journal article·2017-07Open access

The effect of post-sintering treatments on the fatigue and biological behavior of Ti-6Al-4V ELI parts made by selective laser melting

M. Benedetti, E. Torresani, M. Leoni, V. Fontanari, M. Bandini, C. Pederzolli, C. Potrich

Abstract

Fatigue resistance and biocompatibility are key parameters for the successful implantation of hard-tissue prostheses, which nowadays are more and more frequently manufactured by selective laser melting (SLM). For this purpose, the present paper is aimed at investigating the effect of post-sintering treatments on the fatigue behavior and biological properties of Ti samples produced by SLM. After the building process, all samples are heat treated to achieve a complete stress relief. The remaining ones are tribofinished with the aim of reducing the surface roughness of the as-sintered condition. Part of the tribofinished samples are then subjected to one of the following post-sintering treatments: (i) shot peening, (ii) hot isostatic pressing (HIP), and (iii) electropolishing. It is found that shot peening and HIP are the most effective treatments to improve the high and the very-high cycle fatigue resistance, respectively. At the same time, they preserve the good biocompatibility ensured by the biomedical Titanium Grade 23.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Additive manufacturing of dense metal parts by electron beam melting
2. Post-processing of selective laser sintered metal parts10.1108/13552549510086853 ↗
3. Osteoblast adhesion on biomaterials10.1016/S0142-9612(99)00242-2 ↗
4. Corrosion behaviour of commercially pure titanium shot blasted with different materials and sizes of shot particles for dental implant applications10.1016/S0142-9612(02)00314-9 ↗
5. Subsurface crack initiation in high cycle fatigue in Ti6A14V and in a typical martensitic stainless steel10.1016/0036-9748(83)90385-X ↗
6. The effect of different surface morphology and roughness on osteoblast-like cells10.1002/jbm.a.31652 ↗
7. Fatigue behavior of Ti6Al4V and 316 LVM blasted with ceramic particles of interest for medical devices10.1016/j.jmbbm.2013.10.013 ↗
8. Wire based additive layer manufacturing: comparison of microstructure and mechanical properties of Ti–6Al–4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
9. The effect of bi-modal and lamellar microstructures of Ti-6Al-4V on the behaviour of fatigue cracks emanating from edge-notches10.1111/j.1460-2695.2004.00825.x ↗
10. Influence of sharp microstructural gradients on the fatigue crack growth resistance of α + β and near-α titanium alloys10.1111/j.1460-2695.2005.00932.x ↗
11. High- and very high-cycle plain fatigue resistance of shot peened high-strength aluminum alloys: the role of surface morphology10.1016/j.ijfatigue.2014.07.002 ↗
12. On the combination of the critical distance theory with a multiaxial fatigue criterion for predicting the fatigue strength of notched and plain shot-peened parts10.1016/j.ijfatigue.2016.08.015 ↗
13. Additive manufactured Ti-6Al-4V using welding wire: comparison of laser and arc beam deposition and evaluation with respect to aerospace material specifications10.1016/j.phpro.2010.08.087 ↗
14. Brandl, E., Leyens, C., Palm, F., 2011. Mechanical properties of additive manufactured Ti-6Al-4V using wire and powder based processes, in: IOP Conference Series: Materials Science and Engineering. IOP Publishing, p. 012004.10.1088/1757-899X/26/1/012004 ↗
15. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): microstructure, high cycle fatigue, and fracture behavior10.1016/j.matdes.2011.07.067 ↗
16. Mechanical properties of open-cell metallic biomaterials manufactured using additive manufacturing10.1016/j.matdes.2013.01.071 ↗
17. Fatigue characterization of titanium Ti-6Al-4V samples produced by additive manufacturing10.1016/j.prostr.2016.06.395 ↗
18. The removal torque of titanium screw inserted in rabbit tibia treated by dual acid etching10.1016/S0142-9612(03)00218-7 ↗
19. Progress toward an integration of process–structure–property–performance models for “three-dimensional (3-D) printing” of titanium alloys10.1007/s11837-014-1007-y ↗
20. Microstructure and mechanical properties of Ti-6Al-4V produced by electron beam melting of pre-alloyed powders10.1108/13552540910960262 ↗
21. Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
22. Analytical modelling of residual stress in additive manufacturing10.1111/ffe.12560 ↗
23. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
24. Froes · 2014 · 19
25. On the nature and crystallographic orientation of subsurface cracks in high cycle fatigue of Ti-6Al-4V10.1007/BF02656635 ↗
26. Gong, H., Rafi, K., Starr, T., Stucker, B., 2012. Effect of defects on fatigue tests of as-built Ti-6Al-4V parts fabricated by selective laser melting, in: Proceedings of the Solid Freeform Fabrication Symposium, Austin, TX, USA. pp. 6–8.
27. In situ characterization of the deformation and failure behavior of non-stochastic porous structures processed by selective laser melting10.1016/j.msea.2011.07.026 ↗
28. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting
29. Computational prediction of the fatigue behavior of additively manufactured porous metallic biomaterials10.1016/j.ijfatigue.2015.11.017 ↗
30. Significance of nano-and microtopography for cell-surface interactions in orthopaedic implants
31. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
32. Binding mechanisms in selective laser sintering and selective laser melting10.1108/13552540510573365 ↗
33. Titanium nanostructures for biomedical applications
34. Osteoblastic cell behaviour on different titanium implant surfaces10.1016/j.actbio.2007.12.002 ↗
35. Change in surface roughness by dynamic shape-memory acrylate networks enhances osteoblast differentiation10.1016/j.biomaterials.2016.08.004 ↗
36. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
37. The role and future of the laser technology in the additive manufacturing environment10.1016/j.phpro.2010.08.123 ↗
38. Predicting sintering deformation of ceramic film constrained by rigid substrate using anisotropic constitutive law10.1016/j.actamat.2010.07.015 ↗
39. Fatigue behavior of thin-walled grade 2 titanium samples processed by selective laser melting. Application to life prediction of porous titanium implants10.1016/j.jmbbm.2013.08.011 ↗
40. Lütjering · 2007
41. Microstructure and mechanical behavior of Ti–6Al–4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
42. Characterization of titanium aluminide alloy components fabricated by additive manufacturing using electron beam melting10.1016/j.actamat.2009.11.032 ↗
43. Next-generation biomedical implants using additive manufacturing of complex, cellular and functional mesh arrays
44. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
45. Park · 1992
46. Mechanical evaluation of porous titanium (Ti6Al4V) structures with electron beam melting (EBM)10.1016/j.jmbbm.2009.10.006 ↗
47. Pederson · 2002
48. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
49. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
50. Duality of the S–N fatigue curve caused by competing failure modes in a titanium alloy and the role of Poisson defect statistics10.1016/j.actamat.2004.12.032 ↗
51. Porous titanium scaffolds fabricated using a rapid prototyping and powder metallurgy technique10.1016/j.biomaterials.2008.05.032 ↗
52. The effects on bone cells of metal ions released from orthopaedic implants. A review
53. Microstructure and mechanical properties of pure titanium models fabricated by selective laser melting10.1243/0954406041319545 ↗
54. Heat treatment of Ti-6Al-7Nb components produced by selective laser melting10.1108/13552540810907974 ↗
55. Commercially pure titanium (cp-Ti) versus titanium alloy (Ti6Al4V) materials as bone anchored implants — Is one truly better than the other?10.1016/j.msec.2016.01.032 ↗
56. Fatigue performance of additive manufactured metallic parts10.1108/13552541311302932 ↗
57. Development of porous medical implant scaffolds via laser additive manufacturing10.1016/S1003-6326(12)61706-3 ↗
58. Electropolishing of CP titanium and its alloys in an alcoholic solution-based electrolyte10.4012/dmj.27.258 ↗
59. Van Hooreweder, B., Boonen, R., Moens, D., Kruth, J.-P., Sas, P., 2012. On the determination of fatigue properties of Ti6Al4V produced by selective laser melting, in: Structures, Structural Dynamics, and Materials and Co-Located Conferences 53rd Aiaa/Asme/Asce/Ahs/Asc. American Institute of Aeronautics and Astronautics.10.2514/6.2012-1733 ↗
60. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
61. Microstructural and mechanical approaches of the selective laser melting process applied to a nickel-base superalloy10.1016/j.msea.2011.11.092 ↗
62. High Cycle Fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
63. Ti-6Al-4V additively manufactured by selective laser melting with superior mechanical properties10.1007/s11837-015-1297-8 ↗
64. Material properties of Ti6Al4V parts produced by laser metal deposition10.1016/j.phpro.2012.10.056 ↗