002/jbm.b.30807 ↗
81. Fracture of the polyethylene tibial post in posterior stabilized (Insall Burstein II) total knee arthroplasty10.1054/arth.2000.6615 ↗
82. The effect of cyclic true strain on the morphology, structure, and relaxation behavior of ultra high molecular weight polyethylene10.1016/S0032-3861(00)00626-1 ↗
83. Influence of lamella features of UHMWPE on its physical and uniaxial tensile properties. I. Effect of sterilization method in uncrosslinked and unaged materials
84. A novel method of crosslinking ultra high molecular weight polyethylene to improve wear, reduce oxidation, and retain mechanical properties10.1054/arth.2001.20540 ↗
85. Unified wear model for highly crosslinked ultra-high molecular with polyethylenes (UHMWPE)10.1016/S0142-9612(99)00039-3 ↗
86. Murphy, J., Sobieraj, M., et al. 2008. Unpublished data. Musculoskeletal, Mechanics, and Materials Lab, Departments of Mechanical and Aerospace Engineering and of Orthopaedics, Case Western Reserve University and University Hospitals Case Medical Center, Cleveland, OH
87. Effect of cross-linkage by gamma irradiation in heavy doses to low wear polyethylene in total hip prostheses
88. Improvement of polyethylene by irradiation in artificial joints
89. In vivo and in vitro wear behaviour on weight bearing surfaces of polyethylene sockets improved by irraditation in total hip prostheses
90. Wear resistance and mechanical properties of highly cross-linked, ultrahigh-molecular weight polyethylene doped with vitamin E10.1016/j.arth.2005.07.009 ↗
91. The effect of alpha-tocopherol on the oxidation and free radical decay in irradiated UHMWPE. Biomaterials10.1016/j.biomaterials.2006.07.017 ↗
92. α-Tocopherol-doped irradiated UHMWPE for high fatigue resistance and low wear10.1016/j.biomaterials.2003.12.048 ↗
93. Drawing and extrusion of semi-crystalline polymers10.1007/BF01412215 ↗
94. Deformation, yielding, fracture and fatigue behavior of conventional and highly cross-linked ultra high molecular weight polyethylene10.1016/j.biomaterials.2004.03.022 ↗
95. Phase transformation in explanted crystalline UHMWPE acetabular cups and debris after in vivo wear10.1016/j.molstruc.2005.09.029 ↗
96. Fatigue strength of polyethylene after sterilization by gamma irradiation or ethylene oxide10.1097/00003086-199612000-00008 ↗
97. Post-irradiation aging of ultra-high molecular weight polyethylene10.2106/00004623-199407000-00014 ↗
98. In vivo wear and migration of highly cross-linked polyethylene cups–A radiostereometry analysis study10.1016/j.arth.2004.09.040 ↗
99. Dislocation approact to the plastic deformation of semicrystalline polymers: Kinetic aspects for polyethylene and polypropylene
100. Shaw, J.H., 1997. The effect of gamma irradiation on ultra high molecular weight polyethylene. Medical Devices Agency, UK Department of Health, London, pp. 30