Ductility improvement due to martensite α′ decomposition in porous Ti–6Al–4V parts produced by selective laser melting for orthopedic implants
Source abstract
Abstract
Ti-6Al-4V parts obtained by selective laser melting typically have an acicular α' martensitic microstructure whose ductility is low. Thus, post-heat treatments are useful for increasing ductility. In this work, the effects of sub-β-transus heat treatments on the mechanical properties of Ti-6Al-4V parts with porous structures are correlated with martensite α' phase decomposition. The precipitation of β phase and the gradual transformation of α' into α phase by the diffusion of excess vanadium from α' to β phase are proposed to be the main events of martensite α' phase decomposition in parts fabricated by selective laser melting. The heat treatment performed at 650°C for 1h produced no microstructural changes, but the samples treated for at the same temperature 2h showed a fine precipitation of β phase along the α' needle boundaries. The heat treatment performed at 800°C for 1 or 2h produced a fine α+β microstructure, in which β phase are present as particles fewer in number and larger in size, when compared with the ones present in the sample heat-treated at 650°C for 2h. Heat-treatment of the parts at 800°C for 2h proved to be the best condition, which improved the ductility of the samples while only slightly reducing their strength.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Phase transformations during cooling in alpha+beta titanium alloys10.1016/S0921-5093(97)00802-2 ↗
2. Designing biocompatible Ti-based metallic glasses for implant applications10.1016/j.msec.2012.11.015 ↗
3. Ultrafine grain formation in a Ti–6Al–4V alloy by thermomechanical processing of a martensitic microstructure10.1007/s11661-014-2205-5 ↗
4. Modelling of heat transfer and phase transformations in the rapid manufacturing of titanium components
5. Cullity · 1978
6. Micromechanical behavior study of α phase with different morphologies of Ti–6Al–4V alloy by microindentation10.1016/j.msea.2013.05.032 ↗
7. Phase transformation dynamics during welding of Ti–6Al–4V10.1063/1.1737476 ↗
8. Ductility of a Ti–6Al–4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
9. Effect of phase transformations on laser forming of Ti–6Al–4V alloy10.1063/1.1944202 ↗
10. The effect of heat treatment on mechanical properties of pulsed Nd: YAG welded thin Ti6Al4V10.4028/www.scientific.net/AMR.189-193.3672 ↗
11. Ti based biomaterials, the ultimate choice for orthopaedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
12. Henry · 1995
13. Homporová, P., Poletti, C., Stockinger, M., Warchomicka, F., 2011. Dynamic phase evolution in titanium alloy Ti–6Al–4V. In: Zhou, L. (Ed.) Proceedings of the 12th World Conference on Titanium. Beijing, China, pp. 19–42.
14. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
15. Leyens · 2003
16. Surface modification of titanium, titanium alloys, and related materials for biomedical applications10.1016/j.mser.2004.11.001 ↗
17. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
18. Room-temperature ductility of Ti–6Al–4V alloy with α′ martensite microstructure10.1016/j.msea.2010.10.070 ↗
19. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
20. Microstructure and mechanical behavior of Ti–6Al–4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
21. Mechanical evaluation of porous titanium (Ti6Al4V) structures with electron beam melting (EBM)10.1016/j.jmbbm.2009.10.006 ↗
22. Use of high temperature X-ray diffractometry to study phase transitions and thermal expansion properties in Ti–6AI–4V10.1179/026708303225008013 ↗
23. Kinetics of martensite decomposition in Ti–/6Al–/4V–/xH alloys10.1016/S0921-5093(03)00350-2 ↗
24. Microstructure and mechanical behavior of porous Ti–6Al–4V parts obtained by selective laser melting10.1016/j.jmbbm.2013.05.011 ↗
25. Residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
26. Selective laser melting of biocompatible metals for rapid manufacturing of medical parts10.1108/13552540710776142 ↗
27. Properties and applications of titanium alloys: a brief review
28. Effect of heat treatment on mechanical properties of Ti–6Al–4V ELI alloy10.1016/j.msea.2008.11.018 ↗
29. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
30. Rapid prototyping: porous titanium alloy scaffolds produced by selective laser melting for bone tissue engineering10.1089/ten.tec.2008.0288 ↗
31. The design of scaffolds for use in tissue engineering. Part II. Rapid prototyping techniques10.1089/107632702753503009 ↗